# US 2017/0248860 A1 · Electrostatic latent image developing toner

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0248860 A1
- Document ID: US20170248860A1
- Status: Published application
- Kind: A1
- Application number: 15/439,970
- Filed: 2017-02-23
- Published: 2017-08-31
- Earliest claimed: 2016-02-25
- Assignees: KYOCERA Document Solutions Inc.
- Applicants: KYOCERA Document Solutions Inc.
- Inventors: Haruhiro NISHITERA; Tomoyasu ASAKAWA
- Web page: https://patentgrep.com/patent/US20170248860A1

## CPC

- G03G 9/09321: {obtained by reactions only involving carbon-to-carbon unsaturated bonds}
- G03G 9/0819: {characterised by the dimensions of the particles}
- G03G 9/0825: {characterised by their structure; characterised by non-homogenuous distribution of components (microcapsular toners G03G9/093)}
- G03G 9/0935: {specified by the core material}
- G03G 9/09371: {obtained otherwise than by reactions only involving carbon-to-carbon unsaturated bonds}
- G03G 9/09392: {Preparation thereof}
- G03G 9/09716: {treated with organic compounds}
- G03G 9/09725: {Silicon-oxides; Silicates}
- G03G 9/09733: {Organic compounds (G03G9/08782 takes precedence)}
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

An electrostatic latent image developing toner includes a plurality of toner particles each including a core containing a binder resin and a shell layer covering a surface of the core. The shell layer contains a copolymer of at least two vinyl compounds including a compound represented by the following formula (1). The toner contains a ring unopened oxazoline group in an amount of at least 0.10 μmol/g and no greater than 100 μmol/g.

## Claims

### Claim 1

An electrostatic latent image developing toner comprising a plurality of toner particles each including a core containing a binder resin and a shell layer covering a surface of the core, wherein
the shell layer contains a copolymer of at least two vinyl compounds including a compound represented by formula (1) shown below, and
the toner contains a ring unopened oxazoline group in an amount of at least 0.10 μmol/g and no greater than 100 μmol/g:
where, in the formula (1), R1 represents a hydrogen atom or an optionally substituted alkyl group.

### Claim 2 (depends on 1)

The electrostatic latent image developing toner according to claim 1, wherein
the at least two vinyl compounds include at least one vinyl compound selected from the group consisting of styrene-based monomers and acrylic acid-based monomers.

### Claim 3 (depends on 1)

The electrostatic latent image developing toner according to claim 1, wherein
the copolymer contained in the shell layer is a copolymer of monomers including the at least one compound represented by the formula (1) and at least one (meth)acrylic acid alkyl ester.

### Claim 4 (depends on 1)

The electrostatic latent image developing toner according to claim 1, wherein
the toner particles each include a toner mother particle and an external additive, the toner mother particle including the core and the shell layer, the external additive being attached to a surface of the toner mother particle, and
the external additive contains a resin powder that is a powder of crosslinked resin particles having a glass transition point of at least 100° C.

### Claim 5 (depends on 4)

The electrostatic latent image developing toner according to claim 4, wherein
the external additive contains the resin powder and an inorganic powder that is a powder of inorganic particles, and
the resin powder and the inorganic powder constitute a stacked structure in order of the resin powder and the inorganic powder from a side of the toner mother particle.

### Claim 6 (depends on 5)

The electrostatic latent image developing toner according to claim 5, wherein
the resin powder has a number average primary particle diameter of at least 70 nm and no greater than 95 nm, and
the inorganic powder includes a powder of silica particles having a number average primary particle diameter of at least 5 nm and no greater than 40 nm.

### Claim 7 (depends on 6)

The electrostatic latent image developing toner according to claim 6, wherein
the resin powder is present in an amount of at least 0.5 parts by mass and no greater than 5.0 parts by mass relative to 100 parts by mass of the toner mother particles, and
the powder of the silica particles is present in an amount of at least 0.5 parts by mass and no greater than 5.0 parts by mass relative to 100 parts by mass of the toner mother particles.

### Claim 8 (depends on 5)

The electrostatic latent image developing toner according to claim 5, wherein
the shell layers cover at least 70% and no greater than 80% of a total surface area of the toner cores.

### Claim 9 (depends on 6)

The electrostatic latent image developing toner according to claim 6, wherein
the crosslinked resin particles having a glass transition point of at least 100° C. contain a crosslinked acrylic acid-based resin.

### Claim 10 (depends on 9)

The electrostatic latent image developing toner according to claim 9, wherein
the core contains a polyester resin as the binder resin.

### Claim 11 (depends on 10)

The electrostatic latent image developing toner according to claim 10, wherein
the polyester resin is a condensation polymer of at least one aromatic dibasic carboxylic acid and at least one aliphatic diol having a carbon number of at least 2 and no greater than 4.

### Claim 12 (depends on 10)

The electrostatic latent image developing toner according to claim 10, wherein
the core is a pulverized core.