# US 2016/0355937 A1 · System and method for parallel solultion extraction of one or more metal values from metal-bearing materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0355937 A1
- Document ID: US20160355937A1
- Status: Published application
- Kind: A1
- Application number: 15/240,383
- Filed: 2016-08-18
- Published: 2016-12-08
- Earliest claimed: 2011-12-20
- Assignees: Freeport Minerals Corporation
- Applicants: Freeport Minerals Corporation
- Inventors: Anand Raman; Jason M. Morgan; Barbara J. Savage; David G. Meadows; Wayne W. Hazen
- Web page: https://patentgrep.com/patent/US20160355937A1

## CPC

- C25C 1/22: of metals not provided for in groups C25C1/02 - C25C1/20
- B01D 11/0488: {Flow sheets}
- C22B 3/02: Apparatus therefor
- C22B 3/26: by liquid-liquid extraction using organic compounds
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- C22B 11/04: {by wet processes (extraction of metal compounds by leaching in organic solutions C22B3/16; treatment or purification of solutions by liquid-liquid extraction C22B3/26)}
- C22B 19/00: Obtaining zinc or zinc oxide
- C22B 23/0407: {Leaching processes}
- C22B 23/0453: {Treatment or purification of solutions, e.g. obtained by leaching (C22B23/0407 takes precedence)}
- C22B 23/0461: {by chemical methods}
- C22B 34/34: Obtaining molybdenum {(treatment or purification of solutions by adsorption on solids C22B3/24, by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42; preparation of molybdenum involving liquid-liquid extraction, adsorption or ion-exchange C01G39/003)}
- C22B 59/00: Obtaining rare earth metals
- C22B 60/0221: {by leaching}
- C22B 60/0252: {treatment or purification of solutions or of liquors or of slurries (C22B60/0221 takes precedence)}
- C22B 60/0278: {by chemical methods (C22B60/0256, C22B60/026, C22B60/0265 take precedence)}
- C22B 61/00: Obtaining metals not elsewhere provided for in this subclass (iron C21)
- C25C 1/00: Electrolytic production, recovery or refining of metals by electrolysis of solutions (C25C5/00 takes precedence)
- C25C 1/08: of nickel or cobalt
- C25C 1/10: of chromium or manganese
- C25C 7/00: Constructional parts, or assemblies thereof, of cells; Servicing or operating of cells (for the production of aluminium C25C3/06 - C25C3/22)
- Y02P 10/20: Recycling
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present disclosure relates to a process and system for recovery of one or more metal values using solution extraction techniques and to a system for metal value recovery. In an exemplary embodiment, the solution extraction system comprises a first solution extraction circuit and a second solution extraction circuit. A first metal-bearing solution is provided to the first and second circuit, and a second metal-bearing solution is provided to the first circuit. The first circuit produces a first rich electrolyte solution, which can be forwarded to primary metal value recovery, and a low-grade raffinate, which is forwarded to secondary metal value recovery. The second circuit produces a second rich electrolyte solution, which is also forwarded to primary metal value recovery. The first and second solution extraction circuits have independent organic phases and each circuit can operate independently of the other circuit.

## Claims

### Claim 1

(canceled)

### Claim 2

A metal value recovery system comprising:
a primary metal value recovery system;
a secondary metal value recovery system; and
a solution extraction system comprising:
a first solution extraction circuit coupled to the primary metal value recovery system and to the secondary metal value recovery system, and
a second solution extraction circuit coupled to the primary metal value recovery system.

### Claim 3 (depends on 2)

The system of claim 2, wherein the primary metal value recovery system comprises one of an electrowinning circuit, a sulphidation system, a precipitation system, and an ion exchange system.

### Claim 4 (depends on 3)

The system of claim 3, wherein the primary metal value recovery system comprises an electrowinning circuit.

### Claim 5 (depends on 2)

The system of claim 2, wherein the first solution extraction circuit and the second solution extraction circuit are configured to produce a rich electrolyte.

### Claim 6 (depends on 5)

The system of claim 5, wherein the rich electrolyte is in fluid communication with the primary metal value recovery system.

### Claim 7 (depends on 5)

The system of claim 5, wherein the first solution extraction circuit is configured to produce a high-grade raffinate and a low-grade raffinate.

### Claim 8 (depends on 7)

The system of claim 7, wherein the low-grade raffinate is in fluid communication with the secondary metal value recovery system.

### Claim 9 (depends on 8)

The system of claim 8, wherein the secondary metal value recovery system is configured to perform a selective precipitation process to produce a precipitated metal ion and a secondary electrolyte.

### Claim 10 (depends on 9)

The system of claim 9, wherein the precipitated metal ion is uranium.

### Claim 11 (depends on 9)

The system of claim 9, wherein the low-grade raffinate comprises a secondary metal value.

### Claim 12 (depends on 11)

The system of claim 11, wherein the secondary metal value recovery system further comprises a secondary electrowinning circuit configured to extract a secondary metal value from the secondary electrolyte.

### Claim 13 (depends on 12)

The system of claim 12, wherein the secondary metal value is cobalt.

### Claim 14 (depends on 5)

The system of claim 5, wherein the high-grade raffinate is recycled to a reactive processing system.

### Claim 15

A system for extracting metal value comprising:
a solution extraction system comprising a first circuit and a second circuit,
wherein the first circuit is configured to receive a first metal bearing solution and to produce a first rich electrolyte;
wherein the second circuit is configured to receive the first metal bearing solution and to produce a second rich electrolyte; and
wherein the first circuit is configured to receive a second metal bearing solution and to produce a low-grade raffinate;
a primary electrowinning circuit configured to extract a primary metal value from the first rich electrolyte and the second rich electrolyte; and
a secondary metal value recovery system configured to extract a secondary metal value from the low-grade raffinate.

### Claim 16 (depends on 15)

The system of claim 15, wherein the low-grade raffinate comprises a secondary metal value comprising at least one of silver, platinum group metals, molybdenum, zinc, nickel, cobalt, uranium, rhenium, rare earth and actinide metals.

### Claim 17 (depends on 16)

The system of claim 16, wherein the secondary metal value recovery system is configured to perform a selective precipitation process to precipitate a metal ion.

### Claim 18 (depends on 17)

The system of claim 17, wherein the metal ion comprises uranium.

### Claim 19 (depends on 18)

The method of claim 18, wherein the secondary metal value recovery system comprises a secondary electrowinning circuit.

### Claim 20 (depends on 19)

The method of claim 19, wherein the secondary metal value comprises cobalt.

### Claim 21 (depends on 20)

The method of claim 20, wherein the second metal-bearing solution is a low-grade pregnant leach solution.