# US 2017/0250308 A1 · Crystal substrate, ultraviolet light-emitting device, and manufacturing methods therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0250308 A1
- Document ID: US20170250308A1
- Status: Published application
- Kind: A1
- Application number: 15/442,554
- Filed: 2017-02-24
- Published: 2017-08-31
- Earliest claimed: 2016-02-26
- Assignees: Riken
- Applicants: Riken
- Inventors: Masafumi JO; Hideki HIRAYAMA
- Web page: https://patentgrep.com/patent/US20170250308A1

## CPC

- H10H 20/815: having stress relaxation structures, e.g. buffer layers
- C30B 25/183: {being provided with a buffer layer, e.g. a lattice matching layer}
- C30B 29/403: {AIII-nitrides}
- H10H 20/01335: {the light-emitting regions comprising nitride materials}
- H10H 20/818: within the light-emitting regions
- H10H 20/82: Roughened surfaces, e.g. at the interface between epitaxial layers
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

To fabricate a practically useful non-polar AlN buffer layer on a sapphire crystal plate and manufacture a UV light-emitting device on a non-polar crystal substrate by adopting the crystal substrate as an example, an embodiment of the present invention provides a crystal substrate 1D comprising an r-plane sapphire crystal plate 10 and an AlN buffer layer 20D of non-polar orientation. The AlN buffer layer comprises a surface protection layer 22 and a smoothing layer 26. The surface protection layer suppresses roughness increase on a surface of the AlN buffer layer, and the smoothing layer makes the surface of the AlN buffer layer a smoothed surface. Also provided is a crystal substrate 11 comprising an AlN buffer layer 20T to which a dislocation blocking layer 24 for reducing crystallographic defects is added between the surface protection layer 22 and the smoothing layer 26. In another embodiment a deep UV light-emitting device is provided.

## Claims

### Claim 1

A crystal substrate comprising:
a sapphire crystal plate of an r-plane orientation; and
an AlN buffer layer of a non-polar orientation covering at least a part of a surface of the sapphire crystal plate,
wherein the AlN buffer layer comprises first a surface protection layer and above it a smoothing layer, both of which are epitaxially grown layers made of AlN crystal, in this order from the sapphire crystal plate side,
wherein the surface protection layer is configured to suppress roughness on a surface of the AlN buffer layer, and
wherein the smoothing layer is configured to provide a smoothed upper surface for a surface of the AlN buffer.

### Claim 2 (depends on 1)

The crystal substrate according to claim 1,
wherein the AlN buffer layer comprises a dislocation blocking layer that is an epitaxially grown layer made of AlN crystal disposed between the surface protection layer and the smoothing layer, and
wherein the dislocation blocking layer has a sufficient thickness for reducing a number of crystallographic defects through the AlN buffer layer.

### Claim 3 (depends on 1)

The crystal substrate according to claim 1,
wherein the smoothing layer has a root-mean-square (RMS) roughness of 10 nm or below on at least a part of a surface thereof, where the RMS roughness, Rq, is defined as:
Rq=(Σi(zi−zave)2)1/2/N,
where N is a total number of measurement points in a measurement area,
zi is a height value at each measurement point, identified by an index i, in the measurement area,
zave is an average value of zi over the measurement area, and
Σi stands for a summation operation through the indices i.

### Claim 4 (depends on 2)

The crystal substrate according to claim 2,
wherein the surface protection layer has an island structure on a surface thereof, and
wherein the thickness of the dislocation block layer is a sufficient value for burying the island structure.

### Claim 5 (depends on 2)

The crystal substrate according to claim 2,
wherein the dislocation blocking layer has a thickness of 1 μm or above,
wherein the dislocation blocking layer is configured to reduce density of threading dislocations extending through the AlN buffer layer to the smoothed surface.

### Claim 6 (depends on 2)

The crystal substrate according to claim 2,
wherein the AlN buffer layer has such a crystalline quality that a peak of an ω-scan mode X-ray rocking curve has a full-width half maximum value of 1000 arcsec or below for c-axis direction on a (11-20) plane.

### Claim at position 7

7-11. (canceled)

### Claim 12

A method for manufacturing a crystal substrate of a non-polar orientation comprising the steps of:
providing a sapphire crystal plate of an r-plane orientation; and
forming a buffer layer of an AlN buffer layer, so that the AlN buffer layer covers at least a part of a surface of the sapphire crystal plate, the AlN buffer layer being an epitaxially grown layer of AlN crystal of a non-polar orientation,
wherein the step of forming a buffer layer comprises the steps of:
forming a surface protection layer by epitaxially growing a surface protection layer that suppresses roughness on a surface of the AlN buffer layer; and
smoothing by epitaxially growing a smoothing layer on the surface protection layer for providing a surface of the AlN buffer with a smoothed upper surface.

### Claim 13 (depends on 12)

The method for manufacturing a crystal substrate according to claim 12,
wherein the step of forming a buffer layer further comprises a step of forming a dislocation blocking layer that reduces a number of crystallographic defects through the AlN buffer layer between the steps of forming a surface protection layer and smoothing, and
wherein the step of smoothing is epitaxially growing the smoothing layer over the dislocation blocking layer, so that the smoothing layer covers at least a part of the surface protection layer via the dislocation blocking layer.

