# US 2016/0354816 A1 · Method for Producing Aluminum Rod and Aluminum Wire

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0354816 A1
- Document ID: US20160354816A1
- Status: Published application
- Kind: A1
- Application number: 15/242,651
- Filed: 2016-08-22
- Published: 2016-12-08
- Earliest claimed: 2011-02-07
- Assignees: Southwire Company
- Applicants: Southwire Company, LLC
- Inventors: Jeffrey D. Herrin; Thomas Noell Wilson; Clinton E. Watkins; Emory Barber; Tom Stephens
- Web page: https://patentgrep.com/patent/US20160354816A1

## CPC

- B21B 1/16: for rolling {wire rods, bars, merchant bars, rounds} wire or material of like small cross-section
- B21C 1/00: Manufacture of metal sheets, wire, rods, tubes or like semi-manufactured products by drawing
- B21C 1/003: {Drawing materials of special alloys so far as the composition of the alloy requires or permits special drawing methods or sequences}
- C22F 1/04: of aluminium or alloys based thereon
- B21B 2003/001: {Aluminium or its alloys}
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- B21C: MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES, PROFILES OR LIKE SEMI-MANUFACTURED PRODUCTS OTHERWISE THAN BY ROLLING; AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

Systems, methods, and devices for the production of aluminum rods from aluminum bars, aluminum wires from aluminum rods, and aluminum wires from aluminum bars are disclosed and described. Annealing steps are not needed or required in the disclosed methods.

## Claims

### Claim at position 1

1-19. (canceled)

### Claim 20

A method for producing an aluminum wire from an aluminum rod, the method comprising:
cold-drawing the aluminum rod at a temperature in a range from about 40° F. to about 250° F. to reduce the cross-sectional area, producing the aluminum wire;
wherein the aluminum rod is a cylindrical rod having a diameter in a range from about 0.2″ to 0.35″,
the ratio of the cross-sectional area of the aluminum rod to the aluminum wire is in a range from about 3:1 to about 10:1,
the aluminum wire has a tensile strength in a range from about 17,000 to about 22,000 psi, and
the aluminum wire is not annealed.

### Claim 21 (depends on 20)

The method of claim 20, wherein:
the aluminum rod has a tensile strength from about 8,000 to about 12,000 psi; and
the aluminum wire and the aluminum rod comprise an aluminum 1350 alloy.

### Claim 22 (depends on 20)

The method of claim 20, wherein:
the aluminum rod has a tensile strength of less than about 12,000 psi; and
the aluminum wire and the aluminum rod comprise at least 99% aluminum by weight.

### Claim 23 (depends on 20)

The method of claim 20, wherein:
the aluminum rod is a cylindrical rod having a diameter in a range from about ¼″ to about 11/32″; and
the ratio is in a range from about 4:1 to about 9:1.

### Claim 24 (depends on 23)

The method of claim 23, wherein the aluminum wire and the aluminum rod comprise an aluminum 1350 alloy.

### Claim 25 (depends on 23)

The method of claim 23, wherein:
the aluminum wire has an IACS electrical conductivity from about 61% to about 63%; and
the aluminum wire has a tensile strength in a range from about 17,000 to about 21,750 psi.

### Claim 26 (depends on 23)

The method of claim 23, wherein the temperature is in a range from about 50° F. to about 120° F.

### Claim 27 (depends on 20)

The method of claim 20, wherein the aluminum wire has an IACS electrical conductivity of at least 59%.

### Claim 28 (depends on 20)

The method of claim 20, wherein the aluminum wire is a cylindrical wire having a diameter of about 0.114″.

### Claim 29 (depends on 28)

The method of claim 28, wherein the aluminum rod is a cylindrical rod having a diameter of about 5/16″.

### Claim 30 (depends on 29)

The method of claim 29, wherein the aluminum wire has an IACS electrical conductivity from about 61% to about 63%.

### Claim 31 (depends on 29)

The method of claim 29, wherein the aluminum wire has a tensile strength in a range from about 17,000 to about 21,750 psi.

### Claim 32

A method for producing an aluminum wire from an aluminum rod, the method comprising:
cold-drawing the aluminum rod at a temperature in a range from about 40° F. to about 250° F. to reduce the cross-sectional area, producing the aluminum wire;
wherein the aluminum rod is a cylindrical rod having a diameter in a range from about 0.2″ to 0.35″,
the aluminum wire is a cylindrical wire having a diameter in a range from about 0.1″ to about 0.15″,
the aluminum wire has a tensile strength of less than about 22,000 psi, and
the aluminum wire is not annealed.

### Claim 33 (depends on 32)

The method of claim 32, wherein the aluminum wire has a tensile strength in a range from about 17,000 to about 21,750 psi.

### Claim 34 (depends on 33)

The method of claim 33, wherein the aluminum rod has a tensile strength of less than about 12,000 psi.

### Claim 35 (depends on 33)

The method of claim 33, wherein the aluminum wire and the aluminum rod comprise an aluminum 1350 alloy.

### Claim 36 (depends on 35)

The method of claim 35, wherein the ratio of the cross-sectional area of the aluminum rod to the aluminum wire is in a range from about 3:1 to about 10:1.

### Claim 37 (depends on 32)

The method of claim 32, wherein the aluminum rod is a cylindrical rod having a diameter in a range from about ¼″ to about 11/32″.

### Claim 38 (depends on 37)

The method of claim 37, wherein the aluminum wire has a tensile strength in a range from about 17,000 to about 21,750 psi.

### Claim 39 (depends on 38)

The method of claim 38, wherein the ratio of the cross-sectional area of the aluminum rod to the aluminum wire is in a range from about 6:1 to about 9:1.
