# US 2016/0355939 A1 · Polarization stabilizer additive for electroplating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0355939 A1
- Document ID: US20160355939A1
- Status: Published application
- Kind: A1
- Application number: 14/732,306
- Filed: 2015-06-05
- Published: 2016-12-08
- Earliest claimed: 2015-06-05
- Assignees: Lam Research Corporation
- Applicants: Lam Research Corporation
- Inventors: Matthew Sherman Thorum
- Web page: https://patentgrep.com/patent/US20160355939A1

## CPC

- C25D 3/38: of copper
- C25D 5/02: Electroplating of selected surface areas
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

Provided herein are methods and apparatus for electroplating metal into recessed features. The techniques described herein utilize a polarization stabilizer compound to increase the stability of polarization at the substrate-electrolyte interface over time. Polarization stabilizers minimize changes in polarization to achieve improved plating results for a single substrate, and more uniform plating results over the course of several substrates. Furthermore, the polarization stabilizers discussed herein may be used to extend the lifetime of a particular electrolyte, thereby reducing manufacturing costs.

## Claims

### Claim 1

A method of electroplating copper on a workpiece, the method comprising:
(a) contacting a surface of the workpiece with an electroplating solution comprising copper ions, a suppressor, an accelerator, and a polarization stabilizer compound comprising a phenol group; and
(b) applying a negative potential to the workpiece to thereby electroplate copper onto the surface of the workpiece, wherein electroplating occurs over a duration of at least about 10 minutes.

### Claim 2 (depends on 1)

The method of claim 1, wherein the polarization stabilizer compound comprises two phenol groups.

### Claim 3 (depends on 2)

The method of claim 2, wherein the polarization stabilizer compound is a bisphenol compound.

### Claim 4 (depends on 3)

The method of claim 3, wherein the bisphenol compound is bisphenol A.

### Claim 5 (depends on 3)

The method of claim 3, wherein the bisphenol compound is bisphenol S.

### Claim 6 (depends on 1)

The method of claim 1, wherein the polarization stabilizer compound is an antioxidant.

### Claim 7 (depends on 1)

The method of claim 1, wherein the polarization stabilizer compound contains no nitrogen atoms.

### Claim 8 (depends on 1)

The method of claim 1, wherein applying the negative potential to the workpiece produces a current density on the surface of the workpiece of about 5 mA/cm2 or less, on average, over the course of the electroplating.

### Claim 9 (depends on 8)

The method of claim 8, wherein the electroplating is conducted for a duration of at least about 20 minutes.

### Claim 10 (depends on 8)

The method of claim 8, wherein the electroplating is conducted for a duration of at least about 60 minutes.

### Claim 11 (depends on 1)

The method of claim 1, wherein the surface of the workpiece comprises recessed features.

### Claim 12 (depends on 11)

The method of claim 11, wherein the recessed features are through silicon vias.

### Claim 13 (depends on 1)

The method of claim 1, wherein during the electroplating, the polarization of the workpiece-electroplating solution interface does not vary by more than about 0.02 V for at least about 20 minutes.

### Claim 14 (depends on 1)

The method of claim 1, wherein the polarization stabilizer compound provides leveling characteristics to the electroplating solution.

### Claim 15 (depends on 1)

The method of claim 1, wherein the copper ions are present in the electroplating solution at a concentration of between about 40-70 g/L.

### Claim 16 (depends on 1)

The method of claim 1, wherein the electroplating solution further comprises an acid, and wherein the electroplating solution has a pH of at most about 2.

### Claim 17 (depends on 1)

The method of claim 1, wherein the accelerator comprises at least one material selected from the group consisting of: dimercaptopropane sulfonic acid, dimercaptoethane sulfonic acid, mercaptopropane sulfonic acid, mercaptoethane sulfonic acid, bis-(3-sulfopropyl) disulfide (SPS), and derivatives thereof.

### Claim 18 (depends on 1)

The method of claim 1, wherein the suppressor comprises at least one material selected from the group consisting of: polyethylene oxide, polypropylene oxide, polyethylene glycol, and polypropylene glycol, any of which may optionally include S- and/or N-containing functional groups.

### Claim 19 (depends on 1)

The method of claim 1, wherein the electroplating solution does not contain a leveler.

### Claim 20 (depends on 1)

The method of claim 1, wherein the polarization stabilizer compound is provided at a concentration of about 10 ppm or less.