# US 2016/0355914 A1 · Aluminum alloy plastic worked article, method for manufacturing the same, and automobile component

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0355914 A1
- Document ID: US20160355914A1
- Status: Published application
- Kind: A1
- Application number: 15/025,297
- Filed: 2015-02-10
- Published: 2016-12-08
- Earliest claimed: 2015-02-10
- Assignees: Showa Denko K.K.
- Applicants: Showa Denko K.K.
- Inventors: Hideki TAKEMURA
- Web page: https://patentgrep.com/patent/US20160355914A1

## CPC

- C22F 1/047: of alloys with magnesium as the next major constituent
- B22D 21/007: {with low melting point, e.g. Al 659 degrees C, Mg 650 degrees C}
- B60G 7/001: {Suspension arms, e.g. constructional features (B60G7/006 takes precedence)}
- C22C 21/02: with silicon as the next major constituent
- C22C 21/08: with silicon
- C22F 1/04: of aluminium or alloys based thereon
- C22F 1/043: of alloys with silicon as the next major constituent
- C22F 1/05: of alloys of the Al-Si-Mg type, i.e. containing silicon and magnesium in approximately equal proportions
- B60G 2206/10: Constructional features of arms
- B60G 2206/124: the arm having triangular or Y-shape, e.g. wishbone
- B60G 2206/7101: Fiber-reinforced plastics [FRP]
- B60G 2206/7102: Aluminium alloys
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- B60G: VEHICLE SUSPENSION ARRANGEMENTS (air-cushion vehicles B60V; {cycle suspensions B62K25/00})
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

To provide an aluminum alloy plastic worked article in which an aluminum texture state having preferable corrosion resistance and preferable mechanical characteristics in terms of, for example, the strength, the proof stress, and the elongation is formed. In an aluminum alloy plastic worked article including a plastic worked portion which is formed of a thinned portion 22 formed by plastic working and rib portions 21 formed at two ends of this thinned portion 22 and which has an approximately H-shaped or U-shaped cross-section, the plastic worked portion is a plastic worked portion 2 having strain portions 23 in each of which an equivalent strain of up to 4.0 mm/mm generated by plastic working is present, and the strain portions 23 are each located in the vicinity of the surface of the plastic worked portion 2 at a boundary between the thinned portion 22 and each of the rib portions 21 and are each formed of a non-recrystalline texture N of aluminum (atomic symbol: Al) which is not recrystallized or are each formed of the non-recrystalline texture N and a fine crystalline texture M which is recrystallized but has a crystal grain of 500 μm or less.

## Claims

### Claim 1

An aluminum alloy plastic worked article characterized by comprising: a plastic worked portion which is formed of a thinned portion formed by plastic working and rib portions formed at two ends of this thinned portion and which has an approximately H-shaped or U-shaped cross section,
wherein the plastic worked portion has strain portions in each of which an equivalent strain of up to 4.0 mm/mm generated by the plastic working is present,
the strain portions are each located in the vicinity of the surface of the plastic worked portion at a boundary between the thinned portion and each of the rib portions, and
the strain portions are each formed of a non-recrystalline texture of aluminum (atomic symbol: Al) which is not recrystallized or are each formed of the non-recrystalline texture and a fine crystalline texture of the aluminum which is recrystallized but has a crystal grain of 500 μm or less.

### Claim 2 (depends on 1)

The aluminum alloy plastic worked article according to claim 1, characterized in that
the composition contains 0.15 to 0.5 percent by mass of copper (atomic symbol: Cu), 0.8 to 1.15 percent by mass of magnesium (atomic symbol: Mg), 0.95 to 1.15 percent by mass of silicon (atomic symbol: Si), 0.4 to 0.6 percent by mass of manganese (atomic symbol: Mn), 0.2 to 0.3 percent by mass of iron (atomic symbol: Fe), 0.11 to 0.19 percent by mass of chromium (atomic symbol: Cr), 0.25 percent by mass or less of zinc (atomic symbol: Zn), 0.05 percent by mass or less of zirconium (atomic symbol: Zr), 0.012 to 0.035 percent by mass of titanium (atomic symbol: Ti), 0.0001 to 0.03 percent by mass of boron (atomic symbol: B), and the balance including aluminum and inevitable impurities, and
when a width direction length of the rib portion is represented by x (cm), a height direction length of the thinned portion is represented by y (cm), and a height direction length of the rib portion is represented by z (cm), the content (percent by mass) of the manganese satisfies the following equation [Eq. 1]
Manganese (percent by mass)=0.4α{z/(x+y)+0.25} [Eq. 1]
where z/(x+y)≧0.65 and α=0.8 to 0.9 hold.

### Claim 3 (depends on 1)

The aluminum alloy plastic worked article according to claim 1, characterized by being an automobile component.

### Claim 4 (depends on 1)

A method for manufacturing the aluminum alloy plastic worked article according to claim 1, characterized in that
melting/casting is performed, and after a homogenizing treatment and plastic working are performed on a cast product obtained by the melting/casting, a solution treatment, a water quenching treatment, and an artificial age hardening treatment are performed.

### Claim 5 (depends on 4)

The method for manufacturing the aluminum alloy plastic worked article according to claim 4, characterized in that
the artificial age hardening treatment is performed at an aging treatment temperature of 170° C. to 210° C. for an aging treatment time of 0.5 to 18 hours.

### Claim 6 (depends on 4)

The method for manufacturing the aluminum alloy plastic worked article according to claim 4, characterized in that
the solution treatment is performed at a solution treatment temperature of 520° C. to 560° C., and
the water quenching treatment is performed at a water quenching treatment temperature of 70° C. or less.

### Claim 7 (depends on 4)

The method for manufacturing the aluminum alloy plastic worked article according to claim 4, characterized in that
the plastic working is performed by at least one type selected from extruding, forging, and rolling.

### Claim 8 (depends on 4)

An automobile component characterized by being obtained by the method for manufacturing the aluminum alloy plastic worked article according to claim 4.