# US 2016/0365273 A1 · Method for manufacturing bonded wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0365273 A1
- Document ID: US20160365273A1
- Status: Published application
- Kind: A1
- Application number: 15/120,905
- Filed: 2015-02-12
- Published: 2016-12-15
- Earliest claimed: 2014-03-18
- Assignees: Shin-Etsu Handotai Co., Ltd.
- Applicants: Shin-Etsu Handotai Co., Ltd.
- Inventors: Norihiro KOBAYASHI; Hiroji AGA
- Web page: https://patentgrep.com/patent/US20160365273A1

## CPC

- H10P 90/1916: {with separation or delamination along an ion implanted layer, e.g. Smart-cut}
- H10D 86/00: Integrated devices formed in or on insulating or conducting substrates, e.g. formed in silicon-on-insulator [SOI] substrates or on stainless steel or glass substrates
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/208: {of electrically inactive species}
- H10P 30/209: {in silicon to make buried insulating layers}
- H10P 70/15: {by wet cleaning only (H10P70/52 takes precedence)}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10P 95/906: {for altering the shape of semiconductors, e.g. smoothing the surface}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10P 14/6309: {of silicon in uncombined form, i.e. pure silicon}
- H10P 14/6322: {Formation by thermal treatments (formation by plasma treatment H10P14/6319)}
- H10P 50/642: {Chemical etching}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for manufacturing a bonded wafer, includes: ion-implanting a gas ion such as a hydrogen ion from a surface of a bond wafer, thereby forming an ion-implanted layer; bonding the bond wafer and a base wafer; producing a bonded wafer having a thin-film on the base wafer by delaminating the bond wafer along the ion-implanted layer; and performing an RTA treatment on the bonded wafer in a hydrogen gas-containing atmosphere; wherein a protective film is formed onto the surface of the thin-film in a heat treatment furnace in the course of temperature-falling from the maximum temperature of the RTA treatment before the bonded wafer is taken out from the heat treatment furnace; and then the bonded wafer with the protective film being formed thereon is taken out from the heat treatment furnace, and is then cleaned with a cleaning liquid which can etch the protective film and the thin-film.

## Claims

### Claim at position 1

1-4. (canceled)

### Claim 5

A method for manufacturing a bonded wafer, comprising: ion-implanting at least one gas ion selected from a hydrogen ion and a rare gas ion from a surface of a bond wafer, thereby forming an ion-implanted layer into the inside of the wafer; bonding the ion-implanted surface of the bond wafer and a surface of a base wafer directly or through an insulating film; followed by producing a bonded wafer having a thin-film on the base wafer by delaminating the bond wafer along the ion-implanted layer; and flattening the surface of the thin-film by performing an RTA treatment on the bonded wafer in a hydrogen gas-containing atmosphere; wherein
a protective film is formed onto the surface of the thin-film in a heat treatment furnace in the course of temperature-falling from the maximum temperature of the RTA treatment before the bonded wafer is taken out from the heat treatment furnace; and then
the bonded wafer with the protective film being formed thereon is taken out from the heat treatment furnace, and is then cleaned with a cleaning liquid which can etch the protective film and the thin-film.

### Claim 6 (depends on 5)

The method for manufacturing a bonded wafer according to claim 5, wherein the protective film is formed by changing the hydrogen gas-containing atmosphere in the heat treatment furnace to any of an oxidizing atmosphere, a nitriding atmosphere, and an oxynitriding atmosphere in the course of temperature-falling from the maximum temperature of the RTA treatment; thereby exposing the bonded wafer to any of the oxidizing atmosphere, the nitriding atmosphere, and the oxynitriding atmosphere to form any of an oxide film, a nitride film, and an oxynitride film onto the surface of the thin-film.

### Claim 7 (depends on 5)

The method for manufacturing a bonded wafer according to claim 5, wherein the cleaning liquid is an aqueous mixed solution of NH4OH and H2O2.

### Claim 8 (depends on 6)

The method for manufacturing a bonded wafer according to claim 6, wherein the cleaning liquid is an aqueous mixed solution of NH4OH and H2O2.

### Claim 9 (depends on 5)

The method for manufacturing a bonded wafer according to claim 5, wherein the protective film is formed with a thickness of 0.7 to 3 nm.

### Claim 10 (depends on 6)

The method for manufacturing a bonded wafer according to claim 6, wherein the protective film is formed with a thickness of 0.7 to 3 nm.

### Claim 11 (depends on 7)

The method for manufacturing a bonded wafer according to claim 7, wherein the protective film is formed with a thickness of 0.7 to 3 nm.

### Claim 12 (depends on 8)