# US 2017/0253681 A1 · Material for 3d printing, process for preparing the same and article thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253681 A1
- Document ID: US20170253681A1
- Status: Published application
- Kind: A1
- Application number: 15/507,670
- Filed: 2015-04-24
- Published: 2017-09-07
- Earliest claimed: 2014-04-30
- Assignees: Institute of Chemistry, Chinese Academy of Sciences
- Applicants: Institute of Chemistry, Chinese Academy of Sciences
- Inventors: Heng SHEN; Jing GUO; Tang ZHU; Ning ZHAO; Jian XU; Wenhua SUN; Jinyong DONG; Chuncheng LI; Wenxin FU; Xuechun LIN; Yongmei MA
- Web page: https://patentgrep.com/patent/US20170253681A1

## CPC

- C08F 220/1803: {C3-(meth)acrylate, e.g. (iso)propyl (meth)acrylate}
- B28B 1/001: {Rapid manufacturing of 3D objects by additive depositing, agglomerating or laminating of material (selective deposition modelling of metallic powder B22F10/00; rapid manufacturing of 3D objects in general and in particular of plastics B29C64/00)}
- B29C 64/106: using only liquids or viscous materials, e.g. depositing a continuous bead of viscous material
- B29C 64/165: using a combination of solid and fluid materials, e.g. a powder selectively bound by a liquid binder, catalyst, inhibitor or energy absorber
- B33Y 10/00: Processes of additive manufacturing
- B33Y 70/10: Composites of different types of material, e.g. mixtures of ceramics and polymers or mixtures of metals and biomaterials
- C08F 2/44: Polymerisation in the presence of compounding ingredients, e.g. plasticisers, dyestuffs, fillers
- C08F 2/48: by ultraviolet or visible light
- C08F 2/50: with sensitising agents
- C08F 220/1802: {C2-(meth)acrylate, e.g. ethyl (meth)acrylate}
- C08F 220/1807: {C7-(meth)acrylate, e.g. heptyl (meth)acrylate or benzyl (meth)acrylate}
- C08J 3/12: Powdering or granulating
- C08J 3/203: {Solid polymers with solid and/or liquid additives}
- C08K 3/011: Crosslinking or vulcanising agents, e.g. accelerators
- C08K 3/013: Fillers, pigments or reinforcing additives
- C08K 3/08: Metals
- C08F 220/1804: {C4-(meth)acrylate, e.g. butyl (meth)acrylate, isobutyl (meth)acrylate or tert-butyl (meth)acrylate}
- C08F 220/1812: {C12-(meth)acrylate, e.g. lauryl (meth)acrylate}
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- B28B: SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER (foundry moulding B22C; working stone or stone-like material B28D; shaping of substances in a plastic state, in general B29C; making layered products not composed wholly of these substances B32B)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

The present invention provides a composition for 3D printing, a process for preparing the same and an article thereof. By the solidifying method of UV irradiation, 3D printing is implemented. During said implementation, there is no need of high temperature heating, thus energy consumption is reduced, and there is no need for special solvent, thus harm to the environment is reduced. Meanwhile, the present invention uses micro-nano powder as the main material and polymer resin as adhesive, and at the same time, adds irradiation sensitizer. After electron beam irradiation, the polymer resin forms three-dimensional crosslinked network, thereby the strength, heat resistance and chemical resistance are improved after resin adhesion. Additionally, the present invention, by the addition of UV crosslinking agent, and by UV irradiation, cross-links the unsaturated resin after extrusion in 3D printing to form three-dimensional network structure, thus greatly improves the heat resistance, chemical resistance and mechanical strength of the shaping material, and makes the unsaturated resin have broader application prospects in 3D printing material.

## Claims

### Claim 1

A composition for 3D printing comprising the following components:
photosensitive monomer: 100 parts by weight,
photoinitiator: 1 to 3 parts by weight,
micro-nano powder: 1 to 30 parts by weight,
crosslinking agent: 1 to 30 parts by weight,
toughening agent: 1 to 10 parts by weight, and
pigment: 5 to 10 parts by weight;
wherein the photosensitive monomer is monofunctional acrylate which is in liquid state at room temperature.

