# US 2016/0365602 A1 · A solid electrolyte glass for lithium or sodium ions conduction

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0365602 A1
- Document ID: US20160365602A1
- Status: Published application
- Kind: A1
- Application number: 15/121,678
- Filed: 2015-02-26
- Published: 2016-12-15
- Earliest claimed: 2014-02-26
- Assignees: Universidade Do Porto; LaboratóRio Nacional De Energia E Geologia
- Applicants: Universidade Do Porto; LaboratóRio Nacional De Energia E Geologia
- Inventors: Maria Helena SOUSA SOARES DE OLIVEIRA BRAGA; José Jorge DO AMARAL FERREIRA
- Web page: https://patentgrep.com/patent/US20160365602A1

## CPC

- H01M 10/0562: Solid materials
- H01G 9/15: Solid electrolytic capacitors (H01G11/00 takes precedence)
- H01G 11/56: Solid electrolytes, e.g. gels; Additives therein
- H01G 11/84: Processes for the manufacture of hybrid or EDL capacitors, or components thereof
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- H01M 16/00: Structural combinations of different types of electrochemical generators
- H01M 2300/0071: Oxides
- Y02E 60/10: Energy storage using batteries
- Y02E 60/13: Energy storage using capacitors
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Glassy electrolyte for lithium or sodium ions conduction The present disclosure relates to the development and improvement of sodium or lithium-ion electrochemical devices, in particular to the development of a new glassy electrolyte comprising high ionic conductivity for batteries, capacitors, and other electrochemical devices comprising a solid electrolyte glass comprising the formula R3-2xMxHalO wherein R is selected from the group consisting of lithium or sodium; M is selected from the group consisting of magnesium, calcium, strontium or barium; Hal is selected from the group consisting of fluorine, chlorine, bromine, iodine or mixtures thereof; X is the number of moles of M and 0≦x≦0.01 and the solid electrolyte glass has a glass transition point.

## Claims

### Claim 1

A solid electrolyte glass comprising compound of formula R3-2xMxHalO wherein
R is selected from the group consisting of lithium or sodium;
M is selected from the group consisting of magnesium, calcium, strontium or barium;
Hal is selected from the group consisting of fluorine, chlorine, bromine, iodine or mixtures thereof;
X is the number of moles of M and 0≦x≦0.01;
and the solid electrolyte glass has a glass transition point.

### Claim 2 (depends on 1)

The electrolyte glass according to claim 1 wherein R is lithium.

### Claim 3 (depends on 1)

The electrolyte glass according to claim 1 wherein R is sodium.

### Claim 4 (depends on 1, 2)

The electrolyte glass according to claim 1 or 2 comprising an ionic conductivity of at least 13 mScm−1 at 25° C.

### Claim 5

The electrolyte glass according to the previous claim comprising an ionic conductivity of 13-60 mScm−1 at 25° C.

### Claim 6

The electrolyte glass according to the previous claim comprising an ionic conductivity of at least 25 mScm−1 at 25° C.

### Claim 7 (depends on 1, 3)

The electrolyte glass according to claim 1 or 3 comprising an ionic conductivity of at least 17 mScm−1 at 25° C.

### Claim 8

The electrolyte glass according to the previous claim comprising an ionic conductivity of 17-105 mScm−1 at 25° C.

### Claim 9

The electrolyte glass according to the previous claim comprising an ionic conductivity of at least 31 mScm−1 at 25° C.

### Claim 10

The electrolyte glass according to any of the previous claims wherein X is 0.002, 0.005; 0.007 or 0.01.

### Claim 11

The electrolyte glass according to any of the previous claims wherein Hal is a mixture of chlorine and iodine.

### Claim 12

The electrolyte glass according to any of the wherein Hal is Hal=0.5Cl+0.51.

### Claim 13

The electrolyte glass according to any of the previous claims wherein Hal is a mixture of fluorine and iodine.

### Claim 14

The electrolyte glass according to any of the previous claims wherein R is lithium, M is barium, Hal is chlorine and x is 0.005.

### Claim 15

The electrolyte glass according to any of the previous claims wherein R is lithium, M is barium, Hal is a mixture of chlorine and iodine, x is 0.005.

