# US 2016/0365570 A1 · Lithium Secondary Battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0365570 A1
- Document ID: US20160365570A1
- Status: Published application
- Kind: A1
- Application number: 15/178,606
- Filed: 2016-06-10
- Published: 2016-12-15
- Earliest claimed: 2015-06-11
- Assignees: SK Innovation Co., Ltd.
- Applicants: SK Innovation Co., Ltd.
- Inventors: Kook-Hyun Han; Kyung-Bin Yoo; Duck-Chul Hwang
- Web page: https://patentgrep.com/patent/US20160365570A1

## CPC

- H01M 4/364: {as mixtures}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 50/434: Ceramics
- H01M 50/449: having a layered structure
- H01M 50/451: comprising layers of only organic material and layers containing inorganic material
- H01M 50/457: comprising three or more layers
- H01M 50/489: Separators, membranes, diaphragms or spacing elements inside the cells, characterised by their physical properties, e.g. swelling degree, hydrophilicity or shut down properties
- H01M 50/454: comprising a non-fibrous layer and a fibrous layer superimposed on one another
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02T 10/70: Energy storage systems for electromobility, e.g. batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

Disclosed is a lithium secondary battery including a cathode, an anode, and a separation film installed between the cathode and the anode, wherein the cathode includes a cathode active material containing lithium-metal oxide of which at least one of metals has a continuous concentration gradient region between a core part and a surface part thereof, and the separation film includes a base film, and a ceramic coating layer formed on at least one surface of the base film, such that lifespan property is significantly improved, while exhibiting excellent penetration safety.

## Claims

### Claim 1

A lithium secondary battery, comprising a cathode, an anode, and a separation film installed between the cathode and the anode,
wherein the cathode includes a cathode active material containing lithium-metal oxide of which at least one of metals has a continuous concentration gradient region between a core part and a surface part thereof, and
the separation film includes a base film, and a ceramic coating layer formed on at least one surface of the base film.

### Claim 2 (depends on 1)

The lithium secondary battery according to claim 1, wherein another of the metals included in the lithium-metal oxide has a constant concentration between the core part and the surface part.

### Claim 3 (depends on 1)

The lithium secondary battery according to claim 1, wherein the lithium-metal oxide includes a first metal having a concentration gradient region with increased concentration between the core part and the surface part, and a second metal having a concentration gradient region with decreased concentration between the core part and the surface part.

### Claim 4 (depends on 1)

The lithium secondary battery according to claim 1, wherein the lithium-metal oxide is represented by Formula 1 below, and at least one of M1, M2 and M3 has a continuous concentration gradient between the core part and the surface part:
LixM1aM2bM3cOy [Formula 1]
(wherein M1, M2 and M3 are selected from a group consisting of Ni, Co, Mn, Na, Mg, Ca, Ti, V, Cr, Cu, Zn, Ge, Sr, Ag, Ba, Zr, Nb, Mo, Al, Ga and B, and
0<x≦1.1, 2≦y≦2.02, 0≦a≦1, 0≦b≦1, 0≦c≦1, and 0<a+b+c≦1).

### Claim 5 (depends on 4)

The lithium secondary battery according to claim 4, wherein at least one of the M1, M2 and M3 has a concentration gradient region with increased concentration between the core part and the surface part, while the others have a concentration gradient region with decreased concentration between the core part and the surface part.

### Claim 6 (depends on 4)

The lithium secondary battery according to claim 4, wherein at least one of the M1, M2 and M3 has a concentration gradient region with increased concentration between the core part and the surface part, another has a concentration gradient region with decreased concentration between the core part and the surface part, and the other has a constant concentration between the core part and the surface part.

### Claim 7 (depends on 4)

The lithium secondary battery according to claim 4, wherein the M1, M2 and M3 are Ni, Co and Mn, respectively.

### Claim 8 (depends on 4)

The lithium secondary battery according to claim 4, wherein the M1 is Ni, and 0.6≦a≦0.95 and 0.05≦b+c≦0.4.

### Claim 9 (depends on 5)

The lithium secondary battery according to claim 5, wherein the M1 is Ni, and 0.6≦a≦0.95 and 0.05≦b+c≦0.4.

### Claim 10 (depends on 6)

The lithium secondary battery according to claim 6, wherein the M1 is Ni, and 0.6≦a≦0.95 and 0.05≦b+c≦0.4.

### Claim 11 (depends on 4)

The lithium secondary battery according to claim 4, wherein the M1 is Ni, and 0.7≦a≦0.9 and 0.1≦b+c≦0.3.

### Claim 12 (depends on 5)

The lithium secondary battery according to claim 5, wherein the M1 is Ni, and 0.7≦a≦0.9 and 0.1≦b+c≦0.3.

### Claim 13 (depends on 6)

The lithium secondary battery according to claim 6, wherein the M1 is Ni, and 0.7≦a≦0.9 and 0.1≦b+c≦0.3.

### Claim 14 (depends on 1)

The lithium secondary battery according to claim 1, wherein the ceramic coating layer includes ceramic powders having an average particle diameter of 0.01 to 2.0 μm.

### Claim 15 (depends on 1)

The lithium secondary battery according to claim 1, wherein the ceramic coating layer includes the ceramic powders in an amount of 80 to 97% by weight to a total weight of the ceramic coating layer.

### Claim 16 (depends on 1)

The lithium secondary battery according to claim 1, wherein the ceramic coating layer includes metal oxide containing at least one metal selected from a group consisting of aluminum (Al), titanium (Ti), zirconium (Zr), barium (Ba), magnesium (Mg), boron (B), yttrium (Y), zinc (Zn), calcium (Ca), nickel (Ni), silicon (Si), lead (Pb), strontium (Sr), tin (Sn) and cerium (Ce).

### Claim 17 (depends on 1)

The lithium secondary battery according to claim 1, wherein the ceramic coating layer includes at least one selected from a group consisting of Al2O3, TiO2, ZrO2, Y2O3, ZnO, CaO, NiO, MgO, SiO2, SiC, Al(OH)3, AlO(OH), BaTiO3, PbTiO3, PZT, PLZT, PMN-PT, HfO2, SrTiO3, SnO3 and CeO2, as the ceramic powders.

### Claim 18 (depends on 1)

The lithium secondary battery according to claim 1, wherein the ceramic coating layer formed on one surface of the separation film has a thickness of 2 to 10 μm.

### Claim 19 (depends on 1)

The lithium secondary battery according to claim 1, wherein the ceramic coating layers have a sum of total thickness of 4 to 20 μm.