# US 2017/0247514 A1 · Method for making a lignin component, a lignin component and its use and a product

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0247514 A1
- Document ID: US20170247514A1
- Status: Published application
- Kind: A1
- Application number: 15/593,471
- Filed: 2017-05-12
- Published: 2017-08-31
- Earliest claimed: 2011-12-09
- Assignees: Upm-Kymmene Corporation
- Applicants: UPM-Kymmene Corporation
- Inventors: Mauno MIETTINEN
- Web page: https://patentgrep.com/patent/US20170247514A1

## CPC

- C08H 6/00: {Macromolecular compounds derived from lignin, e.g. tannins, humic acids}
- C07G 1/00: Low-molecular-weight derivatives of lignin (high-molecular-weight derivatives of lignin {C08H6/00})
- C08H 8/00: Macromolecular compounds derived from lignocellulosic materials {(pretreatment thereof B27N)}
- C08L 97/005: {Lignin}
- D21C 1/04: with acid reacting compounds
- D21C 3/04: with acids, acid salts or acid anhydrides {(D21C3/003 and D21C3/222 take precedence)}
- D21C 11/0007: {Recovery of by-products, i.e. compounds other than those necessary for pulping, for multiple uses or not otherwise provided for (volatile compounds obtained by decomposition of spent liquors in order to regenerate them D21C11/125; compounds obtained by fractionating the liquors in order to regenerate them D21C11/0042)}
- Y10T 428/2982: Particulate matter [e.g., sphere, flake, etc.]
- C08H: DERIVATIVES OF NATURAL MACROMOLECULAR COMPOUNDS (polysaccharides C08B; natural rubber C08C; natural resins or their derivatives C09F; bituminous materials C10)
- C07G: COMPOUNDS OF UNKNOWN CONSTITUTION (sulfonated fats, oils or waxes of undetermined constitution C07C309/62)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- D21C: PRODUCTION OF CELLULOSE BY REMOVING NON-CELLULOSE SUBSTANCES FROM CELLULOSE-CONTAINING MATERIALS; REGENERATION OF PULPING LIQUORS; APPARATUS THEREFOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention relates to a method for making a lignin component from lignin material by an acid treatment, the method comprising: subjecting the lignin material to at least one acid treatment stage by mixing the lignin material with an acid composition to produce an acid treatment mixture, wherein at least one acid treatment stage has a retention time over 6 hours and wherein the acid treatment mixture is held at a temperature of over 60° C. and a pH of 0.5-4 for the retention time of the acid treatment in order to increase dry solids content of the lignin component and decrease ash and carbohydrates of the lignin component. Further, the invention relates to corresponding lignin components, a use of the lignin component and a product.

## Claims

### Claim at position 1

-128. (canceled)

### Claim 129

A method for making a lignin component from lignin material by an acid treatment, the method comprising:
subjecting the lignin material to at least one acid treatment stage by mixing the lignin material with an acid composition to produce an acid treatment mixture, wherein at least one acid treatment stage has a retention time over 6 hours and wherein the acid treatment mixture is held at a temperature of over 60° C. and a pH of 0.5-4 for the retention time of the acid treatment in order to increase dry solids content of the lignin component and decrease ash and carbohydrates of the lignin component.

### Claim 130 (depends on 129)

The method according to claim 129, wherein the lignin material is pre-treated by slurrying the lignin material, wherein the lignin material is slurried at a temperature of 55-70° C. for less than 2 hours.

### Claim 131 (depends on 129)

The method according to claim 129, wherein the acid treatment stage is acid washing or acid hydrolysis.

### Claim 132 (depends on 129)

The method according to claim 129, wherein the acid composition includes H2SO4, other acid or acidifying chemical.

### Claim 133 (depends on 129)

The method according to claim 129, wherein the lignin material is treated in the at least one acid treatment stage such that dry solids content of the lignin component is between 70-90%.

### Claim 134 (depends on 129)

The method according to claim 129, wherein the pH level during the acid treatment stage is below 3.5.

### Claim 135 (depends on 129)

The method according to claim 129, wherein the pH level during the acid treatment stage is between 2-4.

### Claim 136 (depends on 129)

The method according to claim 129, wherein the retention time during the acid treatment stage is over 8 hours.

### Claim 137 (depends on 129)

The method according to claim 129, wherein the temperature during the acid treatment stage is over 70° C.

### Claim 138 (depends on 129)

The method according to claim 129, wherein the temperature during the acid treatment stage is 70-80° C.

### Claim 139 (depends on 129)

The method according to claim 129, wherein the lignin component is formed from the lignin material by treating the lignin material at two acid treatment stages.

### Claim 140 (depends on 129)

The method according to claim 129, wherein the method comprising: filtrating the acid treated lignin material after the acid treatment stage.

### Claim 141 (depends on 140)

The method according to claim 140, wherein the acid treated lignin material is filtrated by pressure filtration or vacuum filtration.

### Claim 142 (depends on 140)

The method according to claim 140, wherein a temperature is over 50° C. and pH is between 2 and 4 during the filtration.

### Claim 143 (depends on 129)

The method according to claim 129, wherein the lignin material includes flash precipitated lignin.

### Claim 144 (depends on 129)

The method according to claim 129, wherein the lignin material is treated in the at least one acid treatment stage such that carbohydrate content of the lignin component is under 1.0%.

### Claim 145

A lignin component which is formed from lignin material by an acid treatment, wherein the lignin component is formed of lignin material by: treating the lignin material in at least one acid treatment stage comprising mixing the lignin material with an acid composition to form a mixture, and maintaining the mixture at a temperature over 60° C. and a pH level of 0.5-4 for at least 6 hours in order to increase dry solids content of the lignin component and decrease ash and carbohydrates of the lignin component, wherein the lignin component has a dry solids content of 70-90% and a carbohydrate content of less than 1.0%.

### Claim 146

A method of manufacturing a final product from lignin material, the method comprising: subjecting the lignin material to at least one acid treatment stage by mixing the lignin material with an acid composition to produce an acid treatment mixture, wherein at least one acid treatment stage has a retention time over 6 hours and wherein the acid treatment mixture is held at a temperature of over 60° C. and a pH of 0.5-4 for the retention time of the acid treatment in order to increase dry solids content of the lignin component and decrease ash and carbohydrates of the lignin component, wherein the final product is selected from a group consisting of activated carbon, carbon fiber, lignin composite, binder material, phenolic component, dispersion agent and their combinations.

### Claim 147 (depends on 129)

A product which includes the lignin component obtainable by the method of claim 129, wherein the lignin component has a dry solids content of 70-90% and a carbohydrate content of less than 1.0%.

### Claim 148 (depends on 147)

The product according to claim 147, wherein the product is selected from a group consisting of activated carbon, carbon fiber, lignin composite, binder material, phenolic component, dispersion agent and their combinations.