# US 2016/0365222 A1 · Method for imaging wafer with focused charged particle beam in semiconductor fabrication

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0365222 A1
- Document ID: US20160365222A1
- Status: Published application
- Kind: A1
- Application number: 14/739,198
- Filed: 2015-06-15
- Published: 2016-12-15
- Earliest claimed: 2015-06-15
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd
- Inventors: Ting-Tsung CHOU
- Web page: https://patentgrep.com/patent/US20160365222A1

## CPC

- H01J 37/265: {Controlling the tube; circuit arrangements adapted to a particular application not otherwise provided, e.g. bright-field-dark-field illumination}
- H01J 37/21: Means for adjusting the focus
- H10P 74/203: {Structural properties, e.g. testing or measuring thicknesses, line widths, warpage, bond strengths or physical defects}
- H01J 2237/004: Charge control of objects or beams
- H01J 2237/216: Automatic focusing methods
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for processing a semiconductor wafer is provided. The method includes positioning the semiconductor wafer in a scanning electron microscope (SEM). The method further includes producing images of at least a portion of a test region that is designated on a process surface of the semiconductor wafer. The method also includes adjusting the condition of a charged particle beam of the SEM at a check point selected in the test region. In addition, the method includes producing images of another portion of the test region after the condition of the charged particle beam is adjusted.

## Claims

### Claim 1

A method for processing a semiconductor wafer, comprising:
positioning the semiconductor wafer in a scanning electron microscope (SEM);
producing images of at least a portion of a test region which is designated on a process surface of the semiconductor wafer;
adjusting a condition of a charged particle beam of the SEM at a check point in the test region; and
producing images of another portion of the test region after the condition of the charged particle beam is adjusted.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the operation of adjusting a charged particle beam condition comprises adjusting a focal point position of the charged particle beam on the test region.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the operation of adjusting a charged particle beam condition comprises adjusting an acceleration voltage applied to the charged particle beam.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein a plurality of check points are selected, and the condition of the charged particle beam is adjusted in each of the check points.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein a plurality of images of the test region are recorded, and an area of the test region is in a range from about 0.04 mm2 to about 5.7 mm2.

### Claim 6 (depends on 1)

The method as claimed in claim 1, further comprising forming an insulating layer over the process surface of the semiconductor wafer, wherein during the period of the first scanning operation positive charges are generated on the insulating layer.

### Claim 7 (depends on 6)

The method as claimed in claim 6, wherein the insulating layer includes titanium nitride.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein in the operation of positioning the semiconductor wafer in a SEM, the semiconductor wafer is held by a substrate stage of the SEM, and the positive charges are isolated from electrical ground of the substrate stage by the insulating layer.

### Claim 9

A method for inspecting a semiconductor wafer having a process surface, comprising:
performing a first scanning operation for imaging at least a portion of a test region of the process surface on the semiconductor wafer by supplying a charged particle beam;
stopping the first scanning operation before the test region is completely imaged; and
performing a second scanning operation for imaging another portion of the test region by supplying an adjusted charged particle beam.

### Claim 10 (depends on 9)

The method as claimed in claim 9, further comprising forming an insulating layer over the semiconductor wafer, wherein the charged particle beam comprises an electron beam, and during the period of the first scanning operation, positive charges are generated on the insulating layer.

### Claim 11 (depends on 9)

The method as claimed in claim 9, wherein the test region is defined by at least one boundary line, and the first scanning operation is finished at a terminal scanning point which is located in the test region and not overlapped by the boundary line.

### Claim 12 (depends on 9)

The method as claimed in claim 9, wherein a plurality of images are recorded during each of the first scanning operation and the second scanning operation, wherein the number of images recorded during the first scanning operation is the same as the number of images recorded during the second scanning operation.

### Claim 13 (depends on 9)

The method as claimed in claim 9, wherein the charged particle beam is supplied with a first acceleration voltage, and the adjusted charged particle beam is supplied with a second acceleration voltage, wherein the first acceleration voltage is greater than the second acceleration voltage.

### Claim 14 (depends on 9)

The method as claimed in claim 9, further comprising performing a focus tracking function before the second scanning operation to produce focused images on another portion of the test region.

### Claim 15

A method for inspecting a semiconductor wafer having a process surface, comprising:
performing a first scanning operation for imaging at least a portion of a test region of the process surface by supplying a charged particle beam;
stopping the first scanning operation after the first scanning operation has been performed for a first preset time period; and
performing a second scanning operation for imaging another portion of the test region by supplying an adjusted charged particle beam.

### Claim 16 (depends on 15)

The method as claimed in claim 15, further comprising forming an insulating layer over the semiconductor wafer, wherein the charged particle beam comprises an electron beam, and during the period of the first scanning operation positive charges are generated on the insulating layer.

### Claim 17 (depends on 15)

The method as claimed in claim 15, wherein the test region is defined by at least one boundary line, and the first scanning operation is finished at a terminal scanning point which is located in the test region and not overlapped by the boundary line.

### Claim 18 (depends on 15)

The method as claimed in claim 15, wherein the second scanning operation is stopped after the second scanning operation is performed for a second preset time period, wherein the first preset time period is the same as the second preset time period.

### Claim 19 (depends on 15)

The method as claimed in claim 15, wherein the charged particle beam is supplied with a first acceleration voltage, and the adjusted charged particle beam is supplied with a second acceleration voltage, wherein the first acceleration voltage is greater than the second acceleration voltage.

### Claim 20 (depends on 15)

The method as claimed in claim 15, further comprising performing a focus tracking function before the second scanning operation to produce focused images on another portion of the test region.