# US 2016/0365571 A1 · Sulfate Containing Rechargeable Battery Cathode with Oxidized Surface

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0365571 A1
- Document ID: US20160365571A1
- Status: Published application
- Kind: A1
- Application number: 15/121,439
- Filed: 2015-02-25
- Published: 2016-12-15
- Earliest claimed: 2014-02-27
- Assignees: Umicore AG & Co. KG; Umicore Korea Ltd.
- Applicants: Umicore; Umicore Korea Ltd.
- Inventors: Dae-Hyun KIM; Jens PAULSEN
- Web page: https://patentgrep.com/patent/US20160365571A1

## CPC

- H01M 4/366: {as layered products}
- H01B 1/06: mainly consisting of other non-metallic substances
- H01B 1/08: oxides
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/364: {as mixtures}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/052: Li-accumulators
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for preparing a positive electrode material for a rechargeable lithium battery, comprising the steps of: providing a Li metal (M) oxide electroactive material, providing an inorganic oxidizing chemical compound, providing a chemical that is a Li-acceptor, mixing the Li metal (M) oxide, the oxidizing compound and the Li-acceptor, and heating the mixture at a N temperature between 200 and 800° C. in an oxygen comprising atmosphere. In an embodiment the positive electrode material comprises a Li metal (M) oxide electroactive material, and between 0.15 and 5 wt % of a LiNaSO4 secondary phase. The Li metal oxide may have the general formula Li1+a′M1−aO2, with a′<a and 0.9≦(1+a′)/(1−a)≦1.15, and M═Ni1−x−yM′xCoy, with M′═Mni−zAlz, 0≦z≦1, 0.1≦y≦0.4 and x+y≦0.5.

## Claims

### Claim at position 1

1-19. (canceled)

### Claim 20

A positive electrode material for a rechargeable lithium battery comprising a Li metal (M) oxide electroactive material, and between 0.15 and 5 wt % of a LiNaSO4 secondary phase.

### Claim 21 (depends on 20)

The positive electrode material of claim 20, wherein M═Ni1−x−yM′xCoy, with M′═Mn1−zAlz, 0≦z≦1, 0.1≦y≦0.4 and x+y≦0.5.

### Claim 22 (depends on 21)

The positive electrode material of claim 21, wherein 1−y−2x>0.2.

### Claim 23 (depends on 20)

The positive electrode material of claim 20, wherein the Li metal oxide has the general formula Li1+a′M1−aO2, with a′<a and 0.9≦(1+a′)/(1−a)≦1.15.

### Claim 24 (depends on 20)

The positive electrode material of claim 20, wherein the mass fraction of the LiNaSO4 secondary phase is between 0.2 and 2 wt %.

### Claim 25 (depends on 20)

The positive electrode material of claim 20, wherein the material comprises a core comprising the Li metal (M) oxide and a coating comprising the LiNaSO4 secondary phase.

### Claim 26 (depends on 20)

The positive electrode material of claim 20, wherein the secondary phase further comprises up to 1 wt % of one or more compounds selected from the group consisting of Al2O3, LiAlO2, LiF, Li3PO4, MgO and Li2TiO3.

### Claim 27 (depends on 25)

The positive electrode material of claim 25, wherein the LiNaSO4 coating is covered by a second coating comprising one or more of Al2O3, LiAlO2, LiF or MgO, and wherein the second coating represents up to 1 wt % of the material.

### Claim 28 (depends on 20)

The positive electrode material of claim 20, wherein the Li metal (M) oxide is doped with up to 2 mol % of one or more elements selected from the group consisting of Al, Ti, Mg and Zr.

### Claim 29 (depends on 20)

The positive electrode material of claim 20, wherein the Li metal (M) oxide is doped with up to 0.2 mol % of one or more elements selected from the group consisting of Ca, Sr, Si, F, P and K.

### Claim 30 (depends on 20)

A method for preparing the positive electrode material of claim 20, comprising:
providing a Li metal (M) oxide electroactive material,
providing an inorganic oxidizing chemical compound,
providing a chemical that is a Li-acceptor,
mixing the Li metal (M) oxide, the oxidizing compound and the Li-acceptor, and
heating the mixture at a temperature between 300 and 800° C. in an oxygen comprising atmosphere.

### Claim 31 (depends on 30)

The method according to claim 30, wherein the Li metal oxide has the general formula Li1+a′M1−aO2, with a′<a and 0.9≦(1+a′)/(1−a)<1.15, and M═Ni1−x−yM′xCoy, with M′═Mn1−zAlz, 0≦z≦1, 0.1≦y≦0.4 and x+y≦0.5.

### Claim 32 (depends on 30)

The method according to claim 30, wherein the inorganic oxidizing chemical compound comprises NaHSO5 or either one of a chloride, a chlorate, a perchlorate or a hypochloride of either one of potassium, sodium, lithium, magnesium or calcium.

### Claim 33 (depends on 30)

The method according to claim 30, wherein the Li-acceptor chemical comprises one of AlPO4, Li3AlF6 or AlF3.

### Claim 34 (depends on 30)

The method according to claim 30, wherein the inorganic oxidizing chemical compound and the Li-acceptor chemical are the same compound, being one of Li2S2O8, H2S2O8 or Na2S2O8.

### Claim 35 (depends on 30)

The method according to claim 30, wherein the mass fraction of the Li metal (M) oxide in the mixture is between 95 and 99.8 wt %.

### Claim 36 (depends on 30)

The method according to claim 30, wherein the heating temperature is between 350 and 450° C.

### Claim 37 (depends on 34)

The method according to claim 34, wherein the inorganic oxidizing chemical compound and the Li-acceptor chemical are Na2S2O8, and wherein Na2S2O8 is mixed with the Li metal (M) oxide in a dry process.

### Claim 38 (depends on 34)

The method according to claim 34, wherein a nanosized Al2O3 powder is provided as a further Li-acceptor chemical.