# US 2017/0001345 A1 · Process for making a multi-component plastic housing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2017/0001345 A1
- Document ID: US20170001345A1
- Status: Published application
- Kind: A1
- Application number: 14/755,128
- Filed: 2015-06-30
- Published: 2017-01-05
- Earliest claimed: 2015-06-30
- Assignees: Braun GmbH
- Applicants: Braun GmbH
- Inventors: Marc KUNZ; Werner HUEBSCHER; Kris LUECKEL; Sven Schäfer; Stefan Gehard TRIEBIG
- Web page: https://patentgrep.com/patent/US20170001345A1

## CPC

- B29C 45/0003: {of successively moulded portions rigidly joined to each other}
- B29C 45/162: {using means, e.g. mould parts, for transferring an injected part between moulding stations}
- B29C 45/1635: {using displaceable mould parts, e.g. retractable partition between adjacent mould cavities}
- B29C 45/1676: {using a soft material and a rigid material, e.g. making articles with a sealing part}
- B29D 22/003: {Containers for packaging, storing or transporting, e.g. bottles, jars, cans, barrels, tanks}
- B29C 33/444: {for stripping articles from a mould core, e.g. using stripper plates}
- B29C 2045/1629: {turrets with incorporated ejection means}
- B29C 2045/1682: {preventing defects}
- B29C 2045/4078: {using stripping means}
- B29K 2021/003: {Thermoplastic elastomers}
- B29K 2023/10: {Polymers of propylene}
- B29L 2031/425: {Toothbrush}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A process for making a multi-component hollow housing comprises injecting a first plastic material into a first mold cavity and causing it to solidify to form a first component, whereby the first plastic material shrinks lengthwise; injecting a second plastic material into a second mold cavity having the first component transferred thereto and causing the second plastic component to solidify to form a second component, the second component comprising a tolerance-elimination element that is longitudinally attached to the first component at one of the ends thereof, wherein a length of the shrunk first component is at least ten times greater than a length of the tolerance-elimination element, and wherein an absolute lengthwise shrinkage of the second plastic material forming the tolerance-elimination element is at least ten times smaller than the lengthwise shrinkage of the first plastic material; at least partially overmolding an intermediate part comprising the first and second component with a third plastic material in a third mold cavity, thereby forming the multi-component housing in which the tolerance-elimination element is at least partially overmolded by the third plastic material, and wherein the third plastic material forms at least a portion of an outer surface of the multi-component housing; and removing the multi-component housing from the core.

## Claims

### Claim 1

A process for making a multi-component hollow housing from a shrinkable plastic material, the housing having a longitudinal axis, a top end, a bottom end, a length therebetween extending parallel to the length of the housing, the process comprising:
injecting a first plastic material into a first mold cavity having a core at least partially disposed therein, the first mold cavity having a first-cavity length;
causing the first plastic material to solidify, whereby the first plastic material shrinks lengthwise by a first absolute lengthwise shrinkage and whereby a first component is formed, the first component comprising a generally tubular structure having a first end and a second end opposite to the first end and a first solidified length therebetween, wherein the first solidified length is smaller than the first-cavity length;
positioning the core, together with the first component disposed thereon, in a second mold cavity having a second-cavity length that is greater than the first-cavity length by a distance greater than the first absolute lengthwise shrinkage of the first plastic material during solidification;
injecting a second plastic material into the second mold cavity and causing the second plastic component to solidify to form a second component attached to the first component, the second component comprising a tolerance-elimination element that is longitudinally adjacent to the first component at one of the first end and the second end thereof, wherein the tolerance-elimination element has a proximal end adjacent to the first component, a distal end opposite to the proximal end, and an average length that is arithmetic mean of a maximal length and a minimal length of the tolerance-elimination element, the maximal and minimal lengths extending parallel to the longitudinal axis and between the proximal and distal ends of the tolerance-elimination element, wherein the first solidified length of the first component is at least ten times greater than the maximal length of the tolerance-elimination element, and wherein an absolute lengthwise shrinkage of the second plastic material forming the tolerance-elimination element is at least ten times smaller than the first absolute lengthwise shrinkage of the first plastic material;
at least partially overmolding the intermediate part, including the tolerance-elimination element, with a third plastic material in a third mold cavity and causing the third plastic material to solidify to form a third component attached to at least one of the first component and the second component, thereby forming the multi-component housing in which the tolerance-elimination element is at least partially overmolded by the third plastic material, and wherein the third component forms at least a portion of an outer surface of the multi-component housing; and
removing the multi-component housing from the core.