### Claim 14 (depends on 12)

The method for manufacturing a crystal substrate according to claim 12,
wherein the step of forming a surface protection layer is carried out by an MOCVD method at a growth temperature that is below a temperature at which a surface of the r-plane of the sapphire crystal plate may be roughened, and
wherein the step of smoothing is carried out by an MOCVD method at a growth temperature that reaches or exceeds a temperature necessary for smoothing, where the temperature necessary for smoothing is identical to or above the growth temperature for the step of the surface protection layer.

### Claim 15 (depends on 14)

The method for manufacturing a crystal substrate according to claim 14,
wherein the growth temperature for the step of forming a surface protection layer is 1200° C. or below, and
wherein the growth temperature for the step of smoothing is 1400° C. or above.

### Claim 16 (depends on 13)

The method for manufacturing a crystal substrate according to claim 13,
wherein the step of forming a surface protection layer is carried out by an MOCVD method at a growth temperature that is below a temperature at which the r-plane of the sapphire crystal plate may be roughened,
wherein the step of forming a dislocation blocking layer is carried out by an MOCVD method,
wherein the step of smoothing is carried out by an MOCVD method at a growth temperature that reaches or exceeds a temperature necessary for smoothing, where the temperature necessary for smoothing is identical to or above the growth temperature for the step of forming a surface protection layer, and
wherein the MOCVD method for the step of forming a dislocation blocking layer is carried out at a temperature that is identical or above the growth temperature for the step of forming a surface protection layer and below the growth temperature for the step of smoothing.

### Claim 17 (depends on 16)

The method for manufacturing a crystal substrate according to claim 16,
wherein the growth temperature for the step of forming a surface protection layer is 1200° C. or below,
wherein the growth temperature for the step of smoothing is 1400° C. or above, and
wherein the temperature for the step of forming a dislocation blocking layer is identical to or above the growth temperature for the step of forming a surface protection layer and is 1300° C. or below.

### Claim 18 (depends on 12)

The method for manufacturing a crystal substrate according to claim 12,
wherein the step of forming a surface protection layer is carried out with a V/III ratio in a range within which an island structure is formed on a surface of the surface protection layer.

### Claim 19 (depends on 12)

The method for manufacturing a crystal substrate according to claim 12,
wherein the smoothing step is carried out with a V/III ratio in a range within which formation of a wave structure and formation of void-like structural defects on a surface of the smoothing layer are both avoided.

### Claim 20

A method for manufacturing an ultraviolet light emitting device on a crystal substrate comprising steps of:
providing a crystal substrate having a non-polar AlN surface; and
forming a group-III nitride semiconductor crystal layer by epitaxially growing an ultraviolet (UV) emission layer of a non-polar plane on at least a part of the non-polar AlN surface of the crystal substrate, the UV emission layer comprising an n-type conduction layer, a recombination layer, and a p-type conduction layer in this order from the crystal substrate side, all of which are made of group-III nitride semiconductor crystal; and
forming a reflective electrode by disposing a reflective electrode directly or indirectly via another layer on the p-type conductive layer, the reflective electrode having a reflection capability for UV radiation that is an ultraviolet light from the UV emission layer.

### Claim 21 (depends on 20)

The method for manufacturing an ultraviolet light emitting device according to claim 20,
wherein the group-III nitride semiconductor crystal includes a plurality of layers with a mixed crystal of AlN and GaN of different composition ratios,
wherein the step of forming a group-III nitride semiconductor crystal layer is a step of performing growth by an MOCVD method at a temperature over 1200° C., while securing flatness through the growth, and
wherein the step of forming a group-III nitride semiconductor crystal layer comprises a step of controlling the composition ratios by increasing or decreasing a partial pressure of ammonia in material gas for the MOCVD method.

### Claim 22 (depends on 20)

The method for manufacturing an ultraviolet light emitting device according to claim 20,
wherein the group-III nitride semiconductor crystal includes a plurality of layers with a mixed crystal of AlN and GaN of different composition ratios,
wherein the step of forming a group-III nitride semiconductor crystal layer is a step of performing growth by an MOCVD method at a temperature over 1200° C., while securing flatness through the growth, and
wherein the step of forming a group-III nitride semiconductor crystal layer comprises a step of controlling the composition ratios by adjusting material supply ratios while a partial pressure of ammonia in raw material gas for the MOCVD method is so increased that the composition ratios may be modulated by the material supply ratios between aluminum and gallium in raw material gas at the temperature.

### Claim 23 (depends on 20)

The method for manufacturing an ultraviolet light emitting device according to claim 20,
wherein the step of providing the crystal substrate comprises a step of forming a buffer layer by forming an AlN buffer layer, so that the AlN buffer layer covers at least a part of a surface of a sapphire crystal plate of an r-plane orientation,
wherein the step of forming a buffer layer includes steps of:
forming a surface protection layer by epitaxially growing a surface protection layer configured to suppress roughness increase on a surface of the non-polar AlN surface; and
smoothing by epitaxially growing a smoothing layer for providing a smoothed surface for the non-polar AlN surface, and
wherein the non-polar AlN surface corresponds to the surface of the AlN buffer layer.

### Claim 24 (depends on 23)

The method for manufacturing an ultraviolet light emitting device according to claim 23,
wherein the step of forming a buffer layer further comprises a step of forming a dislocation blocking layer for reducing a number of crystallographic defects by epitaxially growing a dislocation blocking layer between the step of forming a surface protection layer and the step of smoothing, and
wherein the step of forming a surface protection layer is epitaxially growing the smoothing layer over the dislocation blocking layer, so that the smoothing layer covers at least a part of the surface protection layer via the dislocation blocking layer.