# US 2016/0365477 A1 · Method of making a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0365477 A1
- Document ID: US20160365477A1
- Status: Published application
- Kind: A1
- Application number: 15/163,173
- Filed: 2016-05-24
- Published: 2016-12-15
- Earliest claimed: 2015-06-12
- Assignees: National Chiao Tung University
- Applicants: National Chiao Tung University
- Inventors: Chun-Yen CHANG; Chen-Yu LI; Hao-Chung KUO
- Web page: https://patentgrep.com/patent/US20160365477A1

## CPC

- H10D 30/015: {of FETs having heterojunction interface channels or heterojunction gate electrodes, e.g. HEMT}
- H10H 20/01335: {the light-emitting regions comprising nitride materials}
- H10H 20/815: having stress relaxation structures, e.g. buffer layers
- H10P 14/20: of semiconductor materials
- H10P 14/2918: {being semiconductor metal oxides (Group IIB-VIA materials H10P14/2913)}
- H10P 14/3216: {Nitrides}
- H10P 14/3248: {consisting of two layers}
- H10P 14/3416: {Nitrides}
- H10D 30/475: {having wider bandgap layer formed on top of lower bandgap active layer, e.g. undoped barrier HEMTs such as i-AlGaN/GaN HEMTs}
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of making a semiconductor device includes: (a) providing a semiconductor substrate that is made from a material containing an element of boron group; (b) forming on the semiconductor substrate a buffer structure that includes an aluminum nitride buffer film formed using a physical vapor deposition technique; and (c) forming on the buffer structure a semiconductor unit that includes a GaN-based epitaxial layer, the GaN-based epitaxial layer having a hexagonal crystal structure and being formed using a chemical vapor deposition technique.

## Claims

### Claim 1

A method of making a semiconductor device, comprising:
(a) providing a semiconductor substrate (21) that is made from a material containing an element of boron group;
(b) forming on the semiconductor substrate (21) a buffer structure (22) that includes an aluminum nitride buffer film (221) formed using a physical vapor deposition technique; and
(c) forming on the buffer structure (22) a semiconductor unit (23) that includes a GaN-based epitaxial layer (230), the GaN-based epitaxial layer having a hexagonal crystal structure and being formed using a chemical vapor deposition technique.

### Claim 2 (depends on 1)

A method of claim 1, wherein, in step (b), the semiconductor substrate (21) is heated to a temperature ranging from 300° C. to 700° C.

### Claim 3 (depends on 1)

A method of claim 1, wherein the buffer structure further includes a GaN buffer film formed between the aluminum nitride buffer film and the GaN-based epitaxial layer, the GaN buffer film being formed using a chemical vapor deposition technique under a condition that the semiconductor substrate (21) and the aluminum nitride buffer film (221) are heated to a temperature ranging from 500° C. to 600° C. and hydrogen is used as a carrier gas.

### Claim 4 (depends on 1)

A method of claim 1, wherein, in step (c), the forming of the semiconductor unit (23) is conducted under a condition that the semiconductor substrate (21) and the buffer structure (22) are heated to a temperature ranging from 1100° C. to 1200° C. and hydrogen is used as a carrier gas.

### Claim 5 (depends on 1)

A method of claim 1, wherein step (c) includes forming the GaN-based epitaxial layer on the buffer structure and laminating a first electrode layer (231), a pre-strained layer (232), a multi-quantum-well layer (233), a barrier layer (234), an electron-blocking layer (235), and a second electrode layer (236) on the GaN-based epitaxial layer (230).

### Claim 6 (depends on 1)

A method of claim 1, wherein step (c) includes forming the GaN-based epitaxial layer on the buffer structure and laminating a buffer layer (237), a channel layer (238), a blocking layer (239), a capping layer (240), and an electrode layer (241) on the GaN-based epitaxial layer (230).

### Claim 7 (depends on 1)

A method of claim 1, wherein step (c) further includes doping the epitaxial layer (230) with one of carbon element and iron element.

### Claim 8 (depends on 1)

A method of claim 1, wherein the physical vapor deposition technique used in step (b) is a sputter technique or a molecular beam epitaxy technique.

### Claim 9 (depends on 1)

A method of claim 1, wherein the chemical vapor deposition technique used in step (c) is a metal organic chemical vapor deposition technique or a hydride vapor phase epitaxy technique.