# US 2017/0253537 A1 · Method of producing solid propellant element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253537 A1
- Document ID: US20170253537A1
- Status: Published application
- Kind: A1
- Application number: 15/057,587
- Filed: 2016-03-01
- Published: 2017-09-07
- Earliest claimed: 2016-03-01
- Assignees: Raytheon Company
- Applicants: Raytheon Company
- Inventors: Jeremy C. Danforth; Matt H. Summers; David G. Garrett
- Web page: https://patentgrep.com/patent/US20170253537A1

## CPC

- C06B 21/0075: {by extrusion}
- B29C 64/106: using only liquids or viscous materials, e.g. depositing a continuous bead of viscous material
- C06B 21/0083: {Treatment of solid structures, e.g. for coating or impregnating with a modifier (compositions therefor C06B23/00)}
- C06B 45/00: Compositions or products which are defined by structure or arrangement of component of product (explosive charges of particular form or shape F42B1/00, F42B3/00)
- F02K 9/08: using solid propellants (F02K9/72 takes precedence; using semi-solid or pulverulent propellants F02K9/70)
- F02K 9/10: Shape or structure of solid propellant charges
- F02K 9/14: made from sheet-like materials, e.g. of carpet-roll type, of layered structure
- B33Y 10/00: Processes of additive manufacturing
- F05D 2230/24: by extrusion
- C06B: EXPLOSIVES OR THERMIC COMPOSITIONS (blasting F42D); MANUFACTURE THEREOF; USE OF SINGLE SUBSTANCES AS EXPLOSIVES (compounds in general C01, C07 or C08; {demolition agents based on cementitious or like materials C04B41/0009})
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- F02K: JET-PROPULSION PLANTS (features of jet-propulsion plants common to gas-turbine plants, air intakes or fuel supply control of air-breathing jet-propulsion plants F02C7/00, F02C9/00)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS

## Abstract

A method of producing a propellant material element, such as an electrically-operated propellant material, includes extruding a propellant material through a heated nozzle. The nozzle may be heated to a temperature that is above the boiling point of a solvent that is part of the propellant material, yet is below a decomposition temperature of the propellant material. This allows some of the solvent to be driven off during the extruding process, while still preventing initiation of an energy-creating reaction within the material. The heating of the material in the extruding process, and especially the heating of the nozzle that the material is extruded through, may be controlled to remove an amount of solvent that results in the extruded material having desirable properties.

## Claims

### Claim 1

A method of additively manufacturing a solid propellant element, the method comprising:
heating a nozzle to produce a heated nozzle; and
extruding through the heated nozzle a propellant material that includes a solvent, to form the solid propellant element;
wherein the extruding occurs when the heated nozzle is at a temperature that above a boiling point of the solvent and below a decomposition temperature of the propellant material; and
wherein the extruding removes some of the solvent from the propellant material.

### Claim 2 (depends on 1)

The method of claim 1,
wherein the solvent is water and/or glycerol; and
wherein the extruding through the heated nozzle removes some of the water and/or glycerol from the propellant material.

### Claim 3 (depends on 1)

The method of claim 1, wherein the extruding includes extruding through a heated nozzle that is between 100 and 210 degrees C.

### Claim 4 (depends on 3)

The method of claim 3, wherein the extruding includes extruding through a heated nozzle that is between 150 and 210 degrees C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the extruding includes directing the propellant material from a reservoir of the propellant material, to the heated nozzle.

### Claim 6 (depends on 5)

The method of claim 5, wherein the directing includes using a stepper motor to control flow of the propellant material from the reservoir to the heated nozzle.

### Claim 7 (depends on 6)

The method of claim 6, wherein the using includes using software to control the stepper motor.

### Claim 8 (depends on 1)

The method of claim 1,
wherein the propellant material is an electrically-operated propellant material; and
wherein the extruding produces an electrically-operated solid propellant element as the solid propellant element.

### Claim 9 (depends on 1)

The method of claim 1, wherein the extruding, by removing some of the solvent from the propellant material, makes the propellant material suitable for curing into the propellant element.

### Claim 10 (depends on 1)

The method of claim 1, wherein the propellant element is built up in layers on a platform, by the extruding.

### Claim 11 (depends on 10)

The method of claim 10, wherein the platform is a heated platform.

### Claim 12 (depends on 10)

The method of claim 10, wherein the layers each have a thickness of on the order of 0.1 mm.

### Claim 13 (depends on 1)

The method of claim 1, wherein the extruding is performed in a heated chamber.

### Claim 14 (depends on 1)

The method of claim 1, further comprising embedding one or more devices in the propellant element during the extruding.

### Claim 15 (depends on 14)

The method of claim 14,
wherein the propellant material is an electrically-operated propellant material; and
wherein the embedding includes embedding electrodes as at least some of the one or more devices.

### Claim 16 (depends on 1)

The method of claim 1,
further comprising, prior to the heating and the extruding, mixing the propellant material, combining together a fuel, the solvent, an oxidizer, and a binder;
wherein the mixing includes combining an excess amount of the solvent, beyond that that would be used to form a cast or molded cured propellant element.

### Claim 17 (depends on 1)

The method of claim 1, wherein the extruding includes extruding the propellant material in a partially cured state.