### Claim 2 (depends on 1)

The composition according to claim 1, wherein the monofunctional acrylate which is in liquid state at room temperature is one or more selected from the group consisting of methyl methacrylate, ethyl methacrylate, propyl methacrylate, isopropyl methacrylate, benzyl methacrylate, lauryl methacrylate and acrylate derivatives;
preferably, the photoinitiator is alkylphenones, the alkylphenone is one or more selected from the group consisting of α,α-diethoxyacetophenone, α-hydroxyalkylphenone, and α-aminoalkylphenone;
the micro-nano powder refers to a particulate matter having a particle size between 1 nm and 100 μm, preferably, the micro-nano powder is one or more selected from the group consisting of inorganic micro-nano powder and organic-inorganic hybrid micro-nano powder, preferably, the inorganic micro-nano powder is one or more selected from the group consisting of metal particles, metal oxide particles, non-metallic particles, silver halide particles, carbonate particles, and phosphate particles, preferably, the organic-inorganic hybrid micro-nano powder has a shell structure or an asymmetric structure;
further preferably, the micro-nano powder has a particle size between 50 nm and 10 μm;
preferably, the micro-nano powder is a micro-nano powder modified by a surface modifier; and
preferably, the surface modifier is one or more selected from the group consisting of dopamine and silane coupling agents such as KH550, KH560, KH570, KH792 or DL602.

### Claim 3 (depends on 1)

The composition according to claim 1, wherein the crosslinking agent is a multifunctional acrylate; preferably, the multifunctional acrylate is one or more selected from the group consisting of bifunctional crosslinking agents (such as diethylene glycol dimethacrylate, triethylene glycol dimethacrylate, tetraethylene glycol dimethacrylate, etc.), and trifunctional crosslinking agents (such as trimethylolpropane trimethacrylate, trimethylolpropane triacrylate, etc.);
preferably, the toughening agent is a liquid polysulfide rubber; and
preferably, the pigment is an inorganic color pigment, more preferably, the inorganic color pigment is one or more selected from the group consisting of chromate pigments (such as lead chrome yellow, molybdenum chrome orange, etc.), cadmium pigments (such as cadmium yellow, cadmium red, etc.), iron pigments (such as iron yellow, iron red, etc.), green pigments (such as chrome green, chromium oxide green, etc.) and blue pigments (such as iron blue, ultramarine, etc.).

### Claim 4 (depends on 1)

A process for preparing the composition for 3D printing according to claim 1, comprising the steps of mixing the various components;
preferably, specifically comprising the following steps:
1) mixing 100 parts by weight of a photosensitive monomer, 1 to 30 parts by weight of a micro-nano powder, 1 to 30 parts by weight of a crosslinking agent and 5 to 10 parts by weight of a pigment; and
2) mixing the mixture obtained in step 1) with 5 to 10 parts by weight of a toughening agent, and 1 to 3 parts by weight of a photoinitiator;
wherein, preferably, both of the mixing operations are carried out at room temperature (20 to 40° C.);
preferably, the mixing in step 1) is carried out sufficiently by mechanical stirring at a rotational speed of 1000 to 4000 rpm for 1 to 2 hours; and
preferably, step 2) is the step of sufficiently mixing for 1 to 2 hours at a rotational speed of 1000 to 4000 rpm under dark condition.

### Claim 5

A high filling level micro-nano powder/polymer composite material for 3D printing using a micro-nano powder as the main raw material and a polymer resin as adhesive, having the following raw materials and their contents (parts by weight):
micro-nano powder: 90 to 70 parts,
polymer resin: 10 to 30 parts, and
irradiation sensitizer: 0.05 to 0.2 parts;
wherein, preferably, the composite material is prepared by a process comprising the mixing of raw materials and extrusion pelletization by a screw extruder;
preferably, the micro-nano powder refers to a particulate matter having a particle size between 1 nm and 100 μm; preferably, the micro-nano powder is an inorganic micro-nano powder; and more preferably, the inorganic micro-nano powder is one or more selected from the group consisting of metal powder, metal oxide powder, non-metallic powder, silver halide powder, carbonate powder, phosphate powder, silicate powder, and clay powder; preferably, the particle size of the micro-nano powder is between 50 nm and 10 μm;
preferably, the micro-nano powder is a micro-nano powder modified by a surface modifier;
preferably, the surface modifier is one or more selected from the group consisting of dopamine and silane coupling agents such as KH550, KH560, KH570, KH792 or DL602;
preferably, the polymer resin is a thermoplastic resin; more preferably, the thermoplastic resin is one or more selected from the group consisting of polyolefins (PE, PP, PVC, PS), polyamide (PA), polycarbonate (PC), polyoxymethylene (POM), ethylene-vinyl acetate copolymer (EVA), polyester (PET, PBT, PCL, PLA), acrylonitrile-styrene-butadiene copolymer (ABS), styrene-butadiene-styrene block copolymer (SBS), styrene-isoprene-styrene block copolymer (SIS), butadiene-styrene transparent impact resin (K resin), and polyacrylate;
preferably, the selected polymer resin has a melt index of at least greater than 10; and
preferably, the radiation sensitizer is one or more selected from the group consisting of triallyl cyanurate, triallyl isocyanurate, trimethallyl isocyanurate, trimethylolpropane trimethacrylate, trimethylolpropane triacrylate, triallyl 1,3,5-benzenetricarboxylate, diallyl isocyanate, dially isophthalate, bismaleimide, triethylene glycol dimethacrylate, and diethylene glycol dimethacrylate.

