- Assignees: Mitsui Chemicals, Inc.
- Applicants: Mitsui Chemicals, Inc.
- Inventors: Koya YOSHIMOTO; Hidetake NAKANO; Tetsuya NAKAMURA
- Web page: https://patentgrep.com/patent/US20160355628A1

## CPC

- C08F 255/10: on to butene polymers
- C08F 255/02: on to polymers of olefins having two or three carbon atoms
- C08L 23/12: Polypropene
- C08L 51/06: grafted on to homopolymers or copolymers of aliphatic hydrocarbons containing only one carbon-to-carbon double bond
- C08L 77/00: Compositions of polyamides obtained by reactions forming a carboxylic amide link in the main chain (of polyhydrazides C08L79/06; of polyamideimides or polyamide acids C08L79/08); Compositions of derivatives of such polymers
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A graft-modified propylene.α-olefin copolymer (A) is obtained by graft-reacting a polar monomer onto a propylene.α-olefin copolymer (a) including 50 to 90 mol % of propylene-derived structural units (C3) and 10 to 50 mol % of C4-8 α-olefin-derived structural units (Cα) (wherein the total of the structural units C3 and Cα is 100 mol %), and satisfies the following requirements (i) to (iv) at the same time: (i) the amount of the polar monomer grafted is 0.4 to 1.5 wt %, (ii) the content of the polar monomer is not more than 1000 ppm, (iii) the content of a gel insoluble in xylene at 140° C. is not more than 2.5 wt %, and (iv) the content of a volatile hydrocarbon compound is not more than 10 ppm.

## Claims

### Claim 1

A graft-modified propylene.α-olefin copolymer (A) obtained by graft-reacting a polar monomer onto a propylene.α-olefin copolymer (a) comprising 50 to 90 mol % of propylene-derived structural units (C3) and 10 to 50 mol % of C4-8 α-olefin-derived structural units (Cα) (wherein the total of the structural units C3 and Cα is 100 mol %), the graft-modified propylene.α-olefin copolymer satisfying the following requirements (i) to (iv) at the same time:
(i) the amount of the polar monomer grafted is 0.4 to 1.5 wt %,
(ii) the content of the polar monomer is not more than 1000 ppm,
(iii) the content of a gel insoluble in xylene at 140° C. is not more than 2.5 wt %, and
(iv) the content of a volatile hydrocarbon compound is not more than 10 ppm.

### Claim 2 (depends on 1)

The graft-modified propylene.α-olefin copolymer (A) according to claim 1, which has an intrinsic viscosity measured at 135° C. in decalin of 0.5 to 1.0 (dl/g).

### Claim 3 (depends on 1)

The graft-modified propylene.α-olefin copolymer (A) according to claim 1, wherein the propylene.α-olefin copolymer (a) satisfies the following requirements (1) to (3):
(1) the intrinsic viscosity measured at 135° C. in decalin is 0.1 to 12 (dl/g),
(2) the molecular weight distribution (Mw/Mn) measured by gel permeation chromatography (GPC) relative to polystyrenes is not more than 3.0, and
(3) the parameter value B representing a randomness of a comonomer sequence distribution is 1.0 to 1.5.

### Claim 4 (depends on 1)

The graft-modified propylene.α-olefin copolymer (A) according to claim 1, wherein the C4-8 α-olefin is 1-butene.

### Claim 5 (depends on 4)

The graft-modified propylene.α-olefin copolymer (A) according to claim 4, wherein the propylene.α-olefin copolymer (a) further satisfies the requirements (4) and (5):
(4) the melting point Tm measured by differential scanning calorimetry (DSC) is 60 to 140° C., and the melting point Tm (T° C.) and the content of 1-butene-derived structural units (M mol %) satisfy −2.6M+130≦T≦−2.3M+155, and
(5) the degree of crystallinity (C %) measured by X-ray diffractometry and the content of 1-butene-derived structural units (M mol %) satisfy C≧−1.5M+75.

### Claim 6 (depends on 1)

The graft-modified propylene.α-olefin copolymer (A) according to claim 1, wherein the polar monomer is maleic acid or maleic anhydride.

### Claim 7 (depends on 1)

The graft-modified α-olefin copolymer (A) according to claim 1, which is produced by modifying the propylene.α-olefin copolymer (a) by melt-kneading, at a temperature of 120 to 220° C., a mixture including the propylene.α-olefin copolymer (a), 0.1 to 20 parts by weight of maleic anhydride (B) per 100 parts by weight of the copolymer (a), and 0.1 to 1.0 part by weight of an organic peroxide (C) per 100 parts by weight of the copolymer (a), the organic peroxide having a one-minute half-life decomposition temperature of 150 to 190° C.

### Claim 8

A method for producing a graft-modified propylene.α-olefin copolymer (A) comprising modifying a propylene.α-olefin copolymer (a) by melt-kneading, at a temperature of 120 to 220° C., a mixture including the propylene.α-olefin copolymer (a), 0.1 to 20 parts by weight of maleic anhydride (B) per 100 parts by weight of the copolymer (a), and 0.1 to 1.0 part by weight of an organic peroxide (C) per 100 parts by weight of the copolymer (a), the organic peroxide having a one-minute half-life decomposition temperature of 150 to 190° C.

### Claim 9 (depends on 1)

A resin composition comprising the graft-modified polypropylene.α-olefin copolymer (A) described in claim 1, and one or more resins selected from polyamide resins and polypropylene resins.