# US 2016/0354871 A1 · Flux and method for manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0354871 A1
- Document ID: US20160354871A1
- Status: Published application
- Kind: A1
- Application number: 15/097,516
- Filed: 2016-04-13
- Published: 2016-12-08
- Earliest claimed: 2015-06-03
- Assignees: Fujitsu Limited
- Applicants: Fujitsu Limited
- Inventors: KOZO SHIMIZU; Seiki Sakuyama; Nobuhiro Imaizumi
- Web page: https://patentgrep.com/patent/US20160354871A1

## CPC

- B23K 35/3613: {Polymers, e.g. resins}
- B23K 35/0222: {for use in soldering or brazing (B23K35/0205 takes precedence)}
- B23K 35/3006: {Ag as the principal constituent}
- B23K 35/36: Selection of non-metallic compositions, e.g. coatings or fluxes (B23K35/34 takes precedence); Selection of soldering or welding materials, conjoint with selection of non-metallic compositions, both selections being of interest
- B23K 35/3612: {with organic compounds as principal constituents}
- B23K 35/362: Selection of compositions of fluxes (B23K35/365, B23K35/368 take precedence)
- B23K 35/262: {Sn as the principal constituent}
- B23K 2101/40: Semiconductor devices
- H10W 72/01271: {Cleaning, e.g. oxide removal or de-smearing}
- H10W 72/072: {of bump connectors}
- H10W 72/07211: {Treating the bond pad before connecting, e.g. by applying flux or cleaning}
- H10W 72/07232: {Compression bonding, e.g. thermocompression bonding}
- H10W 72/07234: {Using a reflow oven}
- H10W 72/07236: {Soldering or alloying}
- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/241: {Dispositions, e.g. layouts}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A flux includes: a first glycol-based polyhydric alcohol having a molecular weight of 300 or less; and a second glycol-based polyhydric alcohol having a molecular weight of 600 or more.

## Claims

### Claim 1

A flux comprising:
a first glycol-based polyhydric alcohol having a molecular weight of 300 or less; and
a second glycol-based polyhydric alcohol having a molecular weight of 600 or more.

### Claim 2 (depends on 1)

The flux according to claim 1,
wherein the first glycol-based polyhydric alcohol is a polyethylene glycol having a molecular weight of 200 or more, and
the second glycol-based polyhydric alcohol is a polyethylene glycol having a molecular weight of 1,000 or less.

### Claim 3 (depends on 1)

The flux according to claim 1,
wherein the first glycol-based polyhydric alcohol is a tetraethylene glycol, and
the second glycol-based polyhydric alcohol is the polyethylene glycol having a molecular weight of 1,000 or less.

### Claim 4 (depends on 1)

The flux according to claim 1,
wherein more of the first glycol-based polyhydric alcohols than the second glycol-based polyhydric alcohols is contained in the flux.

### Claim 5 (depends on 1)

The flux according to claim 1,
wherein the content of the first glycol-based polyhydric alcohol and the second glycol-based polyhydric alcohol in the flux is 80% or more.

### Claim 6 (depends on 1)

The flux according to claim 1,
wherein the flux contains an organic acid or an organic acid anhydride.

### Claim 7 (depends on 1)

The flux according to claim 1,
wherein a volatilization temperature of the first glycol-based polyhydric alcohol is lower than a reflow temperature of a SnAg based solder, and
a volatilization temperature of the second glycol-based polyhydric alcohol is higher than the reflow temperature of the SnAg based solder.

### Claim 8

A method for manufacturing a semiconductor device, comprising:
preparing a semiconductor chip or a semiconductor package and a circuit board; and
bonding the semiconductor chip or the semiconductor package with the circuit board by reflowing an SnAg based solder using a flux which contains a first glycol-based polyhydric alcohol having a molecular weight of 300 or less and a second glycol-based polyhydric alcohol having a molecular weight of 600 or more.

### Claim 9 (depends on 8)

The method according to claim 8,
wherein gaps between a plurality of terminals in a bonding portion of the semiconductor chip or the semiconductor package with the circuit board are 100 μm or less.

### Claim 10 (depends on 8)

The method according to claim 8,
wherein the first glycol-based polyhydric alcohol is a polyethylene glycol having a molecular weight of 200 or more, and
the second glycol-based polyhydric alcohol is a polyethylene glycol having a molecular weight of 1,000 or less.

### Claim 11 (depends on 8)

The method according to claim 8,
wherein the first glycol-based polyhydric alcohol is a tetraethylene glycol, and
the second glycol-based polyhydric alcohol is the polyethylene glycol having a molecular weight of 1,000 or less.

### Claim 12 (depends on 8)

The method according to claim 8,
wherein more of the first glycol-based polyhydric alcohols than the second glycol-based polyhydric alcohols is contained in the flux.

### Claim 13 (depends on 8)

The method according to claim 8,
wherein the content of the first glycol-based polyhydric alcohol and the second glycol-based polyhydric alcohol in the flux is 80% or more.

### Claim 14 (depends on 8)

The method according to claim 8,
wherein the flux contains an organic acid or an organic acid anhydride.

### Claim 15 (depends on 8)

The method according to claim 8,
wherein a volatilization temperature of the first glycol-based polyhydric alcohol is lower than a reflow temperature of a SnAg based solder, and
a volatilization temperature of the second glycol-based polyhydric alcohol is higher than the reflow temperature of the SnAg based solder.