# US 2017/0253674 A1 · Cellulose ethers substituted with hydroxyl and alkyne groups and with hydroxyalkyl, alkyne and azide groups, and use thereof as water-insoluble adhesives

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253674 A1
- Document ID: US20170253674A1
- Status: Published application
- Kind: A1
- Application number: 15/444,904
- Filed: 2017-02-28
- Published: 2017-09-07
- Earliest claimed: 2016-03-03
- Assignees: SE Tylose GmbH & Co. KG
- Applicants: SE Tylose GmbH & Co. KG
- Inventors: Mike KLEINERT; Diana WISCHANG
- Web page: https://patentgrep.com/patent/US20170253674A1

## CPC

- C08B 11/14: with nitrogen-containing groups
- B05D 1/02: performed by spraying
- C08B 11/145: with basic nitrogen, e.g. aminoalkyl ethers
- C08B 11/193: Mixed ethers, i.e. ethers with two or more different etherifying groups
- C08B: POLYSACCHARIDES; DERIVATIVES THEREOF (polysaccharides containing less than six saccharide radicals attached to each other by glycosidic linkages C07H; fermentation or enzyme-using processes C12P19/00; sugar industry C13; production of cellulose D21)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)

## Abstract

Nonionic, water-soluble cellulose ethers are disclosed with hydroxyalkyl groups and ω-alkynyl groups, each joined to the cellulose via an ether bond, the degree of molar substitution MS(alkyne) being in the range from 0.001 to 0.30. The cellulose ethers may further contain azido groups, preferably 3-azido-2-hydroxypropyl groups, likewise joined to the cellulose by an ether bond, the MS(AHP) being in the range from 0.001 to 0.3. To obtain an adhesive, cellulose ether is mixed with water or. if the cellulose ether contains no alkyne groups, is mixed additionally with a non-ionic cellulose ether containing ω-alkyne groups and hydroxyalkyl groups, each bonded to the cellulose by ether bonds. The mixture is applied to at least one of the surfaces to be bonded and then is contacted with a copper(I) catalyst or a ruthenium catalyst. The adhesive is especially suitable for bonding wood, paper, cardboard or other cellulosic material.

## Claims

### Claim 1

Nonionic, water-soluble cellulose ethers comprising hydroxyalkyl groups and ω-alkynyl groups, each joined to the cellulose via an ether bond, the degree of molar substitution MS(alkyne) being in the range from 0.001 to 0.30.

### Claim 2 (depends on 1)

Cellulose ethers according to claim 1, wherein said cellulose ether further contains azido groups which are joined to the cellulose by an ether bond, the MS(AHP) being in the range from 0.001 to 0.3.

### Claim 2 (depends on 2)

se ethers according to claim 2, wherein the MS(AHP) is in the range from 0.05 to 0.25.

### Claim 3 (depends on 2)

Cellulose ethers according to claim 2, wherein said azido groups are 3-azido-2-hydroxypropyl groups.

### Claim 5 (depends on 1)

Cellulose ethers according to claim 1, wherein said cellulose ether additionally contains alkyl groups joined to the cellulose by an ether bond.

### Claim 6 (depends on 5)

Cellulose ethers according to claim 5, wherein the alkyl groups are straight-chain (C1-C6) alkyl groups.

### Claim 7 (depends on 5)

Cellulose ethers according to claim 5, wherein the alkyl groups are methyl or ethyl groups.

### Claim 8 (depends on 1)

Cellulose ethers according to claim 1, wherein the ω-alkynyl groups have 3 to 6 carbon atoms.

### Claim 9 (depends on 8)

Cellulose ethers according to claim 8, wherein the ω-alkynyl groups are propargyl groups.

### Claim 10 (depends on 1)

Cellulose ethers according to claim 1, wherein the hydroxyalkyl groups are 2-hydroxyethyl or 2-hydroxypropyl groups.

### Claim 11 (depends on 1)

Cellulose ethers according to claim 1, wherein the MS(alkyne) is in the range from 0.05 to 0.25.

### Claim 12 (depends on 1)

Cellulose ethers according to claim 1, wherein the cellulose ether has an average degree of polymerization DPn, determined by the Cuoxam method, of 50 to 4000.

### Claim 13 (depends on 12)

Cellulose ether according to claim 12, wherein the cellulose ether has an average degree of polymerization DPn, by the Cuoxam method, of 1000 to 2500.

### Claim 14 (depends on 12)

Cellulose ethers according to one or more of claim 12, wherein the cellulose ether has an average degree of polymerization DPn, by the Cuoxam method, of 700 to 1500.

### Claim 15 (depends on 1)

Process for preparing a cellulose ether according to claim 1, said process comprising coetherifing a cellulose or a cellulose ether with (i) a hydroxyalkyl component, (ii) an alkyne component, and optionally (iii) with an azide component.

### Claim 16 (depends on 15)

Process for preparing a cellulose ether according to claim 15, wherein (i) the hydroxyalkyl component is ethylene oxide or propylene oxide, (ii) the alkyne component is propargyl bromide, and (iii) the azide component is glycidyl azide.

### Claim 17 (depends on 1)

A method of forming a water-resistant adhesive. bond comprising
(i) mixing a cellulose ether according to claim 1 with water or, if the cellulose ether contains no alkyne groups then additionally mixing the cellulose ether with a non-ionic cellulose ether containing ω-alkyne groups and hydroxyalkyl groups that are each bonded to the cellulose, by ether bonds,
(ii) applying the mixture to at least one surface of the surfaces to be bonded, and
(iii) contacting the surface with a copper(I) catalyst or a ruthenium catalyst.

### Claim 18 (depends on 17)

A method according to claim 17, wherein the surfaces to be bonded consist of wood, paper, cardboard or other cellulosic material.