# US 2017/0203965 A1 · High-yield synthesis of nanostructured boron phosphide by a pyrotechnic method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0203965 A1
- Document ID: US20170203965A1
- Status: Published application
- Kind: A1
- Application number: 15/000,593
- Filed: 2016-01-19
- Published: 2017-07-20
- Earliest claimed: 2016-01-19
- Assignees: U.S. Government as represented by the Secretary of the Army
- Applicants: U.S. Government as Represented by the Secretary of the Army
- Inventors: Zhaohua Luan; Lauren A. Morris; Anthony P. Shaw; Christopher D. Haines; Jay C. Poret
- Web page: https://patentgrep.com/patent/US20170203965A1

## CPC

- C01B 25/084: {of boron}
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}

## Abstract

A simplified method for synthesizing boron phosphide at high yields. The method requires mixing of boron phosphate and magnesium metal without diluents into a homogenous mixture, loosely packing the mixture at less than 20,000 psi and igniting the mixture using an energy input that is not greater than 20% of the reaction energy output to create a self-propagating high-temperature reaction wherein the boron phosphate and magnesium metal is completely burned during the reaction to synthesize boron phosphide at high yields.

## Claims

### Claim 1

A process for producing high yield crystalline boron phosphide comprising:
a. mixing a composition consisting essentially of boron phosphate and magnesium metal into a homogenous mixture;
b. loading the homogenous mixture into a column structure;
c. packing the homogenous mixture at a pressure of 0 psi to 20,000 psi to form a pellet;
d. igniting the pellet by applying a minimum energy input to initiate a self-propagating high-temperature synthesis reaction of the pellet.

### Claim 2 (depends on 1)

The process of claim 1, wherein the mass ratio of the magnesium and boron phosphate is about 1:1.

### Claim 3 (depends on 1)

The process of claim 1, wherein the minimum energy input is about 2.3 calories to about 11.5 calories.

### Claim 4 (depends on 1)

The process of claim 1, wherein the minimum energy input is not greater than 218 calories/gram of the pellet.

### Claim 5 (depends on 1)

The process of claim 1, wherein the minimum energy input is about 0.025% to about 20% of the heat output of the homogenous mixture.

### Claim 6 (depends on 1)

The process of claim 1, wherein the homogenous mixture is packed at a pressure of up to about 10,000 psi.

### Claim 7 (depends on 1)

The process of claim 1, wherein the homogenous mixture is packed into a powderous column or self-standing pellet form.

### Claim 8 (depends on 1)

The process of claim 1, wherein the column structure consists essentially of a combustible material.

### Claim 9 (depends on 1)

The process of claim 1, wherein the column structure comprises a material that can maintain structural integrity of the column structure at temperatures above 1000° C.

### Claim 10 (depends on 1)

The process of claim 1, wherein the column structure is a tubular structure comprised of cardboard, ceramic, or steel.

### Claim 11 (depends on 1)

The process of claim 1, wherein the homogenous mixture is coated with an ignition composition.

### Claim 12 (depends on 1)

The process of claim 1, wherein the homogenous mixture is packed into the column without any pressure.

### Claim 13 (depends on 1)

The process of claim 1, wherein the particle size of the magnesium metal is less than 74 microns.

### Claim 14

A process for increasing the yield of crystalline boron phosphide comprising of:
a. Mixing a composition comprising boron phosphate and magnesium metal into a homogenous mixture, wherein the mass ratio of boron phosphate and magnesium is about 1:1
b. loading the homogenous mixture into a column structure;
c. packing the homogenous mixture at a pressure of 0 psi to 10,000 psi to form a pellet;
d. igniting the pellet by applying a minimum energy input to initiate a self-sustaining high temperature synthesis reaction of the pellet, wherein the minimum energy input is about 0.025% to about 20% of the heat output of the homogenous mixture.