# US 2016/0354838 A1 · High-purity tantalum powder and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0354838 A1
- Document ID: US20160354838A1
- Status: Published application
- Kind: A1
- Application number: 15/111,632
- Filed: 2014-02-27
- Published: 2016-12-08
- Earliest claimed: 2014-02-27
- Assignees: Ningxia Orient Tantalum Industry Co., Ltd.
- Applicants: Ningxia Orient Tantalum Industry Co., Ltd.
- Inventors: Zhongxiang LI; YUEWEI CHENG; Xueqing CHEN; Ting WANG; Dejun SHI; Zekun TONG; Yan YAN; Xiaoyu TIAN; Zhonghuan ZHAO
- Web page: https://patentgrep.com/patent/US20160354838A1

## CPC

- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- B22F 1/00: Metallic powder; Treatment of metallic powder, e.g. to facilitate working or to improve properties
- B22F 9/023: {Hydrogen absorption}
- B22F 9/16: using chemical processes
- C22F 1/18: High-melting or refractory metals or alloys based thereon
- C23G 1/00: Cleaning or pickling metallic material with solutions or molten salts (with organic solvents C23G5/02)
- B22F 2009/043: {by ball milling}
- B22F 2301/20: Refractory metals
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C23G: CLEANING OR DE-GREASING OF METALLIC MATERIAL BY CHEMICAL METHODS OTHER THAN ELECTROLYSIS

## Abstract

The present invention relates to a high-purity tantalum powder and a preparation method therefore. The tantalum powder has a purity of more than 99.995%, as analyzed by GDMS. Preferably, the tantalum powder has an oxygen content of not more than 1000 ppm, a nitrogen content of not more than 50 ppm, a hydrogen content of not more than 20 ppm, a magnesium content of not more than 5 ppm, and an average particle diameter D50 of less than 25 μm.

## Claims

### Claim 1

A high purity tantalum powder having a purity of greater than 99.995%, as analyzed by Glow Discharge Mass Spectometry (GDMS):
the tantalum powder having an oxygen content of not more than 1000 ppm, and a magnesium content of not more than 5 ppm, and
the tantalum powder having a particle diameter D50<25 μm.

### Claim 2 (depends on 1)

The high purity tantalum powder of claim 1, wherein the tantalum powder has:
a nitrogen content of not more than 50 ppm, preferably not more than 40 ppm, and
a hydrogen content of not more than 20 ppm, preferably not more than more than 10 ppm.

### Claim 3 (depends on 1)

The high purity tantalum powder of claim 1, wherein the tantalum powder has a particle diameter D50 <20 μm.

### Claim 4 (depends on 1)

A method for preparing a high purity tantalum powder of claim 1, comprising the following steps:
1) subjecting a high purity tantalum ingot to a hydrogenation treatment;
2) crushing the tantalum scraps as prepared after the hydrogenation of the tantalum ingot to tantalum powder, and then purifying the powder by pickling to remove impurity contaminations introduced during ball milling;
3) subjecting the tantalum powder obtained in step 2) to a high-temperature dehydrogenation treatment;
4) subjecting the tantalum powder obtained in step 3) to a deoxygenation treatment;
5) subjecting the tantalum powder obtained in step 4) to pickling, washing, baking to dry, and sieving; and
6) subjecting the tantalum powder obtained in step 5) to a low-temperature heat treatment, and then subjecting the treated tantalum powder to cooling, passivating, discharging, and sieving to achieve the high purity tantalum powder finished product.

### Claim 5 (depends on 4)

The method of claim 4, wherein the high purity tantalum ingot refers to tantalum ingot having a tantalum content of more than 99.995%.

### Claim 6 (depends on 4)

The method of claim 4, wherein the high-temperature dehydrogenation of step 3) is carried out as follows:
tantalum powder is heated at about 800-1000° C. and the temperature is maintained for about 60-300 minutes; and
the tantalum powder is then subjected to cooling, discharging, and sieving operations to achieve the dehydrogenated tantalum powder.

### Claim 7 (depends on 4)

The method according to claim 4, wherein the deoxygenation temperature is lower than the dehydrogenation temperature, preferably by about 50-300° C.

### Claim 8 (depends on 4)

The method of claim 4, wherein said low-temperature heat treatment is performed by keeping the temperature of about 600-1200° C. for about 15-90 minutes, and preferably at a vacuum level of 10−3 Pa or higher.

### Claim 9 (depends on 4)

The method of claim 4, wherein the tantalum scraps is crushed in step 2) to a level that the resultant powder can pass through 400-700-mesh sieves.

### Claim 10 (depends on 1)

A method of using the high purity tantalum powder of claim 1 in semiconductor, medical and/or surface spray coating applications.