# US 2017/0253767 A1 · Silicon wafer polishing composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253767 A1
- Document ID: US20170253767A1
- Status: Published application
- Kind: A1
- Application number: 15/602,679
- Filed: 2017-05-23
- Published: 2017-09-07
- Earliest claimed: 2013-06-07
- Assignees: Fujimi Incorporated; Toagosei Co., Ltd.
- Applicants: Fujimi Incorporated; Toagosei Co., Ltd.
- Inventors: Kohsuke TSUCHIYA; Hisanori TANSHO; Taiki ICHITSUBO; Yoshio MORI
- Web page: https://patentgrep.com/patent/US20170253767A1

## CPC

- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- B24B 37/00: Lapping machines or devices; Accessories (B24B3/00 takes precedence)
- B24B 37/044: {characterised by the composition of the lapping agent}
- C09K 3/1436: {Composite particles, e.g. coated particles}
- C09K 3/1463: {Aqueous liquid suspensions}
- H10P 70/15: {by wet cleaning only (H10P70/52 takes precedence)}
- H10P 90/129: {by polishing}
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

This invention provides a silicon wafer polishing composition used in the presence of an abrasive. The composition comprises a silicon wafer polishing accelerator, an amide group-containing polymer, and water. The amide group-containing polymer has a building unit A in its main chain. The building unit A comprises a main chain carbon atom constituting the main chain of the amide group-containing polymer and a secondary amide group or a tertiary amide group. The carbonyl carbon atom constituting the secondary amide group or tertiary amide group is directly coupled to the main chain carbon atom.

## Claims

### Claim 1

A method for polishing a silicon wafer, the method comprising the steps of:
obtaining a polishing composition comprising a silicon wafer polishing accelerator, an amide group-containing polymer, and water; and
supplying the polishing composition to the silicon wafer to carried out a final polishing of the silicon wafer in the presence of an abrasive,
wherein
the amide group-containing polymer has a building unit A in its main chain,
the building unit A comprises a main chain carbon atom constituting the main chain of the amide group-containing polymer and a secondary amide group or a tertiary amide group, and
the secondary amide group or tertiary amide group has a carbonyl carbon directly coupled to the main chain carbon atom.

### Claim 2 (depends on 1)

The method according to claim 1, further comprising the step of rinsing the silicon wafer after the final polishing step by supplying a rinse composition to the silicon wafer, wherein
the rinse composition comprises a silicon wafer polishing accelerator, an amide group-containing polymer, and water,
the amide group-containing polymer has a building unit A in its main chain,
the building unit A comprises a main chain carbon atom constituting the main chain of the amide group-containing polymer and a secondary amide group or a tertiary amide group, and
a carbonyl carbon atom constituting the secondary amide group or tertiary amide group is directly coupled to the main chain carbon atom.

### Claim 3 (depends on 1)

The method according to claim 1, further comprising the step of carrying out a preliminary polishing of the silicon wafer prior to the final polishing.

### Claim 4 (depends on 3)

The method according to claim 3, further comprising the step of carrying out a lapping of the silicon wafer prior to the preliminary polishing.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the amide group-containing polymer has an adsorption ratio of 10% to 80%, when measured by the following method;
(1) a test solution L0 is prepared, which comprises 0.018% by mass of the amide group-containing polymer and 0.01% by mass of ammonia in water;
(2) a test solution L1 is prepared, which comprises 0.46% by mass of the abrasive, 0.018% by mass of the amide group-containing polymer, and 0.01% by mass of ammonia in water;
(3) the test solution L1 is centrifuged to precipitate the abrasive;
(4) from the mass WO of the measured polymer in the test solution L0 and mass W1 of the measured polymer in the supernatant of the centrifuged test solution L1, the adsorption ratio of the measured polymer is determined by the equation:
Adsorption ratio (%)=[(W0−W1)/W0]×100.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the building unit A is obtainable by polymerizing or copolymerizing at least one species selected from the group consisting of monomers represented by the next general formula (1);
wherein R1 is a hydrogen atom, methyl group, phenyl group, benzyl group, chloro group, difluoromethyl group, trifluoromethyl group, or cyano group; R2 and R3 are identical or different wherein R2 is a hydrogen atom, an alkyl group, alkenyl group, alkynyl group, aralkyl group, alkoxy group, alkoxyalkyl group, alkylol group or acetyl group with 1 to 18 carbon atoms, or an aromatic group with 6 to 60 carbon atoms, with each of which except for the hydrogen atom including a species having a substituent, and R3 is an alkyl group, alkenyl group, alkynyl group, aralkyl group, alkoxy group, alkoxyalkyl group, alkylol group or acetyl group with 1 to 18 carbon atoms, or an aromatic group with 6 to 60 carbon atoms, with each of which including a species having a substituent;
monomers represented by the next general formula (2):
wherein R4 is a hydrogen atom, methyl group, phenyl group, benzyl group, chloro group, difluoromethyl group, trifluoromethyl group, or cyano group; and X is (CH2)n (n is an integer between 4 and 6), (CH2)2O(CH2)2 or (CH2)2S(CH2)2; and
monomers represented by the next general formula (3):
wherein R5 is a hydrogen atom, methyl group, phenyl group, benzyl group, chloro group, difluoromethyl group, trifluoromethyl group, or cyano group; R6 and R7 are identical or different, with each being a hydrogen atom, an alkyl group, alkenyl group, alkynyl group, aralkyl group, alkoxy group, alkoxyalkyl group, alkylol group or acetyl group with 1 to 8 carbon atoms, or an aromatic group with 6 to 60 carbon atoms, with each of which except for the hydrogen atom including a species having a substituent; and a is an integer between 1 and 5.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the amide group-containing polymer is nonionic.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the abrasive is silica grains.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the amide group-containing polymer has a molecular weight of below 40×104.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the amide group-containing polymer has a molecular weight of below 5×104.

