# US 2017/0231080 A1 · Target, apparatus and process for the manufacture of molybdenum-100 targets

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0231080 A1
- Document ID: US20170231080A1
- Status: Published application
- Kind: A1
- Application number: 15/502,338
- Filed: 2015-08-07
- Published: 2017-08-10
- Earliest claimed: 2014-08-11
- Assignees: Best Theratronics, Ltd.
- Applicants: Best Theratronics Ltd.
- Inventors: Richard Ray JOHNSON; William Z. GELBART; Brian ABEYSEKERA; Lidia MATEI; Glenn MCRAE
- Web page: https://patentgrep.com/patent/US20170231080A1

## CPC

- G21G 1/001: {Recovery of specific isotopes from irradiated targets}
- B01D 5/0057: {in combination with other processes}
- B01D 7/00: Sublimation (B01D8/00 takes precedence; freeze-drying F26)
- B01D 15/08: Selective adsorption, e.g. chromatography
- C01G 99/003: {Preparation involving a liquid-liquid extraction, an adsorption or an ion-exchange}
- C01G 99/006: {Compounds containing a metal not provided for elsewhere in this subclass, with or without oxygen or hydrogen, and containing two or more other elements (C01G99/003 takes precedence)}
- G21G 1/02: in nuclear reactors (by thermonuclear reactions G21B; conversion of nuclear fuel G21C)
- G21G 1/10: by bombardment with electrically charged particles (irradiation devices G21K5/00)
- H05H 6/00: Targets for producing nuclear reactions (supports for targets or objects to be irradiated G21K5/08 {; preparation of tritium C01B4/00; targets, e.g. pellets for fusion reactions by laser or charged particles beam injection H05H1/22})
- C01P 2006/80: Compositional purity
- G21G 2001/0042: {Technetium}
- H05H 1/28: Cooling arrangements
- G21G: CONVERSION OF CHEMICAL ELEMENTS; RADIOACTIVE SOURCES (applications of radiation in general G21H5/00; handling particles, e.g. neutrons, or electromagnetic radiation not otherwise provided for G21K)
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H05H: PLASMA TECHNIQUE (apparatus or processes specially adapted for producing X-rays H05G2/00); PRODUCTION OF ACCELERATED ELECTRICALLY-CHARGED PARTICLES OR OF NEUTRONS; PRODUCTION OR ACCELERATION OF NEUTRAL MOLECULAR OR ATOMIC BEAMS
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Apparatuses and methods for production of molybdenum targets, and the formed molybdenum targets, used to produce Tc-99m are described. The target includes a copper support plate having a front face and a back face. The copper support plate desirably has dimensions of thickness of about 2.8 mm, a length of about 65 mm and a width of about 30 mm; and the copper support plate desirably has either a circular or an elliptical cavity centrally formed therein by pressing molybdenum powder into the front face with a depth of about 200-400 microns. Also, the copper support plate includes cooling channels dispensed at the back face; wherein the copper support plate is water cooled by a flow of water during irradiation by a proton beam. Molybdenum powder is embedded and compressed onto the cavity of the copper support plate thereby creating a thin layer of molybdenum onto the copper support plate.

## Claims

### Claim 1

A method for manufacturing a target for the production of Tc-99m, comprising the steps of:
providing a target support plate including copper, the target support plate having a front face and a back face;
placing a molybdenum material in association with the front face of the target support plate; and
applying a pressing force to the molybdenum material to embed the molybdenum material in a cavity formed in the front face by the pressing force, the cavity forming a target material receptacle for the molybdenum material, the pressing force creating a thin substantially uniform layer of the molybdenum material in the formed cavity of the target support plate to form a molybdenum target for forming Tc-99m.

### Claim 2 (depends on 1)

The method for manufacturing a target for the production of Tc-99m of claim 1, wherein the molybdenum material comprises a molybdenum powder or a molybdenum disk or pellet.

