# US 2016/0355732 A1 · Phosphor Ceramic Element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0355732 A1
- Document ID: US20160355732A1
- Status: Published application
- Kind: A1
- Application number: 15/177,212
- Filed: 2016-06-08
- Published: 2016-12-08
- Earliest claimed: 2015-06-08
- Assignees: Nitto Denko Corporation
- Applicants: Nitto Denko Corporation
- Inventors: Hiroaki Miyagawa; Ekambaram Sambandan; Bin Zhang
- Web page: https://patentgrep.com/patent/US20160355732A1

## CPC

- C09K 11/77744: {Aluminosilicates}
- C04B 35/44: based on aluminates
- C04B 35/634: Polymers (C04B35/636 takes precedence)
- C04B 35/638: Removal thereof
- C04B 2235/3224: Rare earth oxide or oxide forming salts thereof, e.g. scandium oxide
- C04B 2235/3229: Cerium oxides or oxide-forming salts thereof
- C04B 2235/3262: Manganese oxides, manganates, rhenium oxides or oxide-forming salts thereof, e.g. MnO
- C04B 2235/3418: Silicon oxide, silicic acids or oxide forming salts thereof, e.g. silica sol, fused silica, silica fume, cristobalite, quartz or flint
- C04B 2235/6025: Tape casting, e.g. with a doctor blade
- C04B 2235/6562: Heating rate
- C04B 2235/6565: Cooling rate
- C04B 2235/6567: Treatment time
- C04B 2235/6581: Total pressure below 1 atmosphere, e.g. vacuum
- C04B 2235/6586: Processes characterised by the flow of gas
- C04B 2235/661: Multi-step sintering
- C04B 2235/663: Oxidative annealing
- C04B 2235/664: Reductive annealing
- C04B 2235/764: Garnet structure A3B2(CO4)3
- C04B 2235/9646: Optical properties
- C04B 2235/9653: Translucent or transparent ceramics other than alumina
- H10H 20/8512: {Wavelength conversion materials}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

A garnet ceramic phosphor with Ce and Mn co-doping, wherein calcium and silicon in the phosphor crystal host can be minimized for enhancing performance, is described herein. Also a ceramic phosphor element comprising a garnet phosphor having composition of formula 1 or 2 is described herein: (A1-x,Cex)3(Al1-y,Mny)5-wSiwO12 (Formula 1) (Lu1-xCex)3(Al1-y,Mny)5-wSiwO12 (Formula 2).

## Claims

### Claim 1

A ceramic phosphor element comprising a garnet phosphor composition described by a formula:
(Lu1-x,Cex)3(Al1-y,Mny)5-wSiwO12
wherein x is greater than 0 and less than about 0.2;
y is greater than 0 and less than 0.1; and
w is greater than 0 and less than 0.455.

### Claim 2 (depends on 1)

The ceramic phosphor element of claim 1, wherein x is in a range of about 0.0001 to about 0.15.

### Claim 3 (depends on 1)

The ceramic phosphor of claim 1, wherein y is in a range of about 0.001 to about 0.1.

### Claim 4 (depends on 1)

The ceramic phosphor of claim 1, wherein w is in a range of about 0.005 to about 0.3.

### Claim 5 (depends on 1)

The ceramic phosphor element of claim 1, wherein the garnet phosphor composition is represented by the formula selected from the group consisting of Lu2.994Ce0.006Al4.936Mn0.032Si0.032O12, Lu2.994Ce0.006Al4.900Mn0.050Si0.050O12, Lu2.970Ce0.030Al4.900Mn0.050Si0.050O12, Lu2.940Ce0.060Al4.900Mn0.050Si0.050O12, Lu2.910Ce0.090Al4.900Mn0.050Si0.050O12, Lu2.910Ce0.090Al4.852Mn0.074Si0.074O12, Lu2.910Ce0.090Al4.708Mn0.146Si0.146O12, Lu2.880Ce0.120Al4.9Mn0.050Si0.050O12, Lu2.880Ce0.120Al4.804Mn0.098Si0.098O12, and Lu2.850Ce0.150Al4.9Mn0.050Si0.050O12.

### Claim 6 (depends on 1)

The ceramic phosphor element of claim 1, having a transmittance of at least about 70% for light having a wavelength of 800 nm.

### Claim 7 (depends on 1)

The ceramic phosphor element of claim 1, having an internal quantum efficiency of at least 75% based upon the absorption of light by the ceramic phosphor element when exposed to monochromatic light having a wavelength of 450 nm.

### Claim 8 (depends on 1)

The ceramic phosphor element of claim 1, prepared by sintering a precursor under a reducing atmosphere.

### Claim 9 (depends on 8)

The ceramic phosphor element of claim 8, wherein the sintering is carried out in an atmosphere containing H2 dispersed in N2.

### Claim 10 (depends on 8)

The ceramic phosphor of claim 8, wherein the sintering is carried out at a temperature in a range of about 1550° C. to 1900° C.

### Claim 11 (depends on 1)

The light emitting device outputting a warm-white light, comprising the ceramic phosphor element of claim 1, disposed with respect to a light source so that a portion of any light emitted from the light source is absorbed by the ceramic phosphor element, and wherein absorption of light from the light source by the ceramic phosphor element results in emission of red-shifted light by the ceramic phosphor element.

### Claim 12

A method for making a ceramic phosphor element comprising:
(a) sintering a laminate at a temperature of about 1550° C. to about 1850° C.;
(b) heating the laminate to a temperature of about 1300° C. to about 1500° C. under oxygen conditions at a near vacuum; and
(c) further heating the laminate to a temperature of about 1200° C. to about 1500° C. under a reducing atmosphere;
wherein the laminate contains a precursor composition so that the ceramic phosphor element resulting from the method has a formula:
(Lu1-x,Cex)3(Al1-y,Mny)5-wSiwO12
wherein x is greater than 0 and less than about 0.2; and
y is greater than 0 and less than 0.1; and
w is greater than 0 and less than 0.455.