# US 2016/0355916 A1 · Method for manufacturing products made of aluminium-copper-lithium alloy with improved fatigue properties, and distributor for this method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0355916 A1
- Document ID: US20160355916A1
- Status: Published application
- Kind: A1
- Application number: 15/102,965
- Filed: 2014-12-11
- Published: 2016-12-08
- Earliest claimed: 2013-12-13
- Assignees: Constellium Issoire
- Applicants: Constellium Issoire
- Inventors: Armelle DANIELOU; Soizic BLAIS; Philippe JARRY; Olivier RIBAUD; Bernard VALENTIN
- Web page: https://patentgrep.com/patent/US20160355916A1

## CPC

- C22F 1/057: of alloys with copper as the next major constituent
- B21B 1/22: for rolling {plates, strips,} bands or sheets of indefinite length (B21B1/42 takes precedence)
- B21C 23/212: {Details (B21C23/217, B21C23/218 take precedence)}
- B21J 5/00: Methods for forging, hammering, or pressing (for working sheet-metal or metal tubes, rods, or profiles B21D; for working wire B21F); Special equipment or accessories therefor
- B22D 11/003: {Aluminium alloys}
- B22D 11/0408: {Moulds for casting thin slabs}
- B22D 11/041: for vertical casting (B22D11/043, B22D11/049 - B22D11/059 take precedence)
- B22D 11/059: Mould materials or platings
- B22D 21/007: {with low melting point, e.g. Al 659 degrees C, Mg 650 degrees C}
- C22C 1/026: {Alloys based on aluminium}
- C22C 21/12: with copper as the next major constituent
- C22C 21/14: with silicon
- C22C 21/16: with magnesium
- C22C 21/18: with zinc
- B21B 2003/001: {Aluminium or its alloys}
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- B21C: MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES, PROFILES OR LIKE SEMI-MANUFACTURED PRODUCTS OTHERWISE THAN BY ROLLING; AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL
- B21J: FORGING; HAMMERING; PRESSING METAL; RIVETING; FORGE FURNACES (rolling of metal B21B; making particular products by forging or pressing B21K; cladding or plating B23K; finishing surfaces by hammering B23P9/04; compacting surfaces by blasting with particulate material B24C1/10; general features of presses, presses for consolidating scrap B30B; furnaces in general F27)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The invention relates to a method for manufacturing an aluminium alloy product including the steps of: creating a bath of liquid metal in an aluminium-copper-lithium alloy, casting said alloy by vertical semi-continuous casting so as to obtain a plate with thickness T and width W such that, during solidification, the hydrogen content of said liquid metal bath (1) is lower than 0.4 ml/100 g, the oxygen content above the liquid surface (14, 15) is less than 0.5% by volume.

## Claims

### Claim 1

Method of manufacturing an aluminum alloy product comprising
(a) Preparing a bath of molten alloy metal comprising, as a percentage by weight, Cu: 2.0-6.0; Li: 0.5-2.0; Mg: 0-1.0; Ag: 0-0.7; Zn 0-1.0; and at least one element selected from Zr, Mn, Cr, Sc, Hf and Ti, the amount of said element, if selected, being 0.05 to 0.20 wt % for Zr, 0.05 to 0.8% wt %t for Mn, 0.05 to 0.3 wt % for Cr and for Sc, 0.05 to 0.5 wt % Hf and 0.01 to 0.15% wt % for Ti, Si≦0.1; Fe≦0.1; others ≦0.05 each and ≦0.15 in total,
(b) said alloy is cast by vertical semi-continuous casting to obtain a slab of thickness T and width W so that upon solidification,
the hydrogen content of said molten metal bath is less than about 0.4 ml/100 g,
the oxygen content measured above the liquid surface is less than about 0.5% by volume,
a distributor device used for casting is made of fabric comprising essentially carbon; said distributor device comprises a lower face, an upper face defining the opening through which the molten metal is introduced and a wall of substantially rectangular section, the wall comprising two longitudinal portions parallel with width W and two transverse portions parallel with thickness T, said transverse and longitudinal portions being formed from at least two fabrics, a first substantially sealing and semi-rigid fabric ensuring that the distributor device keeps shape during casting, and a second non-sealing fabric allowing the passage and filtration of liquid, said first and second fabrics being bonded to each other without overlap or with overlap and no gap separating them, said first fabric continuously covering at least 30% of the surface of wall portions and being positioned so that a liquid surface is in contact therewith over an entire section.

### Claim 2 (depends on 1)

The method according to claim 1 wherein the oxygen content of the atmosphere in contact with the liquid metal bath in a smelter during degassing, filtration is less than 0 5% by volume and optionally wherein the oxygen content of the atmosphere in contact with the liquid metal bath is less than 0 5% by volume for the entire casting facility.

### Claim 3 (depends on 1)

The method according to claim 1 wherein a lid covers the liquid surface during solidification, said lid optionally comprising seals to ensure a leak tight seal with a casting table and wherein an inert gas is introduced into a chamber defined between the lid and the casting table and wherein suction is maintained in a casting pit by means of a pump, optionally so that the pressure within a containment is less than the pressure in the chamber.

