# US 2017/0001903 A1 · Glass for chemical strengthening, chemically strengthened glass, and method for manufacturing chemically strengthened glass

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0001903 A1
- Document ID: US20170001903A1
- Status: Published application
- Kind: A1
- Application number: 15/266,157
- Filed: 2016-09-15
- Published: 2017-01-05
- Earliest claimed: 2014-03-28
- Assignees: Asahi Glass Company, Limited
- Applicants: Asahi Glass Company, Limited
- Inventors: Junko MIYASAKA; Seiki Ohara; Shuji Yamazaki; Shusaku Akiba; Junichiro Kase
- Web page: https://patentgrep.com/patent/US20170001903A1

## CPC

- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 4/18: for ion-sensitive glass
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

An object of the present invention is to provide a glass for chemical strengthening which is capable of improving strength as compared with an ordinary soda lime silicate glass even when the same chemical strengthening treatment as that in a conventional process is applied and has good devitrification characteristics, a chemically strengthened glass using the glass for chemical strengthening, and a method for producing the chemically strengthened glass. The present invention provides a glass for chemical strengthening having a specific glass composition described in the present specification.

## Claims

### Claim 1

A glass for chemical strengthening, comprising, as expressed by mass percentage based on oxides, 60 to 72% of SiO2, 4.4 to 10% of Al2O3, 5 to 10.9% of MgO, 0.1 to 5% of CaO, 14 to 19% of Na2O, and 0 to 3% of K2O, wherein RO is 7% or more and 11% or less (wherein the RO represents the sum of alkaline earth metal oxides, i.e., MgO, CaO, SrO, and BaO) and RO/(RO+R2O) is 0.20 or more and 0.42 or less (wherein the R2O represents the sum of alkali metal oxides).

### Claim 2 (depends on 1)

The glass for chemical strengthening according to claim 1, wherein the RO/(RO+R2O) is 0.40 or less.

### Claim 3 (depends on 1)

The glass for chemical strengthening according to claim 1, comprising 5% or more of Al2O3.

### Claim 4 (depends on 1)

The glass for chemical strengthening according to claim 1, comprising 6% or more of MgO.

### Claim 5 (depends on 1)

The glass for chemical strengthening according to claim 1, comprising 10% or less of MgO.

### Claim 6 (depends on 1)

The glass for chemical strengthening according to claim 1, further comprising 0 to 4% of B2O3, 0 to 1% of Fe2O3 and 0 to 1% of TiO2.

### Claim 7 (depends on 1)

The glass for chemical strengthening according to claim 1, having a temperature (T2) at which a viscosity is 102 dPa·s of 1550° C. or lower.

### Claim 8 (depends on 1)

The glass for chemical strengthening according to claim 1, which has been formed according to a float process.

### Claim 9 (depends on 1)

A chemically strengthened glass obtained by chemically strengthening the glass for chemical strengthening according to claim 1.

### Claim 10 (depends on 9)

The chemically strengthened glass according to claim 9, having a surface compressive stress of 300 MPa or more.

### Claim 11 (depends on 9)

The chemically strengthened glass according to claim 9, having a depth of compressive stress of 10 μm or more.

### Claim 12 (depends on 1)

A method for producing a chemically strengthened glass, comprising a chemical strengthening step of subjecting the glass for chemical strengthening according to claim 1 to an ion-exchange treatment.