### Claim 6 (depends on 5)

The high filling level micro-nano powder/polymer composite material for 3D printing according to claim 5, characterized in that the raw materials further comprise:
Antioxidant: 0.01-0.02 parts;
preferably, the antioxidant is a hindered phenolic antioxidant and/or a phosphite auxiliary antioxidant; more preferably it is one or more selected from the group consisting of antioxidant 1010: pentaerythritol tetra[β-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate]; antioxidant 1096: IRGANOX B-1096; coordinated compound of main antioxidant 1098: 3,3′-bis(3,5-di-tert-butyl-4-hydroxyphenyl)-N,N′-hexamethylenedipropionamide with phosphite antioxidant; and antioxidant 168: tris [2,4-di-tert-butylphenyl] phosphite;
preferably, the raw materials of the material and their contents (parts by weight) are:
micro-nano powder: 90 to 70 parts,
polymer resin: 10 to 30 parts,
irradiation sensitizer: 0.05 to 0.2 parts, and
antioxidant: 0.01 to 0.02 parts.

### Claim 7 (depends on 5)

A process for preparing the high filling level micro-nano powder/polymer composite material for 3D printing according to claim 5, comprising the steps of mixing of raw materials and extrusion pelletization by a screw extruder;
preferably, specifically comprising:
1) modifying the micro-nano powder;
2) mixing the various raw materials; and
3) extruding and pelletizing by a screw extruder;
wherein, preferably, the above step 1) specifically comprises subjecting 100 parts by weight of the micro-nano powder to surface modification with 5 to 20 parts of the surface modifier in solution;
preferably, the step 2) is specifically: uniformly mixing 10 to 30 parts by weight of a polymer resin, 90 to 70 parts of modified micro-nano powder, 0.05 to 0.2 parts of a radiation sensitizer, and 0.01 to 0.02 parts of an antioxidant at room temperature, and feeding the mixture to a twin-screw extruder having an aspect ratio of 36 for extrusion pelletization, wherein the rotational speed of the extruder is 20 to 100 r/min, the temperature ranges of the various sections of the extruder are: feeding section 150 to 170° C., melting section 190 to 200° C., mixing section 190 to 200° C., exhaust section 170 to 190° C., and homogenization section 160 to 180° C.;
preferably, the step specifically comprises:
feeding the pellets of the composite material to the head of the 3D printer, heating and melting the pellets in the head, moving the head along the sectional profile and the filling path of the part while at the same time extruding the melted material, rapidly solidifying the melted material after extrusion under computer control and irradiating it using electron beam, to crosslink the material, and forming shape by accumulation layer by layer; and
more preferably, the electron accelerator energy is 0.3 to 5 MeV, the power is 50 to 150 KW, and the irradiation dose is 5 to 20 KGy.

### Claim 8

A UV radiation crosslinked polymer composition for 3D printing comprising the following main components:
unsaturated resin: 100 parts by weight, and
UV crosslinking agent: 0.5 to 5 parts by weight,
wherein the unsaturated resin is selected from monofunctional or multifunctional ethylenically unsaturated polymers having a molecular weight of from 3,000 to 100,000, and having a melting point (or softening flow temperature) between 100 and 350° C.;
wherein the UV crosslinking agent is a C3 or higher compound containing two or more terminal mercapto groups;
preferably, the monofunctional or multifunctional ethylenically unsaturated polymer is one or more selected from the group consisting of polyolefins (such as PE, PP, PVC, PS, PB, etc.), polyalkynes (such as polyacetylene, polypropyne, etc.), unsaturated polyamides, unsaturated polycarbonates, unsaturated polyesters, ABS resins, and bicomponent or multicomponent copolymers of polyunsaturated olefins (such as butadiene, isoprene, etc.) and other olefinic monomers (such as styrene-butadiene-styrene block copolymer (SBS), styrene-isoprene-styrene block copolymer (SIS) and butadiene-styrene transparent impact resin (K resin)); and
preferably, the UV crosslinking agent includes, but is not limited to, pentaerythritol tetramercaptoacetate, 4′,4-dimercaptodiphenyl sulfide, 2,5-dimercaptothiadiazole, trithiocyanuric acid or their homologues and derivatives, as well as combinations of the above compounds in any ratio.

