# US 2017/0179193 A1 · Double-masking technique for increasing fabrication yield in superconducting electronics

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0179193 A1
- Document ID: US20170179193A1
- Status: Published application
- Kind: A1
- Application number: 15/456,010
- Filed: 2017-03-10
- Published: 2017-06-22
- Earliest claimed: 2006-09-20
- Assignees: Hypres, Inc.
- Applicants: Hypres, Inc.
- Inventors: Sergey K. Tolpygo
- Web page: https://patentgrep.com/patent/US20170179193A1

## CPC

- H10N 69/00: Integrated devices, or assemblies of multiple devices, comprising at least one superconducting element covered by group H10N60/00
- H10N 60/0156: {of devices comprising Nb or an alloy of Nb with one or more of the elements of group IVB, e.g. titanium, zirconium or hafnium}
- H10N 60/0884: {Treatment of superconductor layers by irradiation, e.g. ion-beam, electron-beam, laser beam or X-rays}
- H10N 60/0912: {of Josephson-effect devices}
- H10N 60/12: Josephson-effect devices
- H10N 60/805: {for Josephson-effect devices}
- H10N 60/85: Superconducting active materials
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

An improved microfabrication technique for Josephson junctions in superconducting integrated circuits, based on the use of a double-layer lithographic mask for partial anodization of the side-walls and base electrode of the junctions. The top layer of the mask is a resist material, and the bottom layer is a dielectric material chosen so to maximize adhesion between the resist and the underlying superconducting layer, be etch-compatible with the underlying superconducting layer, and be insoluble in the resist and anodization processing chemistries. The superconductor is preferably niobium, under a silicon dioxide layer, with a conventional photoresist or electron-beam resist as the top layer. This combination results in a substantial increase in the fabrication yield of high-density superconducting integrated circuits, increase in junction uniformity and reduction in defect density. A dry etch more compatible with microlithography may be employed.

## Claims

### Claim 1

An integrated circuit based on a plurality of Nb-based Josephson junctions, comprising:
a Josephson junction trilayer comprising a lower Nb-containing superconductive layer, an insulating layer, and an upper Nb-containing superconductive layer, on a substrate, fabricated into at least one Josephson junction having a defined junction area less than 1 square micron, the at least one Josephson junction comprising an anodized double oxide layer of AlOx on top of NbOx, wherein the double oxide is patterned in a vacuum processing chamber using a dry etch process to provide vertical sidewalls; and
a silicon dioxide layer formed directly on top of the upper Nb-containing superconductor layer.

### Claim 2 (depends on 1)

The integrated circuit of claim 1, wherein the dry etch process comprises ion milling with a neutral beam of argon atoms.

### Claim 3 (depends on 1)

The integrated circuit of claim 1, wherein the dry etch process comprises the two sequential steps of:
using a chlorine-based plasma etch to remove the top layer of AlOx; and
using a fluorine-based plasma etch to remove the bottom layer of NbOx.

### Claim 4 (depends on 1)

The integrated circuit of claim 1, wherein the pattern definition comprises a layer of photoresist on top of the silicon dioxide, wherein the photoresist has a higher adhesion for the silicon dioxide than the upper Nb-containing superconductive layer.

### Claim 5 (depends on 1)

The integrated circuit of claim 1, wherein the Josephson junction trilayer comprises a sequence of Nb, Al, AlOx, and Nb, wherein the AlOx layer is between 1-2 nm thick.

### Claim 6 (depends on 1)

The integrated circuit of claim 1, wherein the at least one Josephson junction comprises at least one thousand Josephson junctions.

### Claim 7 (depends on 6)

The integrated circuit of claim 6, wherein the at least one thousand Josephson junctions each have operating superconducting critical currents that are within about 1% of a respective design specification.

### Claim 8 (depends on 6)

The integrated circuit of claim 6, wherein the integrated circuit comprises a plurality of functional circuits, each configured to operate at clock frequency of at least 100 GHz.

### Claim 9 (depends on 1)

The integrated circuit of claim 1, wherein the integrated circuit comprises at least one functional circuit configured to operate at clock frequency of at least 100 GHz.

### Claim 10

A Josephson junction integrated circuit, produced by a process comprising:
depositing a Josephson junction trilayer comprising a lower superconductive layer, an insulating layer, and an upper superconductive layer, on a substrate;
depositing a silicon dioxide layer directly on top of the upper superconductor layer by plasma-enhanced chemical vapor deposition (PECVD);
depositing a photoresist having an adhesion to the silicon dioxide greater than a respective adhesion of the photoresist to the upper superconductive layer;
patterning the photoresist;
etching through the silicon dioxide layer and the upper superconductor layer to expose the insulating layer;
anodizing exposed portions of the insulating layer and a portion of the lower superconductive layer; and
dry etching the anodized insulating layer and the portion of the lower superconductive layer, to produce a device having vertical sidewalls.

### Claim 11 (depends on 10)

The Josephson junction circuit according to claim 10, further comprising removing the photoresist.

### Claim 12 (depends on 10)

The Josephson junction circuit according to claim 10, wherein the dry etching comprises ion-milling with a neutral beam of argon (Ar) atoms.

### Claim 13 (depends on 10)

The Josephson junction circuit according to claim 10, wherein the dry etching comprises plasma etching with a chlorine-based plasma and then a fluorine-based plasma.

### Claim 14 (depends on 13)

The Josephson junction circuit according to claim 13, wherein the dry etching comprises reactive ion etching.

### Claim 15 (depends on 13)

The Josephson junction circuit according to claim 13, wherein the dry etching comprises a inductively coupled plasma etching.

### Claim 16 (depends on 10)

The Josephson junction circuit according to claim 10, wherein the lower superconductive layer comprises niobium, the insulating layer comprises oxidized aluminum, and the upper superconductive layer comprises niobium.

### Claim 17 (depends on 10)

The Josephson junction circuit according to claim 10, wherein the silicon dioxide layer is formed by chemical vapor deposition with a layer thickness of between about 5-300 nm.

### Claim 18

A method of forming a Josephson junction integrated circuit, comprising:
depositing a Josephson junction trilayer comprising a lower superconductive layer, an insulating layer, and an upper superconductive layer, on a substrate;
depositing a silicon dioxide layer directly on top of the upper superconductor layer by plasma-enhanced chemical vapor deposition (PECVD);
depositing a photoresist having an adhesion to the silicon dioxide greater than a respective adhesion of the photoresist to the upper superconductive layer;
patterning the photoresist;
etching through the silicon dioxide layer and the upper superconductor layer to expose the insulating layer;
anodizing exposed portions of the insulating layer and a portion of the lower superconductive layer; and
dry etching the anodized insulating layer and the portion of the lower superconductive layer, to produce a device having vertical sidewalls.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the integrated circuit is patterned to define a plurality of interconnected Josephson junctions formed, further comprising operating the plurality of Josephson junctions at a clock rate of at least 100 GHz.

### Claim 20 (depends on 18)

The method according to claim 18,
wherein the lower superconductive layer comprises niobium, the insulating layer comprises oxidized aluminum, and the upper superconductive layer comprises niobium;
wherein the silicon dioxide layer is formed by chemical vapor deposition with a layer thickness of between about 5-300 nm; and
wherein the dry etching comprises at least one of:
ion-milling with a neutral beam of argon (Ar) atoms;
inductively coupled plasma etching with a chlorine-based plasma and then a fluorine-based plasma; and
reactive ion etching.