# US 2016/0354996 A1 · Bent, veneer-encapsulated heat-treated safety glass panels and methods of manufacture

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0354996 A1
- Document ID: US20160354996A1
- Status: Published application
- Kind: A1
- Application number: 15/169,797
- Filed: 2016-06-01
- Published: 2016-12-08
- Earliest claimed: 2015-06-03
- Assignees: Precision Glass Bending Corporation
- Applicants: Precision Glass Bending Corporation
- Inventors: Russell Ashley Alder; Richard Ashley Alder
- Web page: https://patentgrep.com/patent/US20160354996A1

## CPC

- B32B 17/10293: {Edge features, e.g. inserts or holes}
- B32B 1/00: Layered products having a non-planar shape
- B32B 17/10036: {comprising two outer glass sheets}
- B32B 17/10091: {thermally hardened}
- B32B 17/10119: {having a composition deviating from the basic composition of soda-lime glass, e.g. borosilicate}
- B32B 17/10137: {Chemical strengthening}
- B32B 17/10155: {Edge treatment or chamfering}
- B32B 17/10174: {Coatings of a metallic or dielectric material on a constituent layer of glass or polymer}
- B32B 17/10302: {Edge sealing}
- B32B 17/10743: {containing acrylate (co)polymers or salts thereof}
- B32B 17/10761: {containing vinyl acetal}
- B32B 17/10853: {the membrane being bag-shaped}
- B32B 17/10889: {shaping the sheets, e.g. by using a mould (B32B17/10816 takes precedence)}
- B32B 17/10935: {as a preformed layer, e.g. formed by extrusion}
- B32B 17/1099: {After-treatment of the layered product, e.g. cooling}
- C03B 23/0252: {by gravity only, e.g. sagging (C03B23/035 takes precedence)}
- C03B 33/082: {using a focussed radiation beam, e.g. laser (C03B33/0855 takes precedence)}
- C03C 3/085: containing an oxide of a divalent metal
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 3/091: containing aluminium
- C03C 3/093: containing zinc or zirconium
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 27/10: with the aid of adhesive specially adapted for that purpose
- E06B 1/006: {of curvilinear outline}
- B32B 2419/00: Buildings or parts thereof
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- E06B: FIXED OR MOVABLE CLOSURES FOR OPENINGS IN BUILDINGS, VEHICLES, FENCES OR LIKE ENCLOSURES IN GENERAL, e.g. DOORS, WINDOWS, BLINDS, GATES (shades or blinds for greenhouses A01G9/22; curtains A47H; lids for car boots or bonnets B62D25/10; skylights E04B7/18; sunshades, awnings E04F10/00)

## Abstract

A laminated, bent, safety glass panel (30) for architectural or interior uses and a method of manufacturing such panels. The panel comprises a single heat-treated bent glass sheet, fully-tempered or heat-strengthened, forming a substrate (32) encapsulated by at least one thin, chemically-strengthened, glass veneer sheet (38). The veneer sheet (38), an alkali-aluminosilicate or other alkali-containing glass recipe strengthened by ion-exchange treatment, is cold-bent over a polymer interlayer (40) and permanently laminated to form a protective barrier on the heat-treated glass that dampens the explosive release of its internal residual stresses in the event of breakage thereby preventing particles dislodging and subsequent disintegration. The vulnerable perimeter (37) and perforation (45) edges of the veneer sheet (38) are equal in size or inset to the edges of the heat-treated substrate (32) with its deeper robust compressive stresses. Veneers may be laminated to both major substrate surfaces.

## Claims

### Claim 1

A bent, laminated, high strength glass panel suitable for use as an enhanced safety glazing material in architectural and interior applications, said panel comprising:
a single heat-treated bent glass sheet forming a substrate having opposed, major exterior convex and concave surfaces; the bent glass substrate having a thickness of between 3.2 mm. and 19.9 mm.; the bent glass substrate characterized as having a surface compressive stress of at least 24 MPa.;
a chemically-strengthened glass veneer sheet, the glass veneer sheet having a thickness of between 0.28 mm. and 3.0 mm. and being substantially thinner than said bent glass substrate;
a polymer interlayer disposed between the bent glass substrate and the glass veneer sheet;
said glass veneer sheet being laminated by means of the polymer interlayer to at least one of said convex or concave surfaces of the bent glass substrate;
wherein the glass veneer sheet is cold-bent to conform to the shape of the bent glass substrate;
wherein the polymer interlayer provides a permanent bond between the cold-bent glass veneer sheet and the thicker bent glass substrate; and,
wherein the residual stress within the heat-treated bent glass substrate is safely encapsulated on a major surface by the polymer interlayer and glass veneer sheet.

