# US 2017/0253692 A1 · Highly functional natural material-derived epoxy resin, preparation method therefor, and epoxy resin curing composition using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253692 A1
- Document ID: US20170253692A1
- Status: Published application
- Kind: A1
- Application number: 15/316,804
- Filed: 2015-06-09
- Published: 2017-09-07
- Earliest claimed: 2014-07-18
- Assignees: Kukdo Chemical Co., Ltd.
- Applicants: Kukdo Chemical Co., Ltd.
- Inventors: HYE SEUNG LEE; JAE IL KIM
- Web page: https://patentgrep.com/patent/US20170253692A1

## CPC

- C08G 59/26: heterocyclic
- C07D 493/04: Ortho-condensed systems
- C08G 59/04: of polyhydroxy compounds with epihalohydrins or precursors thereof
- C08G 59/42: Polycarboxylic acids; Anhydrides, halides or low molecular weight esters thereof
- C08G 59/44: Amides
- C08G 59/504: {containing an atom other than nitrogen belonging to the amine group, carbon and hydrogen}
- C09D 163/00: Coating compositions based on epoxy resins; Coating compositions based on derivatives of epoxy resins
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C07D: HETEROCYCLIC COMPOUNDS (macromolecular compounds C08)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

Disclosed are a highly functional natural material-derived epoxy resin, a preparation method therefor, and an epoxy resin curing composition using the same. The highly functional natural material-derived epoxy resin represented by chemical formula 1 is obtained by reacting a compound, represented by chemical formula 2, and epichlorohydrin (ECH), which is obtained by using glycerin as a starting material, in the presence of a hydroxide salt.

## Claims

### Claim at position 1

-3. (canceled)

### Claim 4

A natural ingredient-derived epoxy resin composition with water debonding property comprising:
a natural material-derived epoxy resin represented by the following Formula 1, the natural material-derived epoxy resin being obtained by reacting a compound represented by Formula 2 with epichlorohydrin (ECH) obtained from glycerin as a starting material in the presence of a hydroxide salt; and
a polyamide curing agent represented by the following formula 4:
wherein n is a natural number of 0 to 300,
wherein R and R′ are each independently H or CxHy, in which x and y are a natural number of 1 to 30.

### Claim 5

A natural ingredient-derived epoxy resin composition with anti-fog property comprising:
a natural material-derived epoxy resin represented by the following Formula 1, the natural material-derived epoxy resin being obtained by reacting a compound represented by Formula 2 with epichlorohydrin (ECH) obtained from glycerin as a starting material in the presence of a hydroxide salt; and
a polyetheramine curing agent represented by the following formula 5:
wherein n is a natural number of 0 to 300,
wherein n is a natural number of 1 to 100.

### Claim 6

(canceled)

### Claim 7

A method of preparing the natural material-derived epoxy resin, the method comprising:
a first step including mixing 550 to 650 parts by weight of epichlorohydrin (ECH) obtained from glycerin as a starting material with 100 parts by weight of a compound represented by the following Formula 2, dissolving the mixture at an elevated temperature of 60 to 75° C., adding 5 to 11 parts by weight of sodium hydroxide (NaOH) to 100 parts by weight of a compound represented by the following Formula 2 and conducting preliminary reaction for 2 to 4 hours:
a second step including conducting main reaction of the reactants of the first step at a temperature of 60 to 75° C. and at a reduced pressure of 180 to 250 torr, the main reaction being carried out for 3 to 6 hours by adding 44 to 60 parts by weight of sodium hydroxide (NaOH) to 100 parts by weight of the compound represented by the following Formula 2;
a third step including standing the reaction solution after reaction of the second step, separating the supernatant by reverse aliquoting and filtering the same; and
a fourth step including collecting epichlorohydrin from the filtrate.
wherein n is a natural number of 0 to 300,

### Claim 8

(canceled)

### Claim 9

(canceled)