### Claim 16

The electrolyte glass according to any of the previous claims wherein R is sodium, M is barium, Hal is chlorine and x is 0.005.

### Claim 17

An electrolyte composition comprising a compound of formula Na3-2xMxHalO wherein
M is selected from the group consisting of magnesium, calcium, strontium or barium;
Hal is selected from the group consisting of fluorine, chlorine, bromine, iodine or mixtures thereof;
X is the number of moles of M and 0<x≦0.01.

### Claim 18

The composition according to the previous claim wherein M is barium, Hal is chlorine and x is 0.005.

### Claim 19 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18)

An electrochemical device comprising the electrolyte glass or composition referred in any of the claims 1-18.

### Claim 20 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18)

A capacitor comprising the electrolyte glass or composition referred in any of the claims 1-18.

### Claim 21 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18)

A battery comprising the electrolyte glass or composition referred in any of the claims 1-18.

### Claim 22 (depends on 20, 21)

An electrochemical device comprising at least one capacitor as referred in claim 20 and at least one battery as referred in claim 21.

### Claim 23

A method for synthetizing a glass electrolyte comprising a compound of formula R3-2xMxHalO wherein
R is lithium;
M is selected from the group consisting of magnesium, calcium, strontium or barium;
Hal is selected from the group consisting of fluorine, chlorine, bromine, iodine or mixtures thereof;
X is the number of moles of M and 0≦x≦0.01;
comprising the following steps:
mixing a stoichiometric quantity of LiHal, LiOH, and one of the following compounds: Mg(OH)2; Ca(OH)2, Sr(OH)2 or Ba(OH)2;
adding to said mixture deionized water and mixing to form a solution in a closed container;
heating said solution up to 250° C. during 2-8 h;
opening the container to evaporate the excess of water in the heated product.

### Claim 24

The method according to the previous claim further comprising:
introducing the synthetized glass material between electrodes the electrodes of an electrochemical device;
heating the glass up to 170-240° C. and cooling.

### Claim 25

A method for synthetizing a glass electrolyte comprising a compound of formula R3-2xMxHalO wherein
R is sodium;
M is selected from the group consisting of magnesium, calcium, strontium and barium;
Hal is selected from the group consisting of fluorine, chlorine, bromine, iodine or mixtures thereof;
X is the number of moles of M and 0≦x≦0.01;
comprising the following steps:
mixing a stoichiometry quantity of NaHal, NaOH and one of the following compounds: Mg(OH)2; Ca(OH)2; Sr(OH)2 or Ba(OH)2;
adding to said mixture deionized water and mixing to form a solution in a closed container;
heating the solution up to 70-90° C. for 2-8 h;
increasing the temperature up to 190-250° C. for 2-8 h, maintaining said temperature for at least 2 h;
opening the container to evaporate the excess water in the heated product.

### Claim 26

The method according to the previous claim further comprising:
introducing the synthetized glass material between electrodes;
heating the glass up to 190-230° C. and cooling.

### Claim 27

A method for synthetizing a glass electrolyte comprising a compound of formula R3-2xMxHalO wherein
R is lithium;
M is selected from the group consisting of magnesium, calcium, strontium or barium;
Hal is selected from the group consisting of fluorine, chlorine, bromine, iodine or mixtures thereof;
X is the number of moles of M and 0≦x≦0.01;
comprising the following steps:
mixing a stoichiometry quantity of LiHal, LiOH and one of the following compounds: Mg(OH)2; Ca(OH)2; Sr(OH)2 or Ba(OH)2;
adding to said mixture deionized water and mixing to form a solution in a closed container;
heating said solution up to 250° C. during 2-8 h;
opening the container to evaporate the excess of water in the heated product.

### Claim 28

The method according to the previous claim further comprising:
introducing the synthetized glass material between electrodes;
heating the glass up to 170-240° C. and cooling.

### Claim 29

Use of the composition of formula R3-2xMxHalO wherein
R is selected from the group consisting of lithium or sodium;
M is selected from the group consisting of magnesium, calcium, barium or strontium;
Hal is selected from the group consisting of fluorine, chlorine, bromine, iodine or mixtures thereof;
X is the number of moles of M and 0≦x≦0.01;
as an enhancer of the ionic conductivity of an electrolyte and/or of the electrochemical window of stability of an electrolyte.