### Claim 9 (depends on 8)

The UV radiation crosslinked polymer composition according to claim 8, characterized in that the composition further comprises an aid for enhancing the printing effect without affecting its main function, specifically including:
Antioxidant: 0.1-0.5 parts by weight,
Powder: 1-20 parts by weight,
Pigment: 0-10 parts by weight, and
other aids: 0-5 parts by weight;
preferably, the antioxidant is one or more selected from the group consisting of antioxidant 1010, antioxidant 1096, coordinated compound of main antioxidant 1098 and phosphite antioxidant and antioxidant 168, wherein, antioxidant 1010 refers to: pentaerythritol tetra[β-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate]; antioxidant 1096 refers to: IRGANOX B-1096; main antioxidant 1098 refers to: 3,3′-bis(3,5-di-tert-butyl-4-hydroxyphenyl)-N,N′-hexamethylenedipropionamide; and antioxidant 168 refers to: tris [2,4-di-tert-butylphenyl] phosphite;
the powder is preferably a particulate material having a particle size between 1 nm and 100 μm (also referred to as micro-nano particles); preferably, the powder is one or more selected from the group consisting of inorganic micro-nano particles, organic polymer micro-nano particles and organic-inorganic hybrid micro-nano particles; preferably, the inorganic micro-nano particles are one or more selected from the group consisting of metal micro-nano particles (such as silver, gold, iron, platinum particles, etc.), metal oxide micro-nano particles (such as Fe3O4, TiO2, Cu2O, ZnO, CdS particles, etc.), non-metallic micro-nano particles (such as carbon, silicon particles, etc.), silver halide micro-nano particles (such as AgCl, AgBr particles, etc.), carbonate micro-nano particles (such as CaCO3, BaCO3 particles, etc.) and phosphate micro-nano particles (such as LiFePO4 particles, etc.); preferably, the organic polymer micro-nano particles are one or more selected from the group consisting of polystyrene, polypropylene, polytetrafluoroethylene, ABS, epoxy resins, and other micro-nano particles; preferably, the organic-inorganic hybrid micro-nano particles have one or more of a core-shell structure or an asymmetric structure, such as PS @ Fe3O4, PS @ Dopa @ Ag, etc.;
preferably, the pigment is an inorganic color pigment; the inorganic color pigment is preferably one or more selected from the group consisting of chromate pigments (such as lead chrome yellow, molybdenum chrome orange, etc.), cadmium pigments (such as cadmium yellow, cadmium red, etc.), iron pigments (such as iron yellow, iron red, etc.), green pigments (such as chrome green, chromium oxide green, etc.) and blue pigments (such as iron blue, ultramarine, etc.); and
preferably, the other aid is an aid suitable for composition for 3D printing, such as inhibitor (mainly for preventing the material from being ineffective due to polymerization during storage and transportation), etc.

### Claim 10 (depends on 8)

A UV radiation crosslinked polymer material for 3D printing, which is prepared from the UV radiation crosslinked polymer composition for 3D printing according to claim 8;
wherein, preferably, the material is prepared by a process comprising the following steps:
uniformly mixing 100 parts by weight of an unsaturated resin, 0.5 to 5 parts by weight of a UV crosslinking agent and optionally 0.1 to 0.5 parts by weight of an antioxidant, 1 to 20 parts by weight of a powder, 0 to 10 parts by weight of a pigment and 0-5 parts by weight of other aids, and extruding into filaments;
preferably, the mixing is carried out with a single screw extruder.

### Claim 11 (depends on 3)

A process for preparing the UV radiation crosslinked polymer material for 3D printing according to claim 3, comprising the following steps:
uniformly mixing 100 parts by weight of an unsaturated resin, 0.5 to 5 parts by weight of a UV crosslinking agent and optionally 0.1 to 0.5 parts by weight of an antioxidant, 1 to 20 parts by weight of a powder, 0 to 10 parts by weight of a pigment and 0 to 5 parts by weight of other aids, and extruding into filaments;
preferably, characterized in that the process comprises following the steps:
uniformly mixing 100 parts by weight of an unsaturated resin, 0.5 to 5 parts by weight of a UV crosslinking agent, 0.1 to 0.5 parts by weight of an antioxidant, 1 to 20 parts by weight of a powder, 0 to 10 parts by weight of a pigment and 0-5 parts by weight of other aids with a single screw extruder, and extruding into filaments.

### Claim 12

-14. (canceled)