# US 2017/0253765 A1 · Polysiloxane Films and Methods of Making Polysiloxane Films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253765 A1
- Document ID: US20170253765A1
- Status: Published application
- Kind: A1
- Application number: 15/059,665
- Filed: 2016-03-03
- Published: 2017-09-07
- Earliest claimed: 2016-03-03
- Assignees: Motorola Mobility LLC
- Applicants: Motorola Mobility LLC
- Inventors: Richard W. Brotzman; Ernest Sirois; Deborah Paskiewicz
- Web page: https://patentgrep.com/patent/US20170253765A1

## CPC

- C09D 183/04: Polysiloxanes
- C09D 183/08: containing silicon bound to organic groups containing atoms other than carbon, hydrogen, and oxygen
- H05K 1/18: structurally associated with non-printed electric components (H05K1/16 takes precedence)
- H05K 3/282: {for inhibiting the corrosion of the circuit, e.g. for preserving the solderability}
- H05K 3/285: {Permanent coating compositions}
- C08G 77/24: halogen-containing groups
- C08G 77/80: {Siloxanes having aromatic substituents, e.g. phenyl side groups}
- H05K 2201/0162: Silicon containing polymer, e.g. silicone
- H05K 2201/09872: Insulating conformal coating
- H05K 2201/10015: Non-printed capacitor
- H05K 2201/10022: Non-printed resistor
- H05K 2203/095: Plasma, e.g. for treating a substrate to improve adhesion with a conductor or for cleaning holes
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

A polysiloxane film comprises Si—O bonds and has a thickness of 0.3 to 1.5 microns. Adjacent electrodes coated with the polysiloxane film have a leakage current of at most 0.01 mA at 10 V after contact with water. An electrode coated with the polysiloxane film has a contact resistance of at least 0.01 ohms at 1.0 mm of pogo pin compression under a 1.0 N load. The polysiloxane film provides IPx7 protection from ingress of water.

## Claims

### Claim 1

A polysiloxane film comprising Si—O bonds and having a thickness of 0.3 to 1.5 microns,
wherein the polysiloxane film passes the corrosion current test, and
the polysiloxane film passes the contact resistance test.

### Claim 2 (depends on 1)

The polysiloxane film of claim 1, wherein the polysiloxane film provides IPx7 protection from ingress of water.

### Claim 3 (depends on 1)

The polysiloxane film of claim 1, wherein the polysiloxane film has a thickness of 0.5 to 1.1 microns.

### Claim 4 (depends on 1)

The polysiloxane film of claim 1, wherein the polysiloxane film comprises fluorine.

### Claim 5 (depends on 1)

The polysiloxane film of claim 1, wherein the polysiloxane film comprises carbon deposits.

### Claim 6 (depends on 1)

The polysiloxane film of claim 1, wherein the polysiloxane film has a thickness of 0.5 to 1.1 microns,
the polysiloxane film provides IPx7 protection from ingress of water, and
the polysiloxane film comprises fluorine.

### Claim 7 (depends on 1)

The polysiloxane film of claim 1, wherein the polysiloxane film comprises (SiO)(R1)2 units,
wherein each R1 is independently selected from the group consisting of amino, hydroxyl, mercapto, alkoxy, alkyl, cycloalkyl, aryl and heteroaryl.

### Claim 8 (depends on 7)

The polysiloxane film of claim 7, wherein R1 is substituted with a substituent selected from the group consisting of alkyl, cycloalky, aryl, heteroaryl, amino, hydroxyl, mercapto, alkoxy, a carboxylic acid, phenethyl, a phosphonic acid, a sulfonic acid, a carboxylic ester, a carboxylic amide, a carboxylic anhydride, a saccharide, a halogen, and salts thereof.

### Claim 9

A method of forming a polysiloxane film, comprising:
polymerizing monomers comprising at least one siloxane monomer having the formula (X1)nSi(R1)4-n, wherein n is 1, 2 or 3; (X1)Si(R1)2OSi(R1)2(X1); (X1)(Si(R1)2O)2Si(R1)2(X1); and [OSi(R1)2]m, wherein m is 3 or 4;
wherein X1 is Cl or OR2,
R2 is alkyl,
each R1 is independently selected from the group consisting of amino, hydroxyl, mercapto, alkoxy, alkyl, cycloalkyl, aryl and heteroaryl,
the polysiloxane film contains Si—O bonds,
the polysiloxane film has a thickness of 0.3 to 1.5 microns,
the polysiloxane film passes the corrosion current test, and
the polysiloxane film passes the contact resistance test.

### Claim 10

A method of forming a polysiloxane film in a reaction chamber, comprising:
polymerizing monomers comprising at least one siloxane monomer having the formula (X1)nSi(R1)4-n, wherein n is 1, 2 or 3; (X1)Si(R1)2OSi(R1)2(X1); (X1)(Si(R1)2O)2Si(R1)2(X1); and [OSi(R1)2]m, wherein m is 3 or 4;
wherein the polymerization is catalyzed by a 30-60 W radio frequency plasma,
the pressure in the reaction chamber during the polymerization is 100-400 mTorr,
X1 is Cl or OR2,
R2 is alkyl,
each R1 is independently selected from the group consisting of amino, hydroxyl, mercapto, alkoxy, alkyl, cycloalkyl, aryl and heteroaryl,
the polysiloxane film contains Si—O bonds,
the polysiloxane film has a thickness of 0.3 to 1.5 microns.

### Claim 11 (depends on 10)

The method of claim 10, wherein the residence time of the siloxane monomer in the reaction chamber is 5-120 minutes.

### Claim 12 (depends on 10)

The method of claim 10, wherein the siloxane monomer is heated to 30-200° C. before entering the reaction chamber.

### Claim 13 (depends on 10)

The method of claim 10, wherein the polymerization is carried out at a temperature of 30-100° C.

### Claim 14 (depends on 10)

The method of claim 10, wherein the reaction chamber comprises an inert gas.

### Claim 15 (depends on 14)

The method of claim 14, wherein the gas further comprises oxygen,
wherein oxygen is present as oxygen (O2), ozone (O3), nitrous oxide (N2O), carbon dioxide (CO2), water (H2O), and mixtures thereof.

### Claim 16 (depends on 1)

An electronic device comprising electrical components coated with the polysiloxane film of claim 1.

### Claim 17 (depends on 2)

An electronic device comprising electrical components coated with the polysiloxane film of claim 2.

### Claim 18 (depends on 1)

The polysiloxane film of claim 1, further comprising a non-volatile diluent.

### Claim 19 (depends on 10)

The method of claim 10, further comprising swelling the polysiloxane film with a non-volatile diluent.

### Claim 20 (depends on 9)

A polysilxane film prepared by the method of claim 9.