### Claim 2 (depends on 1)

The glass panel as defined in claim 1 wherein the bent glass substrate is fully-tempered glass and characterized as having a surface compressive stress of at least 69 MPa.

### Claim 3 (depends on 1)

The glass panel as defined in claim 1 wherein the bent glass substrate is heat-strengthened glass and characterized as having a surface compressive stress of between 24 MPa. and 52 MPa.

### Claim 4 (depends on 1)

The glass panel as defined in claim 1 wherein the bent glass substrate has a thickness of between 5.5 mm. and 19.9 mm.

### Claim 5 (depends on 1)

The glass panel as defined in claim 1 wherein the glass veneer sheet has a thickness of between 0.4 mm. and 1.1 mm.

### Claim 6 (depends on 1)

The glass panel as defined in claim 1 wherein a glass veneer sheet is applied to both of said convex and concave surfaces of said bent glass substrate.7. The glass panel as defined in claim 1 wherein the chemically-strengthened glass veneer sheet is made from material selected from the group consisting of alkali-containing glass including alkali-aluminosilicate, soda-lime silicate glass, alkali-borosilicate glass, alkali-aluminoborosilicate glass, alkali-boron glass, alkali-germinate glass, and alkali-borogermanate glass.

### Claim 8 (depends on 7)

The glass panel as defined in claim 7 wherein the polymer interlayer is made from material selected from the group consisting of PVB polyvinyl butryal, ionoplast, EVA ethyl vinyl acetate, TPU Thermoplastic polyurethane, polycarbonate, urethane, CIP cast-in-place curable resins, and other plastic materials and combinations thereof suitable for permanent lamination.

### Claim 9 (depends on 8)

The glass panel as defined in claim 8 wherein the dimensional characteristics of the glass veneer sheet are optimized to flushly mate with the major surface of the bent glass substrate to which it is laminated;
wherein perimeter edges of said glass veneer sheet are flush with or smaller than the perimeter edges of the bent glass substrate; and
wherein perforations such as holes or notches in said glass veneer sheet are flush with or larger than perforations in the bent glass substrate.

### Claim 10

A bent, laminated, high strength glass panel suitable for use as an enhanced safety glazing material in architectural and interior applications, said panel comprising:
a single fully-tempered bent glass sheet forming a substrate having opposed, major exterior convex and concave surfaces; the bent glass substrate characterized as having a surface compressive stress of at least 69 MPa.; the bent glass substrate having a thickness of between 3.2 mm. and 19.9 mm.;
a chemically-strengthened glass veneer sheet, the glass veneer sheet having a thickness of between 0.28 mm. and 3.0 mm. and being substantially thinner than said bent glass substrate;
the glass veneer sheet characterized as having a surface compressive stress of at least 350 MPa.;
a polymer interlayer disposed between the bent glass substrate and the glass veneer sheet;
said glass veneer sheet being laminated by means of the polymer interlayer to at least one of said convex or concave surfaces of the bent glass substrate;
wherein the glass veneer sheet is cold-bent to conform to the shape of the bent glass substrate;
wherein the polymer interlayer provides a permanent bond between the cold-bent glass veneer sheet and the thicker bent glass substrate; and,
wherein the residual stress within the fully-tempered bent glass substrate is safely encapsulated on a major surface by the polymer interlayer and glass veneer sheet.

### Claim 11 (depends on 10)

The glass panel as defined in claim 10 wherein the bent glass substrate has a thickness of between 5.5 mm. and 19.9 mm.

### Claim 12 (depends on 10)

The glass panel as defined in claim 10 wherein the glass veneer sheet has a thickness of between 0.4 mm. and 1.1 mm.

### Claim 13 (depends on 10)

The glass panel as defined in claim 10 wherein a glass veneer sheet is applied to both of said convex and concave surfaces of said bent glass substrate.

### Claim 14 (depends on 10)

The glass panel as defined in claim 10 wherein the polymer interlayer is made from material selected from the group consisting of PVB polyvinyl butryal, ionoplast, EVA ethyl vinyl acetate, TPU Thermoplastic polyurethane, polycarbonate, urethane, CIP cast-in-place curable resins, and other plastic materials and combinations thereof suitable for permanent lamination.

### Claim 15 (depends on 14)

The glass panel as defined in claim 14 wherein the chemically-strengthened glass veneer sheet is made from material selected from the group consisting of alkali-containing glass including alkali-aluminosilicate, soda-lime silicate glass, alkali-borosilicate glass, alkali-aluminoborosilicate glass, alkali-boron glass, alkali-germinate glass, and alkali-borogermanate glass.

