# US 2016/0355441 A1 · Post-Batching CMA Dosing Into Concrete

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0355441 A1
- Document ID: US20160355441A1
- Status: Published application
- Kind: A1
- Application number: 15/170,199
- Filed: 2016-06-01
- Published: 2016-12-08
- Earliest claimed: 2015-06-04
- Assignees: Verifi LLC
- Applicants: Verifi LLC
- Inventors: Nathan A. Tregger; Mark F. Roberts; Kati Hazrati
- Web page: https://patentgrep.com/patent/US20160355441A1

## CPC

- C04B 40/0032: {Controlling the process of mixing, e.g. adding ingredients in a quantity depending on a measured or desired value (B28C7/00 takes precedence)}
- B28C 7/024: {by measuring properties of the mixture, e.g. moisture, electrical resistivity, density}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B28C: PREPARING CLAY; PRODUCING MIXTURES CONTAINING CLAY OR CEMENTITIOUS MATERIAL, e.g. PLASTER (preparing material for foundry moulds B22C5/00)

## Abstract

The present invention relates to mitigating the deleterious effect of clays, which are born or conveyed by sand aggregates, crushed rock, gravel, and other aggregates used in the manufacture of concrete, upon the dosage efficiency of cement dispersants or other admixtures which are added into concrete. Instead of introducing the entire cement mitigation agent (CMA) into the aggregate material at a quarry or upon batching in the mix plant in a singular, upfront dose, the present invention comprises combining at least 51% and up to 100%, and, most preferably, at least 75% and up to 100%, of the total dosage amount of the CMAs into a given concrete mix batch during the transit portion of the delivery between initial batching at the mix plant and the pour event at the job site.

## Claims

### Claim 1

A method for dosing concrete, comprising:
monitoring the slump, on an automated basis using a processor unit, of a concrete slurry while in a rotatable mixer drum during transit from a mix plant to a construction site to which the concrete slurry is being delivered, the concrete slurry comprising a cement binder, water, aggregate, and clay which, in the absence of a clay mitigation agent, absorbs chemical admixture, and which is present in the concrete slurry in an amount sufficient to diminish the dosage efficiency of a cement dispersant or other chemical admixture added into the concrete slurry;
wherein the automated slump monitoring processor unit
(i) measures loss of slump (dS) of the concrete slurry in the rotatable mixer drum over a period of time (t) during transit to obtain a measured dS/dt value,
(ii) compares the measured dS/dt value with a threshold dS/dt value stored in a memory location which is accessed by the processor unit, and
(iii) detects when the measured dS/dt value meets or exceeds the stored threshold dS/dt value; and
whereupon the processor unit, once the measured dS/dt value meets or exceeds the stored dS/dt threshold value, initiates administration of a controlled dosage of clay mitigation agent (CMA) into the concrete within the rotatable mixer drum during transit, the CMA administered being effective to decrease the dS/dt value as measured by the automated slump processor unit.

### Claim 2 (depends on 1)

The concrete dosing method of claim 1 wherein the slump monitoring processor unit repeating steps (i), (ii) and (iii) whereby clay mitigation agent is administered into the concrete on at least two staggered instances during transit.

### Claim 3 (depends on 2)

The concrete dosing method of claim 2 wherein the slump monitoring computer processor initiates administering clay mitigation agent (CMA) into the concrete, whereby at least 21% and up to 100% of the total volume of CMA dosed into the concrete slurry is dosed during transit rather than at the mix plant where the concrete was batched into the rotatable mixing drum.

### Claim 4 (depends on 2)

The concrete dosing method of claim 2 wherein the slump monitoring computer processor initiates administering clay mitigation agent (CMA) into the concrete, whereby at least 51% and up to 100% of the total volume of CMA dosed into the concrete slurry is dosed during transit rather than at the mix plant where the concrete was batched into the rotatable mixing drum.

### Claim 5 (depends on 2)

The concrete dosing method of claim 2 wherein the slump monitoring computer processor initiates administering clay mitigation agent (CMA) into the concrete, whereby at least 81% and up to 100% of the total volume of CMA dosed into the concrete slurry is dosed during transit rather than at the mix plant where the concrete was batched into the rotatable mixing drum.

### Claim 6 (depends on 1)

The concrete dosing method of claim 1 further comprising administering into the concrete during transit at least one other chemical admixture, in addition to CMA, on at least two different instances during transit.

