# US 2016/0355003 A1 · Method of bonding cover plate and touch sensing film and touch screen

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0355003 A1
- Document ID: US20160355003A1
- Status: Published application
- Kind: A1
- Application number: 14/891,933
- Filed: 2015-05-12
- Published: 2016-12-08
- Earliest claimed: 2014-12-22
- Assignees: Boe Technology Group Co., Ltd.; Hefei Xinsheng Optoelectronics Technology Co., Ltd.
- Applicants: Boe Technology Group Co., Ltd.; Hefei Xinsheng Optoelectronics Technology Co., Ltd.
- Inventors: Hongqiang Luo; Ming Hu; Taofeng Xie; Zouming Zu; Wenjin Fan; Jun Xu
- Web page: https://patentgrep.com/patent/US20160355003A1

## CPC

- B32B 37/12: characterised by using adhesives
- B32B 37/06: characterised by the heating method
- G06F 3/041: Digitisers, e.g. for touch screens or touch pads, characterised by the transducing means
- B32B 37/10: characterised by the pressing technique, e.g. using action of vacuum or fluid pressure
- B32B 37/14: characterised by the properties of the layers
- B32B 38/18: Handling of layers or the laminate
- B32B 2309/02: Temperature
- B32B 2309/04: Time
- B32B 2309/12: Pressure
- B32B 2457/208: Touch screens
- G06F 2203/04103: Manufacturing, i.e. details related to manufacturing processes specially suited for touch sensitive devices
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- G06F: ELECTRIC DIGITAL DATA PROCESSING (computer systems based on specific computational models G06N)

## Abstract

Embodiments of the present disclosure provide a method of bonding a cover plate and a touch sensing film, and a touch screen manufactured by using the method. The method comprises steps of: bonding a cover plate and at least one touch sensing film together by an adhesive so as to form a touch module; deaerating the touch module; and laminating the deaerated touch module. The touch module is laminated after deaerating the touch module, thus water waves in the touch module may be removed, thereby increasing product yield.

## Claims

### Claim 1

A method of bonding a cover plate and a touch sensing film, comprising steps of:
bonding a cover plate and at least one touch sensing film together by an adhesive so as to form a touch module;
deaerating the touch module; and
laminating the deaerated touch module.

### Claim 2 (depends on 1)

The method according to claim 1, comprising deaerating the touch module in a closed deaerator.

### Claim 3 (depends on 1)

The method according to claim 1, comprising laminating the deaerated touch module by using two flat plates.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the step of laminating the deaerated touch module by using two flat plates comprises heating the touch module by at least one of the two flat plates while laminating.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the step of heating the touch module by at least one of the two flat plates while laminating further comprises:
heating at least one of the two flat plates to a predefined lamination temperature;
placing the touch module between the two flat plates; and
laminating the touch module with a predefined lamination pressure by the two flat plates for a lamination duration time.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the two flat plates are respectively provided therein with heating resistance wires for the heating.

### Claim 7 (depends on 5)

The method according to claim 5, wherein the predefined lamination pressure is kept in a range of 1000 kg˜1200 kg, the predefined lamination temperature of the flat plate contacting the cover plate is kept in a range of 70° C.˜80° C., the predefined lamination temperature of the flat plate contacting the touch sensing film is kept in a range of 70° C.˜80° C., and the lamination duration time is kept in a range of 10 s˜80 s.

### Claim 8 (depends on 5)

The method according to claim 5, wherein the predefined lamination temperature of the flat plate contacting the cover plate is kept higher than that of the flat plate contacting the touch sensing film.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the predefined lamination pressure is kept in a range of 1000 kg˜1200 kg, the predefined lamination temperature of the flat plate contacting the cover plate is kept in a range of 75° C.˜85° C., the predefined lamination temperature of the flat plate contacting the touch sensing film is kept in a range of 70° C.˜80° C., and the lamination duration time is kept in a range of 10 s˜80 s.

### Claim 10 (depends on 2)

The method according to claim 2, wherein the step of deaerating the touch module in a closed deaerator comprises:
placing the touch module in the deaerator; and
keeping a gas pressure inside the deaerator at a predefined deaeration pressure so as to apply a pressure to the touch module for a heating and pressing duration time.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the step of deaerating the touch module in a closed deaerator further comprises keeping a temperature inside the deaerator at a predefined deaeration temperature.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the predefined deaeration pressure is set so that the touch module bears a pressure of 5 kg˜6 kg; the predefined deaeration temperature is in a range 40° C.˜60° C.; and the heating and pressing duration time is in a range of 15 min˜45 min.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the step of bonding a cover plate and at least one touch sensing film together by an adhesive so as to form a touch module comprises:
plasma cleaning the cover plate;
covering the adhesive on the cover plate; and
attaching on the cover plate at least one layer of the touch sensing film which has been bonded.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the step of bonding a cover plate and at least one touch sensing film together by an adhesive so as to form a touch module comprises:
plasma cleaning the touch sensing film;
covering the adhesive on the touch sensing film; and
attaching the touch sensing film on the cover plate.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the step of bonding a cover plate and at least one touch sensing film together by an adhesive so as to form a touch module comprises:
plasma cleaning two or more touch sensing films;
covering the adhesive on the two or more touch sensing films, and bonding the two or more touch sensing films together; and
attaching the bonded two or more touch sensing films on the cover plate.

### Claim 16 (depends on 1)

The method according to claim 1, wherein ultraviolet light is used to irradiate the touch module so that the adhesive is cured after the step of laminating the deaerated touch module.

### Claim 17 (depends on 1)

The method according to claim 1, wherein the adhesive is a transparent adhesive.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the transparent adhesive comprises optical clear resin and/or optical clear adhesive.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the transparent adhesive comprises any one or any combination of organic silicon rubber, acrylic resin, unsaturated polyester, polyurethane and epoxy resin.

### Claim 20 (depends on 1)

A touch screen, manufactured by using the method according to claim 1.