# US 2017/0253526 A1 · Axial compression steel tubular column with internal local restraint and filled with high strengthen compound concrete containing normal-strength demolished concrete lumps and construction process of such column

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253526 A1
- Document ID: US20170253526A1
- Status: Published application
- Kind: A1
- Application number: 15/512,068
- Filed: 2014-10-24
- Published: 2017-09-07
- Earliest claimed: 2014-09-17
- Assignees: South China University of Technology
- Applicants: South China University of Technology
- Inventors: Bo WU; Qiang ZHANG
- Web page: https://patentgrep.com/patent/US20170253526A1

## CPC

- C04B 18/167: Recycled materials, i.e. waste materials reused in the production of the same materials
- C04B 28/02: containing hydraulic cements other than calcium sulfates
- E04C 3/34: of concrete other stone-like material, with or without permanent form elements, with or without internal or external reinforcement, e.g. metal coverings (E04C3/36 takes precedence)
- E04C 3/36: of materials not covered by groups E04C3/32 or E04C3/34; of a combination of two or more materials
- C04B 18/04: Waste materials; Refuse
- E04C 3/30: Columns; Pillars; Struts (not designed for end loading E04C3/02; posts, masts, as independent structures E04H12/00)
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- E04C: STRUCTURAL ELEMENTS; BUILDING MATERIALS (for bridges E01D; specially designed for insulation or other protection E04B; elements used as building aids E04G; for mining E21; for tunnels E21D; structural elements with broader range of application than for building engineering F16, particularly F16S)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

An axial compression steel tubular column with internal local restraint and filled with high strengthen compound concrete containing normal-strength demolished concrete lumps and a construction process. The axial compression column includes a steel tube (1), high-strength fresh concrete (2), normal-strength demolished concrete lumps (3), a spiral stirrup (4), and longitudinal erection bars (6). The spiral stirrup (4) is arranged at a middle part inside the steel tube (1). The high-strength fresh concrete (2) is poured and the normal-strength demolished concrete lumps (3) are put alternately inside the steel tube (1). A compressive strength of the high-strength fresh concrete (2) is 30˜90 MPa greater than that of the normal-strength demolished concrete lumps (3).

## Claims

### Claim 1

An axial compression steel tubular column with internal local restraint and filled with high strengthen compound concrete containing normal-strength demolished concrete lumps, characterized in that: a spiral stirrup or a plurality of horizontal stirrups are provided in three-fifths of a height range at a middle part in a steel tube, and high-strength fresh concrete is poured and normal-strength demolished concrete lumps are put alternately inside the steel tube, with a compressive strength of the high-strength fresh concrete being 30-90 MPa greater than that of the normal-strength demolished concrete.

### Claim 2 (depends on 1)

The axial compression steel tubular column with internal local restraint and filled with high strengthen compound concrete containing normal-strength demolished concrete lumps according to claim 1, wherein the spiral stirrup is arranged in three-fifths of a height range at the middle part in the steel tube, with a section of the steel tube being circular; or the horizontal stirrups are arranged in three-fifths of a height range at the middle part in the steel tube, which are dense in the middle and sparse on both sides, with a section of the steel tube being circular or polygonal.

### Claim 3 (depends on 1)

The axial compression steel tubular column with internal local restraint and filled with high strengthen compound concrete containing normal-strength demolished concrete lumps according to claim 1, wherein the normal-strength demolished concrete lumps are waste concrete lumps after demolishing old buildings, structures, roads, bridges or dams and removing protective layers and all or part of steel reinforcements.

### Claim 4 (depends on 1)

The axial compression steel tubular column with internal local restraint and filled with high strengthen compound concrete containing normal-strength demolished concrete lumps according to claim 1, wherein the high-strength fresh concrete is a natural aggregate concrete or a recycled aggregate concrete, and has a compressive strength no less than 60 MPa.

### Claim 5 (depends on 1)

The axial compression steel tubular column with internal local restraint and filled with high strengthen compound concrete containing normal-strength demolished concrete lumps according to claim 1, wherein the normal-strength demolished concrete lump has a characteristic size no less than 100 mm, and a mass ratio of the normal-strength demolished concrete lump and the high-strength fresh concrete is 1:4˜1:1.

### Claim 6 (depends on 1)

A construction process of the axial compression steel tubular column with internal local restraint and filled with high strengthen compound concrete containing normal-strength demolished concrete lumps according to claim 1, characterized in that, it comprises following steps:
(1) spot welding a spiral stirrup or a plurality of horizontal stirrups and two longitudinal erection bars into one, then lifting the two longitudinal erection bars, arranging the spiral stirrup or the plurality of horizontal stirrups in three-fifths of a height range at a middle part in a steel tube, with a stirrup distance being that the stirrups are dense in the middle and sparse on both sides when horizontal stirrup is adopted, then spot welding the two longitudinal erection bars with an inner wall of the steel tube;
(2) fully wetting normal-strength demolished concrete lumps in advance, when putting, pouring high-strength fresh concrete with about 20 mm thickness into a bottom of the steel tube first, then alternately putting wet normal-strength demolished concrete lumps and the high-strength fresh concrete inside the steel tube and fully vibrating until pouring is finished, so that the normal-strength demolished concrete lumps and the high-strength fresh concrete are uniformly mixed into one.