### Claim 3 (depends on 2)

The method for manufacturing a target for the production of Tc-99m of claim 2, wherein the thin substantially uniform layer of the molybdenum material has an elliptical or circular shape corresponding to a shape of a protrusion on a die forming the cavity.

### Claim 4 (depends on 2)

The method for manufacturing a target for the production of Tc-99m of claim 2, wherein the molybdenum powder or the molybdenum disk or pellet is compressed by a die having a corresponding elliptic shaped protrusion or a corresponding circular shaped protrusion to produce the thin substantially uniform layer of the molybdenum material forming the molybdenum target of a corresponding shape.

### Claim 5 (depends on 1)

The method for manufacturing a target for the production of Tc-99m of claim 1, wherein the thin substantially uniform layer of the molybdenum material has a thickness in the range of from about 50 microns to about 200 microns.

### Claim 6 (depends on 1)

The method for manufacturing a target for the production of Tc-99m of claim 1, wherein the thin substantially uniform layer of the molybdenum material has a thickness in a range of from about 60 microns to about 80 microns.

### Claim 7 (depends on 1)

The method for manufacturing a target for the production of Tc-99m of claim 1, wherein the applied pressing force is in a range of from about 100 kiloNewtons (kN) to about 500 kN.

### Claim 8 (depends on 1)

The method for manufacturing a target for the production of Tc-99m of claim 1, further comprising the step of:
forming one or more cooling channels on the back face of the target support plate adapted to cool the molybdenum target during formation of the Tc-99m.

### Claim 9 (depends on 8)

The method for manufacturing a target for the production of Tc-99m of claim 8, further comprising the step of:
forming at least one sealing O-ring groove in at least one of a corresponding one or more of the front face and the back face of the target support plate, the at least one sealing O-ring groove adapted to receive a corresponding sealing O-ring to seal a corresponding one of a target face of the molybdenum target or to seal the back face and the one or more cooling channels during irradiation of the molybdenum target to form the Tc-99m.

### Claim 10 (depends on 1)

The method for manufacturing a target for the production of Tc-99m of claim 1, further comprising the steps of:
forming one or more cooling channels on the back face of the target support plate adapted to cool the molybdenum target during formation of the Tc-99m; and
filling the one or more cooling channels with an aluminum material to support the one or more cooling channels during application of the applied pressing force.

### Claim 11 (depends on 10)

The method for manufacturing a target for the production of Tc-99m of claim 10, wherein the one or more cooling channels are adapted to provide for a flow of a cooling fluid to maintain a temperature of the target support plate at a temperature below about 300 degrees Centigrade (° C.) during irradiation of the molybdenum target to form the Tc-99m.

### Claim 12 (depends on 1)

The method for manufacturing a target for the production of Tc-99m of claim 1, further comprising the step of:
electroplating at least the front face of the target support plate with an inert metal selected from the group consisting of Gold (Au), Platinum (Pt), Iridium (Ir), Osmium (Os), Rhodium (Rh), Nickel (Ni), or a combination of thereof.

### Claim 13 (depends on 1)

The method for manufacturing a target for the production of Tc-99m of claim 1, wherein the molybdenum material comprises at least one of a molybdenum metal powder or a molybdenum disk that includes Mo-100.

### Claim 14

A target apparatus for forming a target for production of Tc-99m, comprising:
a target support plate including copper having a front face and a back face, the front face having formed therein a cavity forming a target material receptacle to receive a molybdenum material to form a molybdenum target; and
one or more cooling channels formed on the back face of the target support plate, the one or more cooling channels being adapted to cool the target support plate during formation of Tc-99m from the formed molybdenum target by a flow of a cooling fluid therein during irradiation of the molybdenum target to form the Tc-99m.

### Claim 15 (depends on 14)

The target apparatus for forming a target for production of Tc-99m of claim 14, wherein a thickness of the target support plate is in the range of from about 2 millimeters to about 4 millimeters, and
the target support plate has a length of about 65 millimeters and a width of about 30 millimeters.

