# US 2016/0355906 A1 · Method of ore processing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0355906 A1
- Document ID: US20160355906A1
- Status: Published application
- Kind: A1
- Application number: 15/241,200
- Filed: 2016-08-19
- Published: 2016-12-08
- Earliest claimed: 2011-01-25
- Assignees: The University of Queensland
- Applicants: The University of Queensland
- Inventors: James VAUGHAN; William HAWKER
- Web page: https://patentgrep.com/patent/US20160355906A1

## CPC

- C22B 23/0476: {Separation of nickel from cobalt}
- C22B 3/045: {Leaching using electrochemical processes}
- C22B 15/0067: {with acids or salts thereof}
- C22B 19/22: {with leaching with acids}
- C22B 23/0415: {with acids or salt solutions except ammonium salts solutions}
- C22B 23/043: {Sulfurated acids or salts thereof}
- C22B 23/0461: {by chemical methods}
- C25C 1/08: of nickel or cobalt
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of selectively leaching a metal such as nickel from an ore or ore processing intermediate comprising the metal and cobalt. The ore or ore processing intermediate is contacted with an acidic leach solution comprising an amount of an oxidising agent sufficient to oxidise a major portion of the cobalt to thereby cause it to be stabilised in the solid phase while a major portion of the metal is dissolved for subsequent recovery.

## Claims

### Claim 1

A method of selectively leaching a metal selected from the group consisting of nickel, copper and zinc from a solid ore or solid ore processing intermediate comprising the metal and cobalt, the method including:
a) providing a mixture comprising an acidic leach solution and an oxidising agent; and
b) mixing the mixture with the solid ore or solid ore processing intermediate,
wherein there is sufficient oxidising agent to stabilize greater than 95% by mass of the cobalt to cause it to be stabilised in a solid phase while greater than 50% by mass of the metal is selectively dissolved.

### Claim 2 (depends on 1)

The method of claim 1, wherein greater than 70% by mass of the metal is selectively dissolved.

### Claim 3 (depends on 1)

The method of claim 1, wherein greater than 90% by mass of the metal is selectively dissolved.

### Claim 4 (depends on 1)

The method of claim 1 wherein the metal is nickel.

### Claim 5 (depends on 1)

The method of claim 1 wherein the solid ore or solid ore processing intermediate is a mixed nickel-cobalt hydroxide precipitate.

### Claim 6 (depends on 1)

The method of claim 1 wherein the oxidising agent has sufficient oxidising potential to oxidise cobalt(II) to cobalt(III).

### Claim 7 (depends on 6)

The method of claim 6 wherein the oxidising agent has an oxidative potential of greater than about 0.5 V (SHE).

### Claim 8 (depends on 6)

The method of claim 6 wherein the oxidising agent has an oxidative potential of greater than 0.5 V to 3.0 V (SHE).

### Claim 9 (depends on 1)

The method of claim 1 wherein the acidic leach solution has a pH from about 1 to about 6.

### Claim 10 (depends on 9)

The method of claim 9 wherein the acidic leach solution has a pH from about 2 to about 5.

### Claim 11 (depends on 8)

The method of claim 8 wherein the oxidising agent has an oxidative potential of about 0.5 V to about 3.0 V (SHE) at a pH from 0 to 6.

### Claim 12 (depends on 11)

The method of claim 11 wherein the oxidising agent has an oxidative potential of about 0.5 V to about 1.0 V (SHE) at a pH from 4 to 6.

### Claim 13 (depends on 11)

The method of claim 11 wherein the oxidising agent has an oxidative potential of about 1.0 V to about 2.0 V (SHE) at a pH from 1 to 4.

### Claim 14 (depends on 1)

The method of claim 1 wherein the oxidising agent is selected from the group consisting of persulphates, peroxides, permanganates, perchlorates, ozone, oxides and chlorine.

### Claim 15 (depends on 1)

The method of claim 1 further including a step of controlling addition of the oxidising agent.

### Claim 16 (depends on 1)

The method of claim 1 further including a step of heating the acidic leach solution to greater than 50° C.

### Claim 17 (depends on 1)

The method of claim 1 wherein a majority of the metal has been leached into the acidic leach solution from the solid ore or solid ore processing intermediate after 1 to 5 hours.

### Claim 18 (depends on 1)

The method of claim 1 wherein the oxidising agent is present in the acidic leach solution in 80% to 200% stoichiometric equivalents to combined cobalt and manganese in the solid ore or solid ore processing intermediate.

### Claim 19 (depends on 1)

The method of claim 1 wherein the solid ore or solid ore processing intermediate further comprises manganese and treatment with the amount of oxidising agent causes a major portion of the manganese to be stabilised in a solid phase while a major portion of the metal is dissolved.

### Claim 20 (depends on 1)

The method of claim 1 wherein, after leaching is complete, extracted metal can be recovered directly from the acidic leach solution by electrowinning or hydrogen reduction.

### Claim 21

A method of recovering nickel and cobalt from a mixed nickel-cobalt hydroxide precipitate including the steps of:
(a) providing a mixture comprising an acidic leach solution and an oxidising agent, wherein there is sufficient oxidising agent to stabilise greater than 95% by mass of the cobalt to cause it to be stabilized in the solid phase while greater than 50% by mass of the nickel is selectively dissolved;
(b) mixing the mixture with the mixed nickel-cobalt hydroxide precipitate,
(c) separating the cobalt in the solid phase from the acidic leach solution containing dissolved nickel to recover the cobalt in the solid phase; and
(d) recovering the nickel from the acidic leach solution.

### Claim 22 (depends on 21)

The method of claim 21 wherein the mixed nickel-cobalt hydroxide precipitate further comprises manganese and addition of an amount of oxidising agent also causes a major portion of the manganese to be stabilised in a solid phase.