# US 2017/0247287 A1 · Glass articles and methods for improving the reliability of glass articles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0247287 A1
- Document ID: US20170247287A1
- Status: Published application
- Kind: A1
- Application number: 15/508,815
- Filed: 2015-09-04
- Published: 2017-08-31
- Earliest claimed: 2014-09-05
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Steven Edward DeMartino; Adam James Ellison; Kyle Christopher Hoff
- Web page: https://patentgrep.com/patent/US20170247287A1

## CPC

- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- A61J 1/1468: {Containers characterised by specific material properties}
- B65D 1/0207: {characterised by material, e.g. composition, physical features}
- C03C 23/0095: {Solution impregnating; Solution doping; Molecular stuffing, e.g. of porous glass (in manufacture of preforms C03B37/012)}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- A61J: CONTAINERS SPECIALLY ADAPTED FOR MEDICAL OR PHARMACEUTICAL PURPOSES; DEVICES OR METHODS SPECIALLY ADAPTED FOR BRINGING PHARMACEUTICAL PRODUCTS INTO PARTICULAR PHYSICAL OR ADMINISTERING FORMS; DEVICES FOR ADMINISTERING FOOD OR MEDICINES ORALLY; BABY COMFORTERS; DEVICES FOR RECEIVING SPITTLE
- B65D: CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS, e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES, DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS; ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR; PACKAGING ELEMENTS; PACKAGES

## Abstract

According to one embodiment, a glass article may include a glass body having a first surface and a second surface opposite the first surface. The first surface and the second surface each have a radius of curvature. The first surface of the glass body comprises a flaw population extending from the first surface into a thickness of the glass body with a maximum initial flaw depth Ai. The first surface of the glass body may be etched to a depth less than or equal to about 25% of the maximum initial flaw depth Ai of the flaw population present in the first surface. When the glass article is under uniaxial compressive loading, at least a portion of the first surface is in tension and a uniaxial compressive strength of the glass article is greater than or equal to 90% of a uniaxial compressive strength of a flaw-free glass article.

## Claims

### Claim 1

A glass article comprising:
a glass body comprising a first surface and a second surface opposite the first surface, the first surface and the second surface each having a radius of curvature;
the first surface of the glass body comprising a flaw population extending from the first surface into a thickness of the glass body with a maximum initial flaw depth Ai, wherein:
the first surface of the glass body is etched to a depth less than or equal to about 25% of the maximum initial flaw depth Ai of the flaw population present in the first surface; and
under uniaxial compressive loading, at least a portion of the first surface is in tension and a uniaxial compressive strength of the glass article is greater than or equal to 90% of a uniaxial compressive strength of a flaw-free glass article.

### Claim 2 (depends on 1)

The glass article of claim 1, wherein a uniaxial compressive strength of the glass article is greater than or equal to 95% of a uniaxial compressive strength of a flaw-free glass article.

### Claim 3 (depends on 1)

The glass article of claim 1, wherein a uniaxial compressive strength of the glass article is greater than or equal to 98% of a uniaxial compressive strength of a flaw-free glass article.

### Claim 4 (depends on 1)

The glass article of claim 1, wherein a failure probability of the glass article is within 10% of a calculated failure probability of a flaw-free glass article.

### Claim 5 (depends on 1)

The glass article of claim 1, wherein a failure probability of the glass article is within 5% of a calculated failure probability of the flaw-free glass article.

### Claim 6 (depends on 1)

The glass article of claim 1, wherein the first surface of the glass article is etched to a depth greater than or equal to about 5% of the maximum initial flaw depth Ai of the flaw population present in the first surface.

### Claim 7 (depends on 1)

The glass article of claim 1, wherein the glass article is a glass container and the first surface of the glass article is an external surface of the glass container and the second surface is an internal surface of the glass container.

### Claim 8 (depends on 7)

The glass article of claim 7, wherein the glass container is a pharmaceutical package.

### Claim 9 (depends on 1)

The glass article of claim 1, wherein the glass article is formed from an alkali-aluminosilicate glass composition.

### Claim 10

A method for improving the reliability of glass articles, the method comprising:
providing a glass article having a first surface, a second surface opposite the first surface, an initial thickness Ti extending from the first surface to the second surface, and a flaw population with a maximum initial flaw depth Ai extending from the first surface into the initial thickness Ti;
selectively removing glass material from the first surface of the glass article and adjacent to each flaw in the flaw population at a uniform rate by chemically processing at least the first surface of the glass article at a temperature and for a time such that, after chemically processing:
flaws having the maximum initial flaw depth Ai remain in the glass article and have a post-processing stress concentration factor Ktpp at a tip of the flaw which is less than an initial stress concentration factor Kti at the tip of the flaw prior to chemical processing;
the flaw population has a maximum post-processing flaw depth App which is substantially equal to Ai;
a post-processing thickness Tpp of the glass article is less than the initial thickness Ti; and
|Tpp−Ti| is substantially equal to |App−Ai|.

### Claim 11 (depends on 10)

The method of claim 10, wherein the first surface and the second surface each have a radius of curvature.

### Claim 12 (depends on 10)

The method of claim 10, wherein:
the glass article is chemically processed by contacting the first surface of the glass article with an etching solution, wherein the etching solution comprises a mixture of hydrofluoric acid having a first molarity from about 0.5 M to about 3.0 M and at least one mineral acid having a second molarity that is 3 to 6 times the first molarity; and
the etching solution uniformly removes glass material from the first surface of the glass article and adjacent to each flaw in the flaw population without creating a gel layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the at least one mineral acid is at least one of hydrochloric acid, nitric acid, phosphoric acid, sulfuric acid, boric acid, hydrobromic acid, and perchloric acid.

### Claim 14 (depends on 10)

The method of claim 10, wherein the glass article is chemically processed by contacting the first surface of the glass article with an etching solution for a treatment time of less than or equal to 360 minutes.

### Claim 15 (depends on 10)

The method of claim 10, wherein the glass article is chemically processed by contacting the first surface of the glass article with an etching solution for a treatment time of less than or equal to 90 minutes.

### Claim 16 (depends on 10)

The method of claim 10, wherein the glass article is chemically process by contacting the first surface of the glass article with an etching solution for a treatment time greater than or equal to 90 minutes and less than or equal to 360 minutes.

### Claim 17 (depends on 10)

The method of claim 10, wherein the glass article has an initial failure probability Pi prior to chemical processing and a post-etching failure probability Ppp after the glass article is chemically processed and Ppp is less than Pi.

### Claim 18 (depends on 10)

The method of claim 10, wherein each flaw in the flaw population has an initial radius of curvature ri at the tip of the flaw prior to chemical processing and a post-etching radius of curvature rpp at the tip of the flaw after chemical processing and ri≦rpp.

### Claim 19 (depends on 10)

The method of claim 10, wherein the glass article is a glass container.

### Claim 20 (depends on 10)

The method of claim 10, wherein the glass article is a pharmaceutical package.