### Claim 16 (depends on 14)

The target apparatus for forming a target for production of Tc-99m of claim 14, wherein the formed cavity forming the target material receptacle on the front face of the target support plate has at least one of a generally circular shape or a generally elliptical shape.

### Claim 17 (depends on 14)

The target apparatus for forming a target for production of Tc-99m of claim 14, further comprising:
at least one sealing O-ring groove formed in at least one of a corresponding one or more of the front face and the back face of the target support plate, the at least one sealing O-ring groove adapted to receive a corresponding sealing O-ring to seal a corresponding one of a target face of the molybdenum target or to seal the back face and the one or more cooling channels when the target apparatus is placed in a target holder during irradiation of the molybdenum target to form the Tc-99m.

### Claim 18 (depends on 14)

The target apparatus for forming a target for production of Tc-99m of claim 14, wherein the formed cavity forming the target material receptacle in the target support plate has a depth in a range of from about 200 microns to about 400 microns for receiving the molybdenum material, the molybdenum material including at least one of a molybdenum powder or a molybdenum disk.

### Claim 19 (depends on 14)

The target apparatus for forming a target for production of Tc-99m of claim 14, wherein the one or more cooling channels are arranged in a longitudinal direction or a perpendicular direction on the back face of the target support plate.

### Claim 20 (depends on 14)

The target apparatus for forming a target for production of Tc-99m of claim 14, wherein the cooling fluid comprises water and the flow of the water to cool the target support plate during irradiation of the molybdenum target is in a range of from about 8 Liters/minute to about 10 liters/minute.

### Claim 21 (depends on 14)

The target apparatus for forming a target for production of Tc-99m of claim 14, wherein the one or more cooling channels in conjunction with the flow of the cooling fluid therein during irradiation of the molybdenum target to form the Tc-99m provide a temperature of the target support plate to be held to less than about 300 degrees Centigrade (° C.).

### Claim 22 (depends on 14)

The target apparatus for forming a target for production of Tc-99m of claim 14, wherein the target support plate has a thickness in a range of from about 2 millimeters to about 4 millimeters.

### Claim 23 (depends on 14)

The target apparatus for forming a target for production of Tc-99m of claim 14, wherein the target support plate has a length in a range of from about 50 millimeters to about 100 millimeters and has a breadth in a range of from about 20 millimeters to about 50 millimeters.

### Claim 24 (depends on 14)

The target apparatus for forming a target for production of Tc-99m of claim 14, further comprising:
a molybdenum target formed in the cavity forming the target material receptacle, the molybdenum material including at least one of a molybdenum powder or a molybdenum disk or pellet.

### Claim 25 (depends on 14)

The target apparatus for forming a target for production of Tc-99m of claim 14, wherein the molybdenum material comprises Mo-100.

### Claim 26 (depends on 14)

The target apparatus for forming a target for production of Tc-99m of claim 14, wherein the molybdenum material when embedded in the cavity forming the target material receptacle forms a thin layer with a thickness in a range of from about 50 microns to about 300 microns.

### Claim 27 (depends on 14)

The target apparatus for forming a target for production of Tc-99m of claim 14, wherein the one or more cooling channels are filled with a supporting material including aluminum to protect the one or more cooling channels during a pressing operation during target formation.

### Claim 28 (depends on 14)

The target apparatus for forming a target for production of Tc-99m of claim 14, wherein at least the front face of the target support plate is electroplated with an inert metal selected from the group consisting of Gold (Au), Platinum (Pt), Iridium (Ir), Osmium (Os), Rhodium (Rh), Nickel (Ni), or a combination of thereof.

### Claim 29

A target apparatus including a molybdenum target for production of Tc-99m, comprising:
a target support plate including copper having a front face and a back face, the front face having formed therein a cavity forming a target material receptacle, the target material receptacle including a pressed molybdenum material forming a molybdenum target; and
one or more cooling channels formed on the back face of the target support plate, the one or more cooling channels being adapted to cool the target support plate during formation of Tc-99m from the formed molybdenum target by a flow of a cooling fluid therein during irradiation of the molybdenum target to form the Tc-99m.