### Claim 2 (depends on 1)

The process of claim 1, wherein the first plastic material, the second plastic material, and the third plastic material differ from one another in at least one characteristic selected from the group consisting of color, opacity, porosity, and hardness.

### Claim 3 (depends on 1)

The process of claim 1, wherein at least one of the first plastic material, the second plastic material, and the third plastic material is a hard-plastic material.

### Claim 4 (depends on 1)

The process of claim 1, wherein at least one of the first plastic material, the second plastic material, and the third plastic material is a soft-plastic material.

### Claim 5 (depends on 1)

The process of claim 1, wherein the first plastic material is a first hard-plastic material, the second plastic material is a second hard-plastic material different from the first hard-plastic material, and the third plastic material is a soft-plastic material.

### Claim 6 (depends on 1)

The process of claim 1, wherein the step of at least partially overmolding the intermediate part with a third plastic material results in the tolerance-elimination element being completely overmolded by the third plastic material.

### Claim 7 (depends on 1)

The process of claim 1, wherein in the step of injecting a second plastic material, the injected second plastic material comprises a first portion and a second portion, wherein the first portion of the second plastic material at least partially overmolds the first component, and the second portion of the second plastic material forms the tolerance-elimination element.

### Claim 8 (depends on 7)

The process of claim 7, wherein both the first portion and the second portion of the second plastic material are formed with a single injection shot.

### Claim 9 (depends on 1)

The process of claim 1, wherein after the second plastic material has solidified, the tolerance-elimination element has the minimal length of from about 1 mm to about 20 mm and the maximal length of from about 10 mm to about 30 mm.

### Claim 10 (depends on 1)

The process of claim 1, wherein after the second plastic material has solidified, the tolerance-elimination element has the average length of from about 5 mm to about 10 mm.

### Claim 11 (depends on 1)

The process of claim 1, wherein the tolerance-elimination element causes the multi-component housing to have a lengthwise tolerance of from 0.01 mm to 0.05 mm.

### Claim 12 (depends on 1)

The process of claim 1, wherein the tolerance-elimination element causes the multi-component housing to have a lengthwise tolerance of from about 0.006% to about 0.03% relative to the length of the multi-component housing.

### Claim 13 (depends on 1)

The process of claim 1, further comprising positioning at least one movable stripper on the core so that the at least one stripper forms a part of at least one of the second mold cavity and the third mold cavity, whereby the at least one stripper contacts at least one of the second plastic material and the third plastic material being injected.

### Claim 14 (depends on 13)

The process of claim 13, wherein the third plastic material extends in the third mold cavity beyond the distal end of the tolerance-elimination element and wherein the stripper contacts the third plastic material at a distance of from about 0.5 mm to about 3 mm from the distal end of the tolerance-elimination element.

### Claim 15 (depends on 14)

The process of claim 14, wherein an orthogonal surface of the distal end of the tolerance-elimination element is at least partially overmolded by the third plastic material to form a touch-up area.

### Claim 16 (depends on 13)

The process of claim 13, wherein the step of removing the multi-component housing from the core is accomplished by moving the stripper in contact with the multi-component hosing.

### Claim 17

A process for making a multi-component housing for a toothbrush handle, the housing having a top end, a bottom end, a longitudinal axis and a length extending parallel to the longitudinal axis and between the top and bottom ends, the process comprising:
injecting a first hard-plastic material into a first mold cavity having a core at least partially disposed therein, the first mold cavity having a first-cavity length;
causing the first hard-plastic material to solidify, whereby the first hard-plastic material shrinks lengthwise by a first absolute lengthwise shrinkage and whereby a first component comprising a generally tubular structure is formed, the first component having a first end and a second end opposite to the first end and a first solidified length therebetween, wherein the first solidified length is smaller than the first-cavity length;
positioning the core, together with the first component disposed thereon, in a second mold cavity having a second-cavity length that is greater than the first-cavity length by a distance greater than the first absolute lengthwise shrinkage of the first hard-plastic material;
injecting a second hard-plastic material into the second mold cavity and causing the second hard-plastic material to solidify thereby forming a second component attached to the first component, the second component comprising a tolerance-elimination element that is longitudinally adjacent to the first component at one of the first end and the second end thereof;
wherein the tolerance-elimination element has a proximal end adjacent to the first component, a distal end opposite to the proximal end, and an average length that is arithmetic mean of a maximal length and a minimal length of the tolerance-elimination element, the maximal length and the minimal length extending parallel to the longitudinal axis and between the proximal and distal ends of the tolerance-elimination element;
wherein the first solidified length of the first component is at least ten times greater than the maximal length of the tolerance-elimination element, and wherein an absolute lengthwise shrinkage of the second hard-plastic material forming the tolerance-elimination element is at least ten times less than the first absolute lengthwise shrinkage of the first hard-plastic material;
at least partially overmolding the intermediate part with a soft-plastic material in a third mold cavity to form a third component attached to at least one of the first component and the second component, thereby forming the multi-component housing in which the tolerance-elimination element is at least partially overmolded by the soft-plastic material, and wherein the soft-plastic material forms at least a portion of an outer surface of the multi-component housing; and
removing the multi-component housing from the core.

