# US 2017/0253547 A1 · Process for hydroxylation of aromatic compounds, hydroxylation catalyst and process for preparing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253547 A1
- Document ID: US20170253547A1
- Status: Published application
- Kind: A1
- Application number: 15/598,400
- Filed: 2017-05-18
- Published: 2017-09-07
- Earliest claimed: 2012-02-17
- Assignees: Rhodia Operations; Centre National De La Recherche Scientifique (C.N. R.S.)
- Applicants: Rhodia Operations; Centre National De La Recherche Scientifique (C.N.R.S.)
- Inventors: Thibaut Corre; Belen Albela; Laurent Bonneviot; Laurent Garel
- Web page: https://patentgrep.com/patent/US20170253547A1

## CPC

- C07C 37/60: by oxidation reactions introducing directly hydroxy groups on a =CH-group belonging to a six-membered aromatic ring with the aid of other oxidants than molecular oxygen or their mixtures with molecular oxygen
- B01J 29/89: Silicates, aluminosilicates or borosilicates of titanium, zirconium or hafnium {(B01J29/005 takes precedence)}
- B01J 35/45: Nanoparticles
- B01J 35/77: Compounds characterised by their crystallite size
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C01B 37/005: {Silicates, i.e. so-called metallosilicalites or metallozeosilites}
- C01B 39/065: {Galloaluminosilicates; Group IVB- metalloaluminosilicates; Ferroaluminosilicates}
- C01B 39/36: Pentasil type, e.g. types ZSM-5, ZSM-8 or ZSM-11
- C07C 37/58: by oxidation reactions introducing directly hydroxy groups on a =CH-group belonging to a six-membered aromatic ring with the aid of molecular oxygen
- B01J 2235/00: Indexing scheme associated with group B01J35/00, related to the analysis techniques used to determine the catalysts form or properties
- B01J 2235/10: Infrared [IR]
- B01J 2235/15: X-ray diffraction
- B01J 2235/30: Scanning electron microscopy; Transmission electron microscopy
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/12: Surface area
- C01P 2006/16: Pore diameter
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

The present invention relates to a process for hydroxylation of a compound of formula (I) by reacting the compound of formula (I) with an oxidizing agent, in the presence of a titanium silicalite zeolite prepared by crystallization preceded by a maturing step. The present invention also relates to a titanium silicalite zeolite and to the process for preparing same.

## Claims

### Claim at position 1

-11. (canceled)

### Claim 12

A matured TS-1 or TS-2 titano-silicalite zeolite having:
an apparent mean particle size of from 35 to 75 nm,
an outer surface area of from 60 m2/g to 150 m2/g, and
an inter-grain distance of from 10 to 30 nm.

### Claim at position 3

-14. (canceled)

### Claim 15 (depends on 12)

The matured TS-1 or TS-2 titano-silicalite zeolite according to claim 12 further having a specific surface area of between 350 and 600 m2/g.

### Claim 16 (depends on 12)

The matured TS-1 or TS-2 titano-silicalite zeolite according to claim 12 further having a specific surface area of between 400 and 500 m2/g.

### Claim 17 (depends on 12)

The matured TS-1 or TS-2 titano-silicalite zeolite according to claim 12 further having micropores of between 0.40 and 0.50 nm.

### Claim 18 (depends on 12)

The matured TS-1 or TS-2 titano-silicalite zeolite according to claim 12 further having micropores of between 0.44 and 0.46 nm.

### Claim 19 (depends on 12)

The matured TS-1 or TS-2 titano-silicalite zeolite according to claim 12 further having a mole ratio Ti/(Ti+Si) of from 0.0001 to 0.10.

### Claim 20

A process for preparing a TS-1 or TS-2 titano-silicalite zeolite, comprising the following steps:
a) preparation of a zeolite precursor from at least one source of silicon, at least one source of titanium, at least one mineralizing agent and at least one structuring agent;
b) maturation of the zeolite precursor for obtaining a matured precursor;
c) crystallization of the matured precursor for obtaining a matured crystalline precursor, and optionally
d) calcination of the matured crystalline precursor,
wherein said maturation step consists in a step of thermal heating of said zeolite precursor, before crystallization, at a temperature of from 70 to 100° C.

### Claim 21 (depends on 20)

The process according to claim 20, wherein said maturation step consists in a step of thermal heating of said zeolite precursor, before crystallization, at a temperature of 80° C. or 90° C.

### Claim 22 (depends on 20)

The process according to claim 20, wherein the maturation step is performed for a time of from 30 minutes to 9 months.

### Claim 23 (depends on 20)

The process according to claim 20, wherein the maturation step is performed for a time of from 1 hour and 15 days.

### Claim 24 (depends on 20)

The process according to claim 20, wherein the source of titanium is a titanium alkoxide.

### Claim 25 (depends on 20)

The process according to claim 20, wherein the source of silicon is a silicon alkoxide.

### Claim 26 (depends on 20)

A TS-1 or TS-2 titano-silicalite zeolite that may be obtained by the process according to claim 20.

### Claim 27 (depends on 12)

A method for hydroxylating an aromatic compound, wherein said aromatic compound is reacted with an oxidizing agent in the presence of a catalyst, said catalyst being a TS-1 or TS-2 titano-silicalite zeolite according to claim 12.

### Claim 28 (depends on 15)

A method for hydroxylating an aromatic compound, wherein said aromatic compound is reacted with an oxidizing agent in the presence of a catalyst, said catalyst being a TS-1 or TS-2 titano-silicalite zeolite according to claim 15.