# US 2016/0365548 A1 · Sodium conducting energy storage devices comprising compliant polymer seals and methods for making and sealing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0365548 A1
- Document ID: US20160365548A1
- Status: Published application
- Kind: A1
- Application number: 15/226,570
- Filed: 2016-08-02
- Published: 2016-12-15
- Earliest claimed: 2014-08-20
- Assignees: Battelle Memorial Institute
- Applicants: Battelle Memorial Institute
- Inventors: Guosheng Li; Hee-Jung Chang; Vincent L. Sprenkle
- Web page: https://patentgrep.com/patent/US20160365548A1

## CPC

- H01M 10/39: working at high temperature
- H01M 50/186: characterised by the disposition of the sealing members
- H01M 50/193: Organic material
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

New compliant polymer seals and methods for making and sealing energy storage devices are disclosed. Compliant polymer seals become viscous at the operation temperature which seals cathode and anode chambers following assembly.

## Claims

### Claim 1

An energy-storage device, comprising:
a first polymer seal disposed in at least one junction of a cathode chamber in contact with a primary solid state electrolyte that is inert to a secondary electrolyte therein comprising an alkali-metal aluminum halide; and
a second polymer seal disposed in at least one junction of an anode chamber in contact with the primary electrolyte that is inert to sodium metal therein;
whereby the seals include a viscosity that seal the respective cathode and anode chambers at operation temperatures from about 100° C. to about 300° C.

### Claim 2 (depends on 1)

The energy-storage device of claim 1, wherein the first polymer seal comprises a polymer different from the polymer in the second polymer seal.

### Claim 3 (depends on 1)

The energy-storage device of claim 1, wherein the first polymer seal or the second polymer seal is comprised of ultra-high molecular weight polyethylene.

### Claim 4 (depends on 1)

The energy-storage device of claim 1, wherein the first polymer seal comprises a polymer selected from: polytetrafluoroethylene (PTFE); fluorinated ethylene propylene (FEP); perfluoroalkoxy alkanes (PFA); or polyethylene (PE).

### Claim 5 (depends on 1)

The energy-storage device of claim 1, wherein the second polymer seal comprises a polymer selected from polyvinylidene fluoride (PVDF), or polyethylene (PE).

### Claim 6 (depends on 1)

The energy-storage device of claim 1, wherein the first and second polymer seals are composite seals comprising a viscosity modifier of up to about 50% by weight therein.

### Claim 7 (depends on 1)

The energy-storage device of claim 1, wherein the first and second polymer seals are composite seals comprising a viscosity modifier that is encapsulated by the first or second polymer therein.

### Claim 8 (depends on 1)

The energy-storage device of claim 1, wherein the first polymer seal comprises a polymer selected from: polytetrafluoroethylene (PTFE); fluorinated ethylene propylene (FEP); perfluoroalkoxy alkanes (PFA); or polyethylene (PE); and the second polymer seal comprises polyvinylidene fluoride (PVDF).

### Claim 9 (depends on 1)

The energy-storage device of claim 1, wherein the first polymer seal comprises polytetrafluoroethylene (PTFE) and the second polymer seal comprises polyvinylidene fluoride (PVDF).

### Claim 10 (depends on 1)

The energy-storage device of claim 1, wherein the first polymer seal comprises polytetrafluoroethylene (PTFE) and the second polymer seal comprises polyethylene (PE).

### Claim 11 (depends on 1)

The energy-storage device of claim 1, wherein the first polymer seal comprises fluorinated ethylene propylene (FEP) and the second polymer seal comprises polyvinylidene fluoride (PVDF).

### Claim 12 (depends on 1)

The energy-storage device of claim 1, wherein the first polymer seal comprises fluorinated ethylene propylene (FEP) and the second polymer seal comprises polyethylene (PE).

### Claim 13 (depends on 1)

The energy-storage device of claim 1, wherein the first polymer seal comprises perfluoroalkoxy alkane (PFA) and the second polymer seal comprises polyvinylidene fluoride (PVDF).

### Claim 14 (depends on 1)

The energy-storage device of claim 1, wherein the first polymer seal comprises perfluoroalkoxy alkane (PFA) and the second polymer seal comprises polyethylene (PE).

### Claim 15 (depends on 1)

The energy-storage device of claim 1, further including a metal mesh disposed in the anode chamber in contact with the solid electrolyte therein.

### Claim 16 (depends on 1)

The energy-storage device of claim 1, further including an anode shim disposed in the anode chamber adjacent the solid electrolyte therein.

### Claim 17

A sodium-conducting energy-storage device, comprising:
a sodium ion-conducting solid state electrolyte as a primary electrolyte;
a first polymer seal comprising a first polymer selected from polytetrafluoroethylene (PTFE); fluorinated ethylene propylene (FEP); perfluoroalkoxy alkanes (PFA); or polyethylene (PE) disposed in at least one junction of a cathode chamber in contact with the primary electrolyte on the cathode side of the storage device that is inert to a secondary electrolyte comprising a sodium-metal or potassium metal aluminum halide therein; and
a metal mesh disposed in the anode chamber in contact with the solid electrolyte configured to maintain contact between sodium metal and the solid electrolyte therein; and
a second polymer seal comprising a polymer selected from polyvinylidene fluoride (PVDF); or polyethylene (PE) disposed in at least one junction of an anode chamber in contact with the primary electrolyte on the anode side of the storage device that is inert to sodium metal formed therein;
whereby the first and second seals have a selected viscosity that seal the respective cathode and anode chambers and prevent influx of external oxidizing gases therein at operation temperatures above about 100° C. to below about 300° C.

### Claim 18

A method for sealing a sodium-conducting energy storage device, comprising the steps of:
introducing a first compliant seal comprising a first polymer selected from polytetrafluoroethylene (PTFE); fluorinated ethylene propylene (FEP); a perfluoroalkoxy alkane (PFA); or polyethylene (PE) disposed in at least one junction of a cathode chamber in contact with a primary electrolyte on the cathode side of the storage device that seals the cathode chamber and is inert to a secondary electrolyte comprising an alkali-metal aluminum halide introduced therein;
introducing a second compliant seal comprising a second polymer different from the first polymer selected from polyvinylidene fluoride (PVDF); or polyethylene (PE) disposed in at least one junction of an anode chamber in contact with the primary electrolyte on the anode side of the storage device that seals the anode chamber and components therein preventing influx of the external oxidizing gas therein and is inert to sodium metal formed therein;
whereby the first and second seals include a viscosity that seal the respective cathode and anode chambers at a selected operation temperature.

### Claim 19 (depends on 18)

The method of claim 18, wherein the operation temperature is selected from about 100° C. to about 300° C.

### Claim 20 (depends on 18)

The method of claim 18, wherein the seals in operation provide a performance degradation in the energy storage device of less than about 5% over at least 200 charge-discharge cycles at a discharge current of 10 mA/cm2.