# US 2016/0355720 A1 · Thermal storage material containing hexanary composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0355720 A1
- Document ID: US20160355720A1
- Status: Published application
- Kind: A1
- Application number: 15/037,611
- Filed: 2014-11-12
- Published: 2016-12-08
- Earliest claimed: 2013-11-19
- Assignees: Korea Institute of Energy Research
- Applicants: Korea Institute of Energy Research
- Inventors: Hong-Soo Kim; Si-Kyoung Kim; Kang Bai; Jong-Kyu Kim; Yong-Heack Kang
- Web page: https://patentgrep.com/patent/US20160355720A1

## CPC

- C09K 5/12: Molten materials, i.e. materials solid at room temperature, e.g. metals or salts
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

The present disclosure relates to a thermal storage material containing a hexanary composition of NaNO3—NaNO2—KNO3—KNO2—Ca(NO3)2—LiNO3 for lowering a melting point of molten salts.

## Claims

### Claim 1

A thermal storage material comprising NaNO3—NaNO2—KNO3—KNO2—Ca(NO3)2—LiNO3.

### Claim 2 (depends on 1)

The thermal storage material of claim 1, wherein the Ca(NO3)2 is from 0.05 mol % to 0.1 mol %.

### Claim 3 (depends on 1)

The thermal storage material of claim 1, wherein the NaNO3 is from 0.1 mol % to 0.2 mol %, the Ca(NO3)2 is from 0.05 mol % to 0.4 mol % and the LiNO3 is from 0.05 mol % to 0.5 mol %.

### Claim 4 (depends on 1)

The thermal storage material of claim 1, wherein the NaNO2 is from 0.1 mol % to 0.2 mol %, the Ca(NO3)2 is from 0.05 mol % to 0.4 mol % and the LiNO3 is from 0.05 mol % to 0.5 mol %.

### Claim 5 (depends on 1)

The thermal storage material of claim 1, wherein the KNO3 is from 0.1 mol % to 0.2 mol %, the Ca(NO3)2 is from 0.05 mol % to 0.4 mol % and the LiNO3 is from 0.05 mol % to 0.5 mol %.

### Claim 6 (depends on 1)

The thermal storage material of claim 1, wherein the KNO2 is from 0.1 mol % to 0.2 mol %, the Ca(NO3)2 is from 0.05 mol % to 0.4 mol % and the LiNO3 is from 0.05 mol % to 0.5 mol %.

### Claim 7 (depends on 1)

The thermal storage material of claim 1, wherein a molar ratio of the NaNO3:NaNO2:KNO3:KNO2:Ca(NO3)2:LiNO3 is 1:1:1:1:0.2 to 0.5:0.8 to 2.2.

### Claim 8 (depends on 1)

The thermal storage material of claim 1, wherein a sum of the Ca(NO3)2 and the LiNO3 is from 1.3 mol to 2.7 mol with respect to 1 mol of the NaNO3.

### Claim 9 (depends on 1)

A solar heat storage system provided with the thermal storage material of claim 1.