# US 2016/0365608 A1 · Method of manufacturing nonaqueous electrolyte secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0365608 A1
- Document ID: US20160365608A1
- Status: Published application
- Kind: A1
- Application number: 15/174,097
- Filed: 2016-06-06
- Published: 2016-12-15
- Earliest claimed: 2015-06-11
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Jidosha Kabushiki Kaisha
- Inventors: Yuichi ITO
- Web page: https://patentgrep.com/patent/US20160365608A1

## CPC

- H01M 10/446: {Initial charging measures}
- H01M 10/0567: characterised by the additives
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/052: Li-accumulators
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of manufacturing a nonaqueous electrolyte secondary battery includes: constructing a nonaqueous electrolyte secondary battery including an electrode body and an electrolytic solution, the electrode body including a negative electrode, and the electrolytic solution containing a nonaqueous solvent and a negative electrode film forming agent having a decomposition voltage that is lower than a decomposition voltage of the nonaqueous solvent; performing first charging of the nonaqueous electrolyte secondary battery at a voltage that is equal to or higher than the decomposition voltage of the negative electrode film forming agent and lower than the decomposition voltage of the nonaqueous solvent and at −30° C. to 0° C.; and performing second charging of the nonaqueous electrolyte secondary battery at a voltage that is equal to or higher than the decomposition voltage of the nonaqueous solvent and at a temperature of 25° C. or higher and lower than a boiling point of the electrolytic solution.

## Claims

### Claim 1

A method of manufacturing a nonaqueous electrolyte secondary battery, the method comprising:
constructing a nonaqueous electrolyte secondary battery including an electrode body and an electrolytic solution, the electrode body including a negative electrode, and the electrolytic solution containing a nonaqueous solvent and a negative electrode film forming agent having a decomposition voltage that is lower than a decomposition voltage of the nonaqueous solvent;
performing a first charging of the nonaqueous electrolyte secondary battery at a voltage that is equal to or higher than the decomposition voltage of the negative electrode film forming agent and lower than the decomposition voltage of the nonaqueous solvent and at −30° C. to 0° C.; and
performing a second charging of the nonaqueous electrolyte secondary battery at a voltage that is equal to or higher than the decomposition voltage of the nonaqueous solvent and at a temperature of 25° C. or higher and lower than a boiling point of the electrolytic solution.

### Claim 2 (depends on 1)

The method according to claim 1, wherein
after the voltage reaches a value that is equal to or higher than the decomposition voltage of the negative electrode film forming agent and lower than the decomposition voltage of the nonaqueous solvent, the voltage is retained in a range that is equal to or higher than the decomposition voltage of the negative electrode film forming agent and lower than the decomposition voltage of the nonaqueous solvent for 3 hours or longer.

### Claim 3 (depends on 1)

The method according to claim 1, wherein
after the voltage reaches a value that is equal to or higher than the decomposition voltage of the negative electrode film forming agent and lower than the decomposition voltage of the nonaqueous solvent, the voltage at a temperature of −30° C. to 0° C. is retained in a range that is equal to or higher than the decomposition voltage of the negative electrode film forming agent and lower than the decomposition voltage of the nonaqueous solvent for 1 hour or longer.

### Claim 4 (depends on 1)

The method according to claim 1, wherein
a charging rate at which the voltage is increased to a value that is equal to or higher than the decomposition voltage of the negative electrode film forming agent and lower than the decomposition voltage of the nonaqueous solvent is 10 mV/sec or lower.

### Claim 5 (depends on 1)

The method according to claim 1, wherein
the negative electrode film forming agent is vinylene carbonate or a lithium salt containing an oxalato complex as an anion.

### Claim 6 (depends on 1)

The method according to claim 1, wherein
a temperature during the second charging is 25° C. to 35° C.

### Claim 7 (depends on 1)

The method according to claim 1, wherein
a charging rate during the second charging is higher than a charging rate during the first charging.