### Claim 16 (depends on 15)

The glass panel as defined in claim 15 wherein the dimensional characteristics of the glass veneer sheet are optimized to flushly mate with the major surface of the bent glass substrate to which it is laminated,
wherein perimeter edges of said glass veneer sheet are flush with or smaller than the perimeter edges of the bent glass substrate; and
wherein perforations such as holes or notches in said glass veneer sheet are flush with or larger than perforations in the bent glass substrate.

### Claim 17

A method of manufacturing a high strength glass panel suitable for use as an enhanced safety glazing material in architectural and interior applications, the method comprising the steps of:
a) fabricating a single thick, bent, fully-tempered or heat strengthened glass sheet to be used as a bent glass substrate; the bent glass substrate having a thickness of between 3.2 mm. and 19.9 mm.; the bent glass substrate characterized as having a surface compressive stress of at least 24 MPa.;
b) defining the dimensional characteristics for one or more glass veneer sheets;
c) fabricating at least one thin, strong chemically-strengthened glass veneer sheet with a thickness of between 0.28 mm. and 3.0 mm. to the dimensional characteristics defined in step (b), the glass veneer sheet made from materials selected from group consisting of alkali-containing glass including alkali-aluminosilicate, soda-lime silicate glass, alkali-borosilicate glass, alkali-aluminoborosilicate glass, alkali-boron glass, alkali-germinate glass, and alkali-borogermanate glass;
d) assembling at least one thin glass veneer sheet onto the bent glass substrate, with a polymer interlayer placed therebetween, and cold-bending the glass veneer sheet so it mechanically conforms to the shape of the major surface of the bent glass substrate onto which it is assembled;
e) laminating to permanently bond the one or more glass veneer sheets in their cold-bent orientation by polymer interlayer to the bent glass substrate; and,
f) finishing by trimming excess polymer interlayer.

### Claim 18 (depends on 17)

The method as defined in claim 17 where said polymer interlayer is made from material selected from the group consisting of PVB polyvinyl butryal, ionoplast, EVA ethyl vinyl acetate, TPU Thermoplastic polyurethane, polycarbonate, urethane, CIP cast-in-place curable resins, and other plastic materials and combinations thereof suitable for permanent lamination.

### Claim 19 (depends on 18)

The method as defined in claim 18 where said step of defining the dimensional characteristics for one or more glass veneer sheets includes creating a virtual, dimensioned representation of the glass assembly in Computer-aided Design software in which dimensional characteristics for one or more glass veneer sheets are developed and optimized so as to flushly mate after lamination with the major surface of the bent glass substrate,
wherein perimeter edges of said glass veneer sheet are flush with or smaller than the perimeter edges of the bent glass substrate; and
wherein perforations such as holes or notches in said glass veneer sheet are flush with or larger than perforations in the bent glass substrate.

### Claim 20 (depends on 19)

The method as defined in claim 19 where said step of defining the dimensional characteristics for one or more glass veneer sheets includes the scanning the thick bent glass substrate with an optical, non-contact scanner to generate many thousands of dimensional points, a “point cloud”, representing its dimensional properties.

### Claim 21 (depends on 17)

The method as defined in claim 17 where said step of glass veneer sheet fabricating is conducted in various sequences comprised from among the following steps:
cutting;
adding perforations such as holes or notches;
optionally hot bending in a furnace to thermally pre-form to a shape approximately matching that of the bent glass substrate;
strengthening by ion-exchange.

### Claim 22 (depends on 21)

The method as defined in claim 21 wherein said steps of cutting or adding perforations such as holes or notches in the glass veneer sheets is by means of an ultra short pulse laser.

### Claim 23 (depends on 17)

The method as defined in claim 17 wherein the said step of finishing includes trimming excess polymer interlayer in planes extending from the edge finish of the thick bent glass substrate to impart the appearance of a solid edge.

### Claim 24 (depends on 23)

The method as defined in claim 23 where said final step of trimming polymer interlayer includes cutting or adding perforations such as holes or notches or abrasive grinding to one or more thin glass veneer sheets after lamination but with a reduction in strength of the glass veneer sheet to a level less than otherwise achievable were no dimensional changes made after strengthening by ion-exchange.
wherein perimeter edges of said glass veneer sheet are flush with or smaller than the perimeter edges of the bent glass substrate; and
wherein perforations such as holes or notches in said glass veneer sheet are flush with or larger than perforations in the bent glass substrate.

### Claim 25 (depends on 24)

The method as defined in claim 24 wherein said steps of cutting or adding perforations such as holes or notches in the glass veneer sheets is by means of an ultra short pulse laser.