### Claim 18 (depends on 17)

The process of claim 17, wherein the multi-component housing has a lengthwise tolerance of from 0.01 mm to 0.05 mm.

### Claim 19 (depends on 17)

The process of claim 17, wherein the multi-component housing has a lengthwise tolerance of from about 0.006% to about 0.03% relative to the length of the multi-component housing.

### Claim 20 (depends on 17)

The process of claim 17, wherein the step of at least partially overmolding the intermediate part with a soft-plastic material results in the tolerance-elimination element being completely overmolded by the soft-plastic material.

### Claim 21 (depends on 17)

The process of claim 17, wherein during the step of injecting a second hard-plastic material, the second hard-plastic material comprises a first portion that at least partially overmolds the first component and a second portion that forms the tolerance-elimination element.

### Claim 22 (depends on 21)

The process of claim 21, wherein both the first portion and the second portion of the second hard-plastic material are formed with a single injection shot.

### Claim 23 (depends on 17)

The process of claim 17, wherein after the second hard-plastic material has solidified, the tolerance-elimination element has the minimal length of from about 1 mm to about 20 mm.

### Claim 24 (depends on 17)

The process of claim 17, wherein after the second hard-plastic material has solidified, the tolerance-elimination element has the minimal length of from about 2 mm to about 15 mm.

### Claim 25 (depends on 17)

The process of claim 17, wherein after the second hard-plastic material has solidified, the tolerance-elimination element has the minimal length of from about 3 mm to about 10 mm.

### Claim 26 (depends on 17)

The process of claim 17, wherein after the second hard-plastic material has solidified, the tolerance-elimination element has the maximal length of from about 10 mm to about 30 mm.

### Claim 27 (depends on 17)

The process of claim 17, wherein after the second hard-plastic material has solidified, the tolerance-elimination element has an average length of from about 5 mm to about 10 mm.

### Claim 28 (depends on 17)

The process of claim 17, wherein the tolerance-elimination element causes the multi-component housing to have a lengthwise tolerance of less than 0.05 mm.

### Claim 29 (depends on 17)

The process of claim 17, wherein the tolerance-elimination element causes the multi-component housing to have a lengthwise tolerance of from about 0.006% to about 0.03% relative to the length L of the multi-component housing.

### Claim 30 (depends on 17)

The process of claim 17, wherein during the step of at least partially overmolding the second component with a soft-plastic material, the soft-plastic material completely overmolds the tolerance-elimination element and extends beyond the distal end thereof.

### Claim 31 (depends on 30)

The process of claim 30, further comprising positioning a sliding stripper on a mold core to cause the sliding stripper to touch the soft-plastic material being injected when the soft-plastic material extends beyond the distal end of the tolerance-elimination element, thereby forming an edge of the soft-plastic material, wherein a distance of from about 0.5 mm to about 3 mm is formed between the edge of the soft-plastic material in contact with the stripper and a portion of the distal end of the tolerance-elimination element, and wherein the sliding stripper forms a part of the third mold cavity.

### Claim 32 (depends on 31)

The process of claim 31, wherein the soft-plastic material at least partially overmolds an orthogonally oriented surface of the distal end of the tolerance-elimination element.

### Claim 33 (depends on 17)

The process of claim 17, wherein the first hard-plastic material and the second hard-plastic material differ from one another in at least one characteristic selected from the group consisting of color, opacity, porosity, and hardness.

### Claim 34 (depends on 17)

The process of claim 17, wherein at least one of the first hard-plastic material and the second hard-plastic material is transparent or translucent, and the soft material is opaque.

### Claim 35 (depends on 17)

The process of claim 17, wherein the step of removing the multi-component housing from the core is accomplished by moving a sliding stripper that forms a part of the third mold cavity and is in contact with the multi-component housing.