### Claim 7 (depends on 6)

The concrete dosing method of claim 6 wherein the at least one other chemical admixture is a cement dispersant selected from a mid-range water reducer or high-range water reducer.

### Claim 8 (depends on 7)

The concrete dosing method of claim 7 wherein the cement dispersant is dosed simultaneously with CMA on at least two staggered instances during transit.

### Claim 9 (depends on 7)

The concrete dosing method of claim 7 wherein cement dispersant is dosed after CMA is dosed at least two staggered instances during transit.

### Claim 10 (depends on 1)

The concrete dosing method of claim 1 further comprising measuring temperature of the concrete slurry during transit and obtaining temperature data, and adjusting the stored threshold dS/dt value based on the obtained temperature data.

### Claim 11 (depends on 1)

The concrete dosing method of claim 1 wherein air content of the concrete slurry is monitored during transit and air content data is obtained, and adjustment of the stored threshold dS/dt value is based on the obtained air content data.

### Claim 12 (depends on 1)

The concrete dosing method of claim 1 wherein the rotatable mixer drum has an inner wall upon which are spirally-mounted at least two mixing blades for agitating the concrete slurry during rotation of the mixer drum.

### Claim 13 (depends on 2)

The concrete dosing method of claim 2 wherein, after each of the at least two post-batching doses of CMA into the concrete slurry, the automated slump monitoring processor unit initiates additions of a controlled amount of water or at least one chemical admixture other than a CMA into the concrete slurry.

### Claim 14 (depends on 13)

The concrete dosing method of claim 13 wherein the automated slump monitoring processor unit initiates separate additions of a controlled amount of at least one chemical admixture into the concrete slurry, the at least one chemical admixture being selected from the group consisting of cement dispersant, air entraining admixture, air detraining admixture, and a mixture thereof.

### Claim 15 (depends on 14)

The concrete dosing method of claim 14 further comprising storing into processor-accessible memory the transit history of the concrete slurry (i) before and after at least two additions of CMA into the concrete slurry; (ii) before and after at least two additions of at least one chemical admixture into the concrete slurry, and (iii) the transit histories of both (i) and (ii).

### Claim 16 (depends on 15)

The concrete dosing method of claim 15 further comprising graphically illustrating the transit histories of both (i) and (ii).

### Claim 17 (depends on 1)

The concrete dosing method of claim 1 wherein the CMA is selected from the group consisting of a quaternary amine, polyquaternary amine, polycondensate of dimethylamine and epichorohydrin, functionalized amine, carboxylate graft polymers, cationic copolymers, and mixtures and derivatives thereof.

### Claim 18 (depends on 1)

The concrete dosing method of claim 1 wherein a portion of the cumulative total amount of CMA added into a given concrete load contained in the mixer drum is added at the mix plant, the portion being added at the batch plant comprising no greater than 49 percent of the cumulative total amount of CMA.

### Claim 19 (depends on 1)

The concrete dosing method of claim 1 wherein the CMA has minimal or no water-reducing capability by itself in the absence of clay when administered alone into a fresh concrete (in accordance with standard specification for water reducers in ASTM C494-13).

### Claim 20 (depends on 1)

The concrete dosing method of claim 1, further comprising
adding a polycarboxylate high range water reducing (HRWR) admixture into the concrete slurry during transit;
monitoring for an increase in the slump of the concrete slurry (dS) over a period of time immediately following addition of the polycarboxylate high range water reducing admixture to obtain a dS value for the period after said addition of the HRWR; and
comparing the obtained dS value with a second threshold dS value stored in a memory location which is accessed by the processor unit;
detecting when the obtained dS value fails to meet or exceed the stored second threshold dS value stored in the memory location; and, upon detection that the second threshold dS value is not met,
adjusting the stored threshold dS/dt value described in (ii) of claim 1, adjusting the controlled dosage of clay mitigation agent (CMA) to be administered into the concrete slurry, or both.

### Claim 21

A dosing method, comprising: administering a clay mitigation agent (CMA) on at least two instances in a mixer, wherein at least 21%-100% of the total CMA added into the concrete is added after initial batching of water, cement binder, and clay-bearing aggregates to form the concrete slurry in the mixer.

### Claim 22 (depends on 1)

An automated slump monitoring system having a processor unit which is programmed to effectuate the method of claim 1.