# US 2017/0253487 A1 · Electrode active composite materials and methods of making thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0253487 A1
- Document ID: US20170253487A1
- Status: Published application
- Kind: A1
- Application number: 15/597,314
- Filed: 2017-05-17
- Published: 2017-09-07
- Earliest claimed: 2009-05-04
- Assignees: Meecotech, Inc.
- Applicants: Meecotech, Inc.
- Inventors: Tao Gu
- Web page: https://patentgrep.com/patent/US20170253487A1

## CPC

- C01B 25/45: containing plural metal, or metal and ammonium
- C01B 25/37: Phosphates of heavy metals
- H01M 4/366: {as layered products}
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/625: {Carbon or graphite}
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- Y02E 60/10: Energy storage using batteries
- Y10T 428/2982: Particulate matter [e.g., sphere, flake, etc.]
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method of synthesizing a lithium metal phosphate composite usable for a lithium secondary battery includes the steps of forming a nanometer-size precursor comprising lithium source and metal phosphate nanoparticles having each nanoparticle at least partially coated a layer of carbon precursor, spray drying the nanometer-size precursor at a first desired temperature to form micron-size particles packed with the lithium metal phosphate precursor nanoparticles, and sintering the micron-size particles at a second desired temperature under an inert and/or reduction atmosphere to form a micron-size lithium metal phosphate composite.

## Claims

### Claim 1

A method of synthesizing a lithium iron phosphate composite usable for a lithium secondary battery, comprising the steps of:
providing a first solution and a second solution, wherein the first solution comprises ferric chloride hexahydrate dissolved in water, and wherein the second solution comprises diammonium hydrogen phosphate and pyrrole dissolved in water;
drop-wisely adding the first solution into the second solution with stirring to form a first mixture;
stirring the first mixture for a first period of time;
filtering and rinsing the stirred mixture with water to obtain solid substances;
forming a composite of FePO4 and carbon precursor from the solid substances;
mixing an equivalent mole of a lithium compound and a sucrose with the FePO4 composite to form a second mixture;
ball-milling the second mixture for a second period of time to form a lithium iron phosphate precursor comprising nanometer-sized particles; and
sintering the lithium iron phosphate precursor under an argon and hydrogen gas mixture at a first temperature for a third period of time to form a lithium iron phosphate composite.

### Claim 2 (depends on 1)

The method of claim 1, wherein the lithium compound comprises Li2CO3.

### Claim 3 (depends on 1)

The method of claim 1, wherein the lithium iron phosphate precursor is formed with Li:Fe:P=1:1:1 by mole ratio.

### Claim 4 (depends on 1)

The method of claim 1, wherein the argon and hydrogen gas mixture comprises about 95% argon and about 5% hydrogen by volume.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first temperature is in a range of about 500-1200° C.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first period of time, the second period of time and the third period of time are respectively in ranges of about 1-10 hours, about 18-30 hours and about 5-24 hours.

### Claim 7 (depends on 1)

The method of claim 1, wherein the forming step comprises the steps of:
drying the solid substances at a second temperature for a fourth period of time;
heating the dried solid substances to a third temperature under argon for a fifth period of time, and cooling it to the room temperature to form the composite of FePO4 and carbon precursor.

### Claim 8 (depends on 7)

The method of claim 7, wherein the second temperature and the third temperature are respectively in ranges of about 20-150° C. and about 20-500° C.

### Claim 9 (depends on 7)

The method of claim 7, wherein the fourth period of time and the fifth period of time are respectively in ranges of about 6-18 hours and about 1-3 hours.

### Claim 10 (depends on 1)

The method of claim 1, wherein the lithium iron phosphate composite comprises a micron-size composite that is packed with a plurality of nanometer-sized LiFePO4 particles.

### Claim 11 (depends on 1)

The method of claim 1, wherein the lithium iron phosphate composite has a tap density that is in a range of about 0.5 to 3 g/cm3.

### Claim 12 (depends on 1)

A lithium iron phosphate composite synthesized according to the method of claim 1.

### Claim 13

A method of synthesizing a lithium metal phosphate composite usable for a lithium secondary battery, comprising the steps of:
forming a nanometer-size precursor comprising lithium source and metal phosphate nanoparticles having each nanoparticle at least partially coated a layer of carbon precursor;
spray drying the nanometer-size precursor at a first desired temperature to form micron-size particles packed with the lithium metal phosphate precursor nanoparticles; and
sintering the micron-size particles at a second desired temperature under an inert and/or reduction atmosphere to form a micron-size lithium metal phosphate composite.

### Claim 14 (depends on 13)

The method of claim 13, wherein the first desired temperature and the second temperature are respectively in ranges of about 20-500° C. and about 500-1200° C.

### Claim 15 (depends on 13)

The method of claim 13, wherein the inert and/or reduction atmosphere comprises an argon and hydrogen gas mixture.

### Claim 16 (depends on 13)

The method of claim 13, wherein the layer of carbon precursor comprises at least one of carbonaceous materials, and is coated through in situ oxidation polymerization during the formation of the nanometer-size metal phosphate nanoparticles.

### Claim 17 (depends on 13)

The method of claim 13, wherein the metal comprises a transitional metal or a mixture of transition metals.

### Claim 18 (depends on 17)

The method of claim 17, wherein the transitional metal comprises Fe, Mn, V, Co, Ni, or a combination of them, and preferably comprises Fe.

### Claim 19 (depends on 17)

The method of claim 17, wherein the metal comprises optionally at least one non-transition metal.

### Claim 20 (depends on 13)

A lithium metal phosphate composite synthesized according to the method of claim 13.