### Claim 30 (depends on 29)

The target apparatus for forming a target for production of Tc-99m of claim 29, further comprising:
at least one sealing O-ring groove formed in at least one of a corresponding one or more of the front face and the back face of the target support plate, the at least one sealing O-ring groove adapted to receive a corresponding sealing O-ring to seal a corresponding one of a target face of the molybdenum target or to seal the back face and the one or more cooling channels when the target apparatus is placed in a target holder during irradiation of the molybdenum target to form the Tc-99m.

### Claim 31

A process for the production of Tc-99m, comprising the steps of:
providing a target apparatus including a molybdenum target to be irradiated, the target apparatus comprising:
a target support plate including copper having a front face and a back face, the front face including in a cavity formed therein a molybdenum target formed of a molybdenum material; and
one or more cooling channels formed on the back face of the target support plate, the one or more cooling channels being adapted to cool the molybdenum target during formation of Tc-99m by a flow of a cooling fluid therein during irradiation of the molybdenum target to form the Tc-99m;
irradiating the molybdenum target with a proton beam having an energy to induce a 100Mo (p, 2n) nuclear reaction in the molybdenum material of the molybdenum target to form the Tc-99m;
flowing a cooling fluid through the one or more cooling channels during the irradiating of the molybdenum target to provide a temperature of the target support plate to be held to less than about 300 degrees Centigrade (° C.);
separating the irradiated molybdenum target from the target support plate to form a separated irradiated molybdenum material which includes the formed Tc-99m;
heating the separated irradiated molybdenum material to a temperature in a range of from about 300° C. to about 1,200° C. to generate a vaporized compound containing the Tc-99m;
condensing the vaporized compound containing the Tc-99m to form a reaction product;
adding a base to the condensed reaction product to form a pertechnetate;
collecting the condensed reaction product containing the solution of a pertechnetate Tc-99m [TcO4]−; and
purifying the Tc-99m [TcO4]− pertechnetate solution from the condensed reaction product to provide the Tc-99m as a radiochemical compound.

### Claim 32 (depends on 31)

The process for the production of Tc-99m of claim 31, wherein the energy of the proton beam irradiating the molybdenum target is greater than about 10 Megaelectron-volts (MeV).

### Claim 33 (depends on 31)

The process for the production of Tc-99m of claim 31, wherein the molybdenum target is exposed to a proton beam generated by a cyclotron at grazing incidence of about 15 degrees)(°.

### Claim 34 (depends on 31)

The process for the production of Tc-99m of claim 31, wherein the molybdenum target comprises molybdenum-100, the radiochemical compound comprises Tc-99m sodium pertechnetate (NaTcO4), and purifying the Tc-99m [TcO4]− pertechnetate solution from the condensed reaction product includes using column chromatography.

### Claim 35 (depends on 31)

The process for the production of Tc-99m of claim 31, wherein the separating the irradiated molybdenum target from the target support plate to form the separated irradiated molybdenum material comprises a dissolution process, and purifying the Tc-99m [TcO4]− pertechnetate solution from the condensed reaction product includes using column chromatography.

### Claim 36

A method for manufacturing a target for the production of Tc-99m, comprising the steps of:
placing a molybdenum material on a target support plate including copper having a front face and a back face, the front face including a target material receptacle providing a cavity adapted to receive the molybdenum material; and
applying a pressing force to the molybdenum material placed in the cavity of the target material receptacle on the target support plate to create a pressed thin substantially uniform layer of the molybdenum material in the cavity of the target support plate to form a molybdenum target to form Tc-99m.

### Claim 37

A method for manufacturing a target for the production of Tc-99m, comprising the steps of:
embedding a molybdenum material on a target support plate including copper, the target support plate providing a physical support for a molybdenum target to be formed from the molybdenum material; and
applying a pressing force on the molybdenum material embedded on the target support plate to create a pressed thin layer of the molybdenum material on the target support plate forming a molybdenum target to form Tc-99m.