# US 2017/0250193 A1 · Method of manufacturing three-dimensional semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0250193 A1
- Document ID: US20170250193A1
- Status: Published application
- Kind: A1
- Application number: 15/311,000
- Filed: 2014-07-10
- Published: 2017-08-31
- Earliest claimed: 2014-05-16
- Assignees: Institute of Microelectronics, Chinese Academy of Sciences
- Applicants: Institute of Microelectronics, Chinese Academy of Sciences
- Inventors: Zongliang HUO
- Web page: https://patentgrep.com/patent/US20170250193A1

## CPC

- H10B 43/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10D 64/037: {comprising charge-trapping insulators}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10P 95/906: {for altering the shape of semiconductors, e.g. smoothing the surface}
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing three-dimensional semiconductor device, comprising the steps of: forming a stack structure of a plurality of a first material layers and a second material layers on a substrate in the memory cell region; etching said stack structure to form a plurality of trenches; forming channel layers in said plurality of trenches; performing annealing treatment to at least one surface of the channel layers to reduce the surface roughness and the interface state. In accordance with the three-dimensional semiconductor device manufacturing method of the present invention, the formation of interface states is depressed by introducing a dummy channel sacrificial layer for the interface treatment on the channel surface and back surface, and/or the channel surface roughness is reduced by introducing a buffer layer on the channel surface and back surface during the treatment, which can improve the channel carrier mobility, improve the channel current as well as the reliability of the memory cell.

## Claims

### Claim 1

A method of manufacturing three-dimensional semiconductor device, comprising the steps of:
forming a stack structure of a plurality of a first material layers and a second material layers on a substrate in the memory cell region;
etching said stack structure to form a plurality of trenches;
forming channel layers in said plurality of trenches;
performing annealing treatment to at least one surface of the channel layers to reduce the surface roughness and the interface state.

### Claim 2 (depends on 1)

The method of manufacturing three-dimensional semiconductor device of claim 1, wherein, before forming said channel layers, further comprising forming a dummy channel sacrificial layer on the sidewalls of said plurality of trenches.

### Claim 3 (depends on 2)

The method of manufacturing three-dimensional semiconductor device of claim 2, wherein, the material of said dummy channel sacrificial layer comprises silicon nitride, silicon oxynitride or combinations thereof, and having a high etching selectivity ratio to the material of the first material layers and/or the second material layers.

### Claim 4 (depends on 1)

The method of manufacturing three-dimensional semiconductor device of claim 1, wherein, after forming said channel layers but before said annealing treatment, further comprising forming a buffer layer on at least one surface of said channel layers.

### Claim 5 (depends on 4)

The method of manufacturing three-dimensional semiconductor device of claim 4, wherein, the material of the buffer layer includes silicon oxide, silicon nitride, silicon oxynitride, or combinations thereof.

### Claim 6 (depends on 4)

The method of manufacturing three-dimensional semiconductor device of claim 4, wherein, said buffer layer is formed on the surface of said channel layers facing towards and/or back away from said stack structure.

### Claim 7 (depends on 1)

The method of manufacturing three-dimensional semiconductor device of claim 1, wherein, said annealing treatment is performed at a gas atmosphere containing nitrogen group, fluoro group, chloro group, bromo group, or combinations thereof.

### Claim 8 (depends on 1)

The method of manufacturing three-dimensional semiconductor device of claim 1, wherein, after the surface of the channel layer facing back away from said stack structure is annealed, filling the channel layers with an insulating spacer layer and forming drain regions of the device transistor.

### Claim 9 (depends on 8)

The method of manufacturing three-dimensional semiconductor device of claim 8, wherein, after forming said drain regions, further comprising selectively removing the second material layers, leaving a plurality of discrete vertical stack structures on the substrate, exposing the surface of the channel layers facing towards said first material layers.

### Claim 10 (depends on 9)

The method of manufacturing three-dimensional semiconductor device of claim 9, wherein, the surface of the channel layers facing towards said first material layers are annealed.

### Claim 11 (depends on 10)

The method of manufacturing three-dimensional semiconductor device of claim 10, wherein, before the annealing treatment of the surface of the channel layers facing towards said first material layers, further comprising forming a buffer layer on the surface of the channel layers facing towards said first material layers.

### Claim 12 (depends on 1)

The method of manufacturing three-dimensional semiconductor device of claim 1, wherein, after said annealing treatment to at least one surface of the channel layers, further comprising forming a plurality of lateral recesses on sidewalls of said plurality of trenches in said stack structure, and then forming a plurality of gate stack structures composed of a gate dielectric layer and a gate conductive layer in said plurality of recesses; forming a plurality of source regions in said substrate.

### Claim 13 (depends on 12)

The method of manufacturing three-dimensional semiconductor device of claim 12, wherein, said gate dielectric layer further comprises a tunneling layer, a storage layer and a barrier layer.

### Claim 14 (depends on 12)

The method of manufacturing three-dimensional semiconductor device of claim 12, wherein, between said gate dielectric layer and said gate conductive layer a metal nitride layer may be included.

### Claim 15 (depends on 1)

The method of manufacturing three-dimensional semiconductor device of claim 1, wherein, the cross-sectional shape of the channel layers parallel to the substrate surface comprises geometric shapes selected from rectangular, square, diamond, circular, semi-circular, elliptical, triangular, pentagonal, hexagonal, octagonal and the combinations thereof, and includes those selected from solid geometry, hollow annular geometry, or a combination of a hollow annular peripheral layer and a central insulating layer as a result of revolution of geometric shapes.

### Claim 16 (depends on 1)

The method of manufacturing three-dimensional semiconductor device of claim 1, wherein, both of the materials of said first material layers and said second material layers include insulating material, furthermore the first material layers have a first etch selectivity, and the second material layers have a second etch selectivity which is different from the first etch selectivity.

### Claim 17 (depends on 1)

The method of manufacturing three-dimensional semiconductor device of claim 1, wherein, the material of the first material layers comprise insulating material, the material of the second material layers may comprise doped semiconductor material or conductive material used to form control gates.