# US 2017/0247536 A1 · Thermoplastic Vulcanizate with Crosslinked Olefin Block Copolymer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0247536 A1
- Document ID: US20170247536A1
- Status: Published application
- Kind: A1
- Application number: 15/592,859
- Filed: 2017-05-11
- Published: 2017-08-31
- Earliest claimed: 2015-06-12
- Assignees: Dow Global Technologies LLC
- Applicants: Dow Global Technologies LLC
- Inventors: Shuwen Peng; Yabin Sun; Mahalia Soediono; Shih-Yaw Lai
- Web page: https://patentgrep.com/patent/US20170247536A1

## CPC

- C08L 53/00: Compositions of block copolymers containing at least one sequence of a polymer obtained by reactions only involving carbon-to-carbon unsaturated bonds; Compositions of derivatives of such polymers
- C08K 5/3435: Piperidines
- C08L 23/142: {at least partially crystalline copolymers of propene with other olefins}
- C08L 23/16: Ethylene-propylene or ethylene-propylene-diene copolymers
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2312/00: Crosslinking
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

The present disclosure provides a composition comprising or obtained from a reaction mixture comprising a first propylene-based polymer, an olefin block copolymer, and a cure component. The cure component comprises (i) a second propylene/α-olefin copolymer, (ii) a scorch retardant, and (iii) a crosslinking agent.

## Claims

### Claim 1

A composition comprising or obtained from a reaction mixture comprising:
a first propylene-based polymer;
an olefin block copolymer; and
a cure component comprising:
i. a second propylene/α-olefin copolymer;
ii. a scorch retardant; and
iii. a crosslinking agent.

### Claim 2 (depends on 1)

The composition of claim 1 wherein the first propylene-based polymer is a first propylene/ethylene copolymer.

### Claim 3 (depends on 1)

The composition of claim 1 wherein the olefin block copolymer is an ethylene/octene multi-block copolymer.

### Claim 4 (depends on 1)

The composition of claim 1 wherein the second propylene/α-olefin copolymer is a second propylene/ethylene copolymer.

### Claim 5 (depends on 1)

The composition of claim 1 wherein the scorch retardant is selected from the group consisting of 2,2,6,6-tetramethylpiperidinoxyl (TEMPO) and 4-hydroxy-2,2,6,6-tetramethylpiperidinoxyl (4-hydroxy-TEMPO), and combinations thereof.

### Claim 6 (depends on 1)

The composition of claim 1 wherein the crosslinking agent is a peroxide.

### Claim 7 (depends on 1)

The composition of claim 1 wherein the cure component further comprises a cure promoter.

### Claim 8 (depends on 1)

The composition of claim 1 comprising:
from 14 wt % to 50 wt % of the first propylene/ethylene copolymer;
from 35 wt % to 76 wt % olefin block copolymer;
from 3 wt % to 36 wt % of the second propylene/ethylene copolymer;
from 0.01 wt % to 1.0 wt % scorch retardant; and
from 0.1 wt % to 5.0 wt % peroxide.

### Claim 9 (depends on 8)

The composition of claim 8 comprising an additive selected from the group consisting of antioxidant, extender oil, filler, UV stabilizer, and combinations thereof.

### Claim 10

A thermoplastic vulcanizate composition comprising:
a continuous phase comprising a first propylene-based polymer; and
a discontinuous phase dispersed in the continuous phase, the discontinuous phase comprising a crosslinked olefin block copolymer.

### Claim 11 (depends on 10)

The thermoplastic vulcanizate composition of claim 10 wherein the first propylene-based polymer is a first propylene/ethylene copolymer.

### Claim 12 (depends on 10)

The thermoplastic vulcanizate composition of claim 10 comprising a second propylene/ethylene copolymer.

### Claim 13 (depends on 12)

The thermoplastic vulcanizate composition of claim 12 comprising
from 5 wt % to 50 wt % of a first propylene-based polymer;
from 15 wt % to 76 wt % crosslinked olefin block copolymer; and
from 1 wt % to 40 wt % of a second propylene/ethylene copolymer.

### Claim 14 (depends on 10)

The thermoplastic vulcanizate composition of claim 10 having a tensile strength from 4 MPa to 20 MPa.

### Claim 15 (depends on 10)

The thermoplastic vulcanizate composition of claim 10 having an elongation at break from 200% to 900%.