### Claim 4 (depends on 1)

The method according to claim 1 in which a molten salt containing lithium is not used throughout the entire casting facility.

### Claim 5 (depends on 1)

The method according to claim 1 in which said distributor device is such that the first fabric has a height hl as measured from the upper face on the circumference of a wall such that h1≧0.3 h and optionally h1≧0.5 h, where h is the total height of a wall of the distributor device.

### Claim 6 (depends on 1)

The method according to claim 1 in which the height of a wall immersed in liquid metal of the distributor device covered by the first fabric is selected from the group consisting of at least 20%, 40%, and 60% of the total height of the immersed wall.

### Claim 7 (depends on 1)

The method according to claim 1 in which a surface portion covered by the first fabric is from 30 and 90%, and optionally from 50 and 80% for longitudinal portions and, and/or from 30 and 70% and optionally from 40 and 60% for lateral portions, and/or from 30 and 100% and optionally from 50 and 80% for a bottom.

### Claim 8 (depends on 1)

The method according to claim 1 wherein after (a) and (b),
(c) Homogenizing said slab before or after optionally machining to obtain a shape that can be hot-worked,
(d) said homogenized shape is then hot-worked and optionally cold-worked to obtain a wrought product.
(e) said wrought product is solution heat-treated and quenched,
(f) optionally said wrought product that has undergone solution heat treatment is stress-relieved by plastic deformation with a deformation of at least 1%,
(g) said solution heat-treated and optionally stress relieved product is subjected to aging.

### Claim 9 (depends on 1)

The method according to claim 1 wherein said hot working and/or cold-working is performed by extrusion, rolling and/or forging.

### Claim 10 (depends on 1)

The method according to any of claim 1 wherein said wrought product has a thickness of at least 80 mm

### Claim 11 (depends on 8)

The method according to claim 8 in which the deformation ratio during (d) is lower than 85%, and optionally lower than 80%.

### Claim 12 (depends on 1)

The method according to claim 1 in which the alloy comprises, as a percentage by weight, Cu: 3.0-3.9; Li: 0.7-1.3; Mg: 0.1 to 1.0, at least one element selected from Zr, Mn and Ti, the amount of said element, if selected, is from 0.06 to 0.15 wt % for Zr, 0.05 to 0.8 wt % for Mn and 0.01 to 0.15% by weight for Ti; Ag: 0-0.7; Zn≦0.25; Si≦0.08; Fe≦0.10; others ≦0.05 each and ≦0.15 in total.

### Claim 13

Distributor used for semi-continuous casting of aluminum alloy slabs made of fabric comprising essentially carbon, having a lower face, an upper face defining an opening through which the molten metal is introduced and a wall of substantially rectangular section, the wall comprising two longitudinal portions parallel with width W and two transverse portions parallel with thickness T, said transverse and longitudinal portions being formed from at least two fabrics, a first substantially sealing and semi-rigid fabric ensuring that the distributor device keeps shape during casting, and a second non-sealing fabric allowing passage and filtration of liquid, said first and second fabrics being bonded to each other without overlap or with overlap and no gap separating them, said first fabric continuously covering at least 30% of the surface of wall portions and being positioned so that a liquid surface is in contact therewith over an entire section.

### Claim 14 (depends on 13)

Distributor according to claim 13 wherein the first fabric has a height h1 as measured from the upper face on the circumference of the wall such that h1≧0.3 h and optionally h1≧0.5 h, where h is the total height of a wall of the distributor device.

### Claim 15 (depends on 13)

Distributor according to claim 13 wherein the section of the wall changes linearly as a function of height h, optionally so that a surface of a lower face of the distributor is higher or lower by at most 10% than a surface of an upper face of the distributor.

### Claim 16 (depends on 13)

Distributor according to claim 13 wherein a surface portion covered by the first fabric is between 30 and 90%, and preferably optionally between 50 and 80% for longitudinal portions, and/or between 30 and 70% and preferably optionally between 40 and 60% for lateral portions, and/or between 30 and 100% and preferably between 50 and 80% for a bottom.

### Claim 17 (depends on 13)

Distributor according to claim 13 wherein length L1 of the first fabric located in a bottom is greater than length L2 of the first fabric in a portion of longitudinal walls in contact with the bottom.

### Claim 18 (depends on 13)

Distributor according to claim 13 wherein the first fabric and the second fabric are obtained by weaving a graphite wire.

### Claim 19 (depends on 18)

Distributor according to claim 18 wherein the wire is coated with a layer to facilitate sliding.

### Claim 20 (depends on 13)

Distributor according to any of claim 13 wherein the first fabric is substantially sealing, optionally having a mesh size of less than 0.5 mm, optionally less than 0.2 mm and/or the second fabric is non-sealing and allows molten metal to pass through, optionally having a mesh size of between 1 and 5 mm, optionally 2 to 4 mm.