### Claim 11 (depends on 6)

The method according to claim 6, wherein the building unit A is obtainable by polymerizing or copolymerizing the monomer represented by the formula (2) or the monomer represented by the general formula (3), and
the amide group-containing polymer has a molecular weight of below 10×104.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the silicon wafer polishing composition consists of the abrasive, the silicon wafer polishing accelerator, the amide group-containing polymer, water and optionally a surfactant, an optional polymer and an additive,
the additive is selected from the group consisting of a chelating agent, an inorganic acid, an inorganic acid salt, a preservative and an antifungal agent.

### Claim 13 (depends on 2)

The method according to claim 2, wherein the rinse composition is free of an abrasive which consists of inorganic grains.

### Claim 14 (depends on 2)

The method according to claim 2, wherein the rinse composition is free of an abrasive which consists of inorganic grains, the inorganic grains being silica grains, alumina grains, cerium oxide grains, chromium oxide grains, titanium dioxide grains, zirconium oxide grains, magnesium oxide grains, manganese dioxide grains, zinc oxide grains, red oxide grains, silicon nitride grains, boron nitride grains, silicon carbide grains, boron carbide grains, diamond grains, calcium carbonate grains, and barium carbonate grains.

### Claim 15 (depends on 2)

The method according to claim 2, wherein the building unit A of the amide group-containing polymer contained in the rinse composition is obtainable by polymerizing or copolymerizing at least one species selected from the group consisting of monomers represented by the next general formula (1):
wherein R1 is a hydrogen atom, methyl group, phenyl group, benzyl group, chloro group, difluoromethyl group, trifluoromethyl group, or cyano group; R2 and R3 are identical or different wherein R2 is a hydrogen atom, an alkyl group, alkenyl group, alkynyl group, aralkyl group, alkoxy group, alkoxyalkyl group, alkylol group or acetyl group with 1 to 18 carbon atoms, or an aromatic group with 6 to 60 carbon atoms, with each of which except for the hydrogen atom including a species having a substituent, and R3 is an alkyl group, alkenyl group, alkynyl group, aralkyl group, alkoxy group, alkoxyalkyl group, alkylol group or acetyl group with 1 to 18 carbon atoms, or an aromatic group with 6 to 60 carbon atoms, with each of which including a species having a substituent;
monomers represented by the next general formula (2):
wherein R4 is a hydrogen atom, methyl group, phenyl group, benzyl group, chloro group, difluoromethyl group, trifluoromethyl group, or cyano group; and X is (CH2)n (n is an integer between 4 and 6), (CH2)2O(CH2)2 or (CH2)2S(CH2)2; and
monomers represented by the next general formula (3):
wherein R5 is a hydrogen atom, methyl group, phenyl group, benzyl group, chloro group, difluoromethyl group, trifluoromethyl group, or cyano group; R6 and R7 are identical or different, with each being a hydrogen atom, an alkyl group, alkenyl group, alkynyl group, aralkyl group, alkoxy group, alkoxyalkyl group, alkylol group or acetyl group with 1 to 8 carbon atoms, or an aromatic group with 6 to 60 carbon atoms, with each of which except for the hydrogen atom including a species having a substituent; and a is an integer between 1 and 5.

### Claim 16 (depends on 2)

The method according to claim 2, wherein the amide group-containing polymer contained in the rinse composition is nonionic.

### Claim 17 (depends on 2)

The method according to claim 2, wherein the amide group-containing polymer contained in the rinse composition has a molecular weight of below 40×104.

### Claim 18 (depends on 2)

The method according to claim 2, wherein the amide group-containing polymer contained in the rinse composition has a molecular weight of below 5×104.

### Claim 19 (depends on 2)

The method according to claim 2, wherein the building unit A of the amide group-containing polymer contained in the rinse composition is obtainable by polymerizing or copolymerizing a monomer represented by the general formula (2) or a monomer represented by the general formula (3), and the amide group-containing polymer has a molecular weight of below 10×104.

### Claim 20

A method for rinsing a silicon wafer, comprising
the step of obtaining a rinse composition; and
rinsing the silicon wafer by supplying the rinse composition to the silicon wafer; wherein
the rinse composition comprises a silicon wafer polishing accelerator, an amide group-containing polymer, and water,
the amide group-containing polymer has a building unit A in its main chain,
the building unit A comprises a main chain carbon atom constituting the main chain of the amide group-containing polymer and a secondary amide group or a tertiary amide group, and
a carbonyl carbon atom constituting the secondary amide group or tertiary amide group is directly coupled to the main chain carbon atom.