# US 2016/0365535 A1 · Encapsulating method, display panel and display apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0365535 A1
- Document ID: US20160365535A1
- Status: Published application
- Kind: A1
- Application number: 14/905,504
- Filed: 2015-04-23
- Published: 2016-12-15
- Earliest claimed: 2015-01-13
- Assignees: Ordos Yuansheng Optoelectronics Co., Ltd.
- Applicants: Ordos Yuansheng Optoelectronics Co., Ltd.
- Inventors: Zhiliang JIANG
- Web page: https://patentgrep.com/patent/US20160365535A1

## CPC

- H10K 59/8722: {Peripheral sealing arrangements, e.g. adhesives, sealants}
- H10K 71/40: Thermal treatment, e.g. annealing in the presence of a solvent vapour
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

An encapsulating method, a display panel and a display apparatus, the encapsulating method including: forming a frit layer in an encapsulating area of a first substrate; forming a glass network modifier oxide layer on the surface of the frit layer; a first-sintering for the frit layer and the glass network modifier oxide layer; and aligning and attaching the first substrate and a second substrate, and forming an encapsulating structure through irradiating the encapsulating area by a laser. The encapsulating method can improve the liquidity of the surface of the frit layer and make the surface of the frit planarization after sintering at high temperature, so that the production of the holes of the surface of the frit layer can be reduced in the process of being encapsulated by a laser, and then the effect of encapsulating is improved.

## Claims

### Claim 1

An encapsulating method, comprising:
forming a frit layer in an encapsulating area of a first substrate;
forming a glass network modifier oxide layer on a surface of the frit layer;
first-sintering the frit layer and the glass network modifier oxide layer; and
aligning and attaching the first substrate with a second substrate, and irradiating the encapsulating area by a laser to form an encapsulating structure.

### Claim 2 (depends on 1)

The encapsulating method according to claim 1, wherein, forming of the frit layer in the encapsulating area of the first substrate comprises:
dispersing a frit in a carrier to form a glass cement;
disposing the glass cement in the encapsulating area of the first substrate; and
second-sintering the glass cement.

### Claim 3 (depends on 2)

The encapsulating method according to claim 2, wherein the second-sintering is carried out at a temperature of 120° C.-150° C.,

### Claim 4 (depends on 1)

The encapsulating method according to claim 1 wherein a material of the glass network modifier oxide layer is one or more selected from the group consisting of Na2O and K2O.

### Claim 5 (depends on 4)

The encapsulating method according to claim 4, wherein, the material of the glass network modifier oxide layer is formed on the surface of the frit layer through a method of vapor deposition or sputtering to obtain the glass network modifier oxide layer.

### Claim 6 (depends on 1)

The encapsulating method according to claim 1, wherein, the first-sintering is carried out at a temperature of 350° C.-550° C.

### Claim 7 (depends on 1)

The encapsulating method according to claim 1, wherein, the glass network modifier oxide layer has a thickness of 0.5 nm˜10 nm.

### Claim 8

A display panel, comprising a first substrate, a second substrate and an encapsulating structure which is disposed in an encapsulating area to seal the first substrate and the second substrate, wherein, the encapsulating structure comprises an encapsulating glass layer and a glass network modifier oxide layer with the encapsulating glass layer being between the first substrate and the second substrate and the glass network modifier oxide layer being between the encapsulating glass layer and the second substrate.

### Claim 9 (depends on 8)

The display panel according to claim 8, wherein, a material of the glass network modifier oxide layer is one or more selected from the group consisting of Na2O and K2O.

### Claim 10 (depends on 8)

The display panel according to claim 8, wherein, the glass network modifier oxide layer has a thickness of 0.5 nm˜10 nm.

### Claim 11 (depends on 8)

A display apparatus, comprising the display panel according to claim 8.

### Claim 12 (depends on 11)

The display apparatus according to claim 11, wherein, a material of the glass network modifier oxide layer is one or more selected from the group consisting of Na2O and K2O.

### Claim 13 (depends on 11)

The display apparatus according to claim 11, wherein, the glass network modifier oxide layer has a thickness of 0.5 nm˜10 nm.

### Claim 14 (depends on 9)

The display panel according to claim 9, wherein, the glass network modifier oxide layer has a thickness of 0.5 nm˜10 nm,

### Claim 15 (depends on 2)

The encapsulating method according to claim 2, wherein, a material of the glass network modifier oxide layer is one or more selected from the group consisting of Na2O and K2O.

### Claim 16 (depends on 15)

The encapsulating method according to claim 15, wherein, the material of the glass network modifier oxide layer is formed on the surface of the frit layer through a method of vapor deposition or sputtering to obtain the glass network modifier oxide layer.

### Claim 17 (depends on 16)

The encapsulating method according to claim 16, wherein, the first-sintering is carried out at a temperature of 350° C.-550° C.

### Claim 18 (depends on 17)

The encapsulating method according to claim 17, wherein, the glass network modifier oxide layer has a thickness of 0.5 nm˜10 nm.