- Number: US 2016/0355680 A1
- Document ID: US20160355680A1
- Status: Published application
- Kind: A1
- Application number: 15/239,975
- Filed: 2016-08-18
- Published: 2016-12-08
- Earliest claimed: 2014-12-01
- Assignees: Taiwan Textile Research Institute
- Applicants: Taiwan Textile Research Institute
- Inventors: Lung-Chang Hung; Sheng-Shan Chang; Nai-Yun Liang; Chun-Hung Lin
- Web page: https://patentgrep.com/patent/US20160355680A1

## CPC

- C08L 79/08: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- C08G 73/1046: {Polyimides containing oxygen in the form of ether bonds in the main chain}
- C08J 3/12: Powdering or granulating
- G02B 1/04: made of organic materials, e.g. plastics (G02B1/08 takes precedence)
- G02B 6/3865: {fabricated by using moulding techniques (shaping techniques of plastic materials in general B29C; producing plastic optical fiber connectors B29D11/0075)}
- C08J 2379/08: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- C08J 2467/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08J2467/06 takes precedence)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

A method for preparing a polyetherimide/polyester blend chip includes providing a composition. The composition includes a polyetherimide powder and a polyester powder. The polyetherimide powder has a variable diameter in a range of 10 μm to 600 μm. The polyester powder has a variable diameter in a range of 10 μm to 600 μm and a limiting viscosity in a range of 0.85 dl/g to 1.10 dl/g. Then, performing a powder dispersion treatment on the composition. The composition undergoes melt compounding after performing the powder dispersion treatment. The composition is next pelletizing melt compounding.

## Claims

### Claim 1

A method for preparing a polyetherimide/polyester blend chip, comprising:
providing a composition for preparing a polyetherimide/polyester blend chip, the composition comprising:
a polyetherimide powder, wherein the polyetherimide powder has a variable diameter in a range of 10 μm to 600 μm; and
a polyester powder, wherein the polyester powder has a variable diameter in a range of 10 μm to 600 μm and a limiting viscosity in a range of 0.85 dl/g to 1.10 dl/g, the polyetherimide powder has an amount greater than 70 wt % and less than or equal to 90 wt % based on a total weight of the polyetherimide powder and the polyester powder, and the polyester powder has an amount greater than or equal to 10 wt % and less than 30 wt % based on the total weight of the polyetherimide powder and the polyester powder;
performing a powder dispersion treatment on the composition;
melt compounding the composition after performing the powder dispersion treatment; and
pelletizing the composition after melt compounding the composition.

### Claim 2 (depends on 1)

The method for preparing the polyetherimide/polyester blend chip of claim 1, wherein providing the composition comprises:
providing a polyetherimide chip and a polyester chip; and
grinding the polyetherimide chip and the polyester chip to obtain the polyetherimide powder and the polyester powder.

### Claim 3 (depends on 1)

The method for preparing the polyetherimide/polyester blend chip of claim 1, wherein the powder dispersion treatment has a rotational speed in a range of 30 rpm to 30,000 rpm.

### Claim 4 (depends on 1)

The method for preparing the polyetherimide/polyester blend chip of claim 1, wherein melt compounding the composition has a melt compounding temperature in a range of 250° C. to 320° C. and a rotational speed in a range of 30 rpm to 300 rpm.

### Claim 5 (depends on 1)

A polyetherimide/polyester blend chip prepared by the method of claim 1.

### Claim 6 (depends on 5)

The polyetherimide/polyester blend chip of claim 5, wherein the polyetherimide/polyester blend chip has a melt flow index (Ml) greater than 20 when a melting temperature is 320° C. and a load is 5 kg.

### Claim 7 (depends on 5)

An article made of the polyetherimide/polyester blend chip of claim 5.

### Claim 8 (depends on 7)

The article of claim 7, wherein the article has a transmittance greater than or equal to 80% when a wavelength is 850 nm and a thickness of the article is 1 mm.

### Claim 9 (depends on 7)

The article of claim 7, wherein the article is an optical connector element.