# US 2016/0355618 A1 · Silica Supports With High Aluminoxane Loading Capability

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0355618 A1
- Document ID: US20160355618A1
- Status: Published application
- Kind: A1
- Application number: 15/142,961
- Filed: 2016-04-29
- Published: 2016-12-08
- Earliest claimed: 2015-06-05
- Assignees: ExxonMobil Chemical Patents Inc.
- Applicants: ExxonMobil Chemical Patents Inc.
- Inventors: Lubin Luo; Anupriya Jain; Xuan Ye
- Web page: https://patentgrep.com/patent/US20160355618A1

## CPC

- C08F 110/06: Propene
- C08F 4/02: Carriers therefor
- C08F 4/65916: {supported on a carrier, e.g. silica, MgCl2, polymer}
- C08F 4/65912: {in combination with an organoaluminium compound}
- C08F 4/65927: {two cyclopentadienyl rings being mutually bridged}
- C08F 2410/06: Catalyst characterized by its size
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Olefin polymerization catalyst systems having high aluminoxane loading and methods for making and using them are disclosed herein.

## Claims

### Claim 1

An olefin polymerization catalyst system comprising a silica support, wherein the silica support comprises silica gel particles having:
a. an average surface area of from about 400 to 800 m2/g;
b. an average pore diameter of from about 60 to 200 Angstrom; and
c. at least 20% of the incremental pore volume comprised of pores having a pore diameter larger than about 100 Angstrom;
wherein the catalyst system further comprises an aluminoxane, and the aluminoxane loading on the support is greater than about 9.5 mmol Al/g silica.

### Claim 2 (depends on 1)

The catalyst system of claim 1, wherein said silica gel particles have an average surface area of from about 550 to 650 m2/g.

### Claim 3 (depends on 1)

The catalyst system of claim 1, wherein said silica gel particles have an average pore diameter of from about 80 to 130 Angstrom.

### Claim 4 (depends on 1)

The catalyst system of claim 1, wherein said silica gel particles have an average pore volume of from about 0.5 to 2.5 ml/g of silica.

### Claim 5 (depends on 1)

The catalyst system of claim 1, wherein said silica gel particles have an average particle size of from about 20 to 200 micrometers.

### Claim 6 (depends on 1)

The catalyst system of claim 1, wherein at least 50% of the incremental pore volume is comprised of pores having a pore diameter larger than about 100 Angstrom.

### Claim 7 (depends on 1)

The catalyst system of claim 1, wherein said aluminoxane is methylaluminoxane.

### Claim 8 (depends on 1)

The catalyst system of claim 1, wherein said aluminoxane loading on the support is greater than about 12 mmol Al/g silica.

### Claim 9 (depends on 1)

The catalyst system of claim 1, further comprising a single site catalyst component.

### Claim 10 (depends on 1)

The catalyst system of claim 1, further comprising a metallocene catalyst component.

### Claim 11 (depends on 1)

The catalyst system of claim 1, wherein a raw silica surface area and a supported aluminoxane surface area differ by about or less than 10%.

### Claim 12 (depends on 1)

The catalyst system of claim 1, wherein a raw silica particle size and a supported aluminoxane particle size differ by about or less than 10% on a volumetric basis.

### Claim 13 (depends on 1)

The catalyst system of claim 1, wherein the silica particles do not comprise agglomerates.

### Claim 14

A method for making an olefin polymerization catalyst system comprising contacting:
d. a silica support, wherein the silica support comprises silica gel particles having:
i. an average surface area of from about 400 to 800 m2/g;
ii. an average pore diameter of from about 60 to 200 Angstrom; and
iii. at least 20% of the incremental pore volume is comprised of pores having a pore diameter larger than about 100 Angstrom;
e. an aluminoxane; and
f. an olefin catalyst component,
wherein the catalyst system has an aluminoxane loading on the support of greater than about 9.5 mmol Al/g silica.

### Claim 15 (depends on 14)

The method of claim 14, wherein said silica gel particles have an average surface area of from about 500 to 700 m2/g.

### Claim 16 (depends on 14)

The method of claim 14, wherein said silica gel particles have an average pore volume of from about 0.5 to 2.5 ml/g of silica.

### Claim 17 (depends on 14)

The method of claim 14, wherein said silica gel particles have an average particle size of from about 20 to 200 micrometers.

### Claim 18 (depends on 14)

The method of claim 14, wherein at least 50% of the incremental pore volume is comprised of pores having a pore diameter larger than about 100 Angstrom.

### Claim 19 (depends on 14)

The method of claim 14, wherein said aluminoxane is methylaluminoxane.

### Claim 20 (depends on 14)

The method of claim 14, wherein said aluminoxane loading is greater than about 12 mmol Al/g silica.

### Claim 21 (depends on 14)

The method of claim 14, wherein said olefin catalyst component is a single site catalyst component.

### Claim 22 (depends on 14)

The method of claim 14, wherein said olefin catalyst component is a metallocene catalyst component.

### Claim 23 (depends on 14)

The method of claim 14, wherein a raw silica surface area and a supported aluminoxane surface area differ by about or less than 10%, and/or wherein a raw silica particle size and a supported aluminoxane particle size differ by about or less than 10% on a volumetric basis.

### Claim 24 (depends on 14)

The method of claim 14, wherein the silica particles do not comprise agglomerates.

### Claim 25 (depends on 1)

A method for polymerizing olefins using the catalyst system of claim 1.