# US 2016/0355900 A1 · Process for manufacturing cold-rolled and annealed steel sheet with a very high strength, and sheet thus produced

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0355900 A1
- Document ID: US20160355900A1
- Status: Published application
- Kind: A1
- Application number: 15/243,610
- Filed: 2016-08-22
- Published: 2016-12-08
- Earliest claimed: 2007-05-11
- Assignees: ArcelorMittal
- Applicants: ArcelorMittal
- Inventors: Javier Gil Otin; Antoine Moulin
- Web page: https://patentgrep.com/patent/US20160355900A1

## CPC

- C21D 9/46: for sheet metals
- B22D 11/001: {of specific alloys}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 9/52: for wires; for strips {; for rods of unlimited length}
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/22: with molybdenum or tungsten
- C22C 38/28: with titanium or zirconium
- C22C 38/32: with boron
- C22C 38/38: with more than 1.5% by weight of manganese
- C23G 1/00: Cleaning or pickling metallic material with solutions or molten salts (with organic solvents C23G5/02)
- C23G 1/08: Iron or steel
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23G: CLEANING OR DE-GREASING OF METALLIC MATERIAL BY CHEMICAL METHODS OTHER THAN ELECTROLYSIS

## Abstract

The present invention provides a cold-rolled and annealed steel sheet with a strength greater than 1200 MPa, the composition of which includes, the contents being expressed by weight: 0.10%≦C≦0.25%, 1%≦Mn≦3%, A≧0.010%, Si≦2.990%, S≦0.015%, P≦0.1%, N≦0.008%, it being understood that 1%≦Si+Al≦3%, it being understood that Cr+3Mo≧0.3%, Ti in an amount such that Ti/N≧4 and Ti≦0.040%. A balance of the composition includes iron and inevitable impurities resulting from the smelting. The microstructure of the steel includes 15 to 90% bainite, the remainder includes martensite and residual austenite.

## Claims

### Claim 1

A cold-rolled and annealed steel sheet with a strength greater than 1200 MPa, the composition the composition of which comprises, the contents being expresses by weight:
0.10%≦C≦0.25%
1%≦Mn≦3%
Al≧0.010%
Si≦2.990%
S≦0.015%
P≦0.1% and
N≦0.008%,
it being understood that
1%≦Si+Al≦3%,
the composition optionally comprising:
0.05%≦V≦0.15%
B≦0.005%
Mo≦0.25%
Cr≦1.65%,
it being understood that
Cr+3Mo≧0.3%, and
Ti in an amount so that Ti/N≧4 and Ti≦0.040%,
the balance of the composition consisting of iron and inevitable impurities resulting from the smelting, the microstructure of said steel comprising 15 to 90% bainite, the remainder consisting of islands of martensite and residual austenite.

### Claim 2 (depends on 1)

The steel sheet as claimed in claim 1, with an elongation at break greater than 10%, wherein:
Mo<0.005%
Cr<0.005% and
B=0%,
the microstructure of said steel comprising 65 to 90% bainite, the remainder consisting of islands of martensite and residual austenite.

### Claim 3 (depends on 1)

The steel sheet as claimed in claim 1, wherein it includes:
Mo≦0.25% and
Cr≦1.65%,
it being understood that
Cr+3Mo≧0.3%, and
B=0%,
the microstructure of said steel comprising 65 to 90% bainite, the remainder consisting of islands of martensite and residual austenite.

### Claim 4 (depends on 1)

The steel sheet as claimed in claim 1, with a strength greater than 1400 MPa and an elongation at break greater than 8%, wherein it includes:
Mo≦0.25% and
Cr≦1.65%,
it being understood that
Cr+3Mo≧0.3%,
the microstructure of said steel comprising 45 to 65% bainite, the remainder consisting of islands of martensite and residual austenite.

### Claim 5 (depends on 1)

The steel sheet as claimed in claim 1, with a strength greater than 1600 MPa and an elongation at break greater than 8%, wherein it includes:
Mo≦0.25% and
Cr≦1.65%,
it being understood that
Cr+3Mo≧0.3%,
the microstructure of said steel comprising 15 to 45% bainite, the remainder consisting of martensite and residual austenite.

### Claim 6 (depends on 1)

The steel sheet as claimed in claim 1, characterized ion that the composition of said steel includes, the content being expressed by weight:
0.19%≦C≦0.23%.

### Claim 7 (depends on 1)

The steel sheet as claimed in claim 1, characterized ion that the composition of said steel includes, the content being expressed by weight:
1.5%≦Mn≦2.5%.

### Claim 8 (depends on 1)

The steel sheet as claimed in claim 1, characterized ion that the composition of said steel includes, the content being expressed by weight:
1.2%≦Si≦1.8%.

### Claim 9 (depends on 1)

The steel sheet as claimed in claim 1, characterized ion that the composition of said steel includes, the content being expressed by weight:
1.2%≦Al≦1.8%.

### Claim 10 (depends on 1)

The steel sheet as claimed in claim 1, characterized in that the composition of said steel includes, the contents being expressed by weight:
0.05%≦V≦0.15%
0.0045≦N≦0.008%.

### Claim 11 (depends on 1)

The steel sheet as claimed in claim 1, characterized in that the composition of said steel includes, the contents being expressed by weight: 0.12%≦V≦0.15%.

### Claim 12 (depends on 1)

The steel sheet as claimed in claim 1, characterized in that the composition of said steel includes, the content being expressed by weight: 0.00055≦B≦0.003%.

### Claim 13 (depends on 1)

The steel sheet as claimed in claim 1, characterized in that the the average size of said islands of martensite and residual austenite is less than 1 micron, and the average distance between said islands is less than 6 microns.

### Claim 14 (depends on 2)

A process for manufacturing a cold-rolled steel sheet with a strength greater than 1200 MPa and an elongation at break greater than 10%, in which:
a steel is provided having a composition as claimed in claim 2; then
a semifinished product is cast from this steel; then
said semifinished product is brought to a temperature greater than 1150° C.; then
said semifinished product is hot-rolled so as to obtain a hot-rolled sheet; then
said sheet is coiled; then
said hot-rolled sheet is pickled; then
said sheet is cold-rolled with a reduction ratio of between 30 and 80% so as to obtain a cold-rolled sheet; and then
said cold-rolled sheet is reheated at a rate Vc between 5 and 15° C./s up to a temperature T1 between Ac3 and Ac3+20° C., and held there for a time t1 between 50 and 150 s, then said sheet is cooled at a rate VR1 greater than 40° C./s but below 100° C./s down to a temperature T2 between (Ms−30° C. and Ms+30° C.), said sheet is maintained at said temperature T2 for a time t2 between 150 and 350 s and then it is cooled at a rate VR2 of less than 30° C./s down to the ambient temperature.

### Claim 15 (depends on 1)

A process for manufacturing a cold-rolled steel sheet with a strength greater than 1200 MPa and an elongation at break greater than 8%, in which:
a steel is provided having a composition as claimed in claim 1, the Mo and Cr contents being Mo≦0.25% and Cr≦1.65%, it being understood that: Cr+3Mo≧0.3%; then
a semifinished product is cast from this steel; then
said semifinished product is brought to a temperature greater than 1150° C.; then
said semifinished product is hot-rolled so as to obtain a hot-rolled sheet; then
said sheet is coiled; then
said hot-rolled sheet is pickled; then
said sheet is cold-rolled with a reduction ratio of between 30 and 80% to obtain a cold-rolled sheet; and then
said cold-rolled sheet is reheated at a rate Vc between 5 and 15° C./s up to a temperature T1 between Ac3 and Ac3+20° C., and held there for a time t1 between 50 and 150 s, then said sheet is cooled at a rate VR1 greater than 25° C./s but below 100° C./s down to a temperature T2 between Bs and (Ms−20° C.), said sheet is maintained at said temperature T2 for a time t2 between 150 and 350 s and then it is cooled at a rate VR2 of less than 30° C./s down to the ambient temperature.

### Claim 16 (depends on 14)

The manufacturing process as claimed in claim 14, characterized in that the temperature T1 is between Ac3+10° C. and Ac3+20° C.

### Claim 17 (depends on 1, 14)

The use of a cold-rolled and annealed steel sheet as claimed in claim 1, or manufactured by process as claimed in claim 14, for the manufacture of structural parts or reinforcing elements in the automotive field.