# US 2016/0354766 A1 · Catalyst for synergistic control of oxynitride and mercury and method for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0354766 A1
- Document ID: US20160354766A1
- Status: Published application
- Kind: A1
- Application number: 15/104,045
- Filed: 2013-12-11
- Published: 2016-12-08
- Earliest claimed: 2013-12-11
- Assignees: Zhejiang University
- Applicants: Zhejiang University
- Inventors: Xiang GAO; Kunzan QIU; Chenghang ZHENG; Hao SONG; Weihong WU; Xinbo ZHU; Hongmin YU; Dian XU; Zhongyang LUO; Kefa CEN; Mingjiang NI
- Web page: https://patentgrep.com/patent/US20160354766A1

## CPC

- B01J 23/888: Tungsten
- B01D 53/8628: {Processes characterised by a specific catalyst}
- B01D 53/8665: {Removing heavy metals or compounds thereof, e.g. mercury}
- B01J 21/063: {Titanium; Oxides or hydroxides thereof}
- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- B01J 23/30: Tungsten
- B01J 37/0203: {the impregnation liquid containing organic compounds}
- B01J 37/0213: {Preparation of the impregnating solution}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/088: {Decomposition of a metal salt}
- B01J 37/343: {of ultrasonic wave energy}
- B01D 2255/207: Transition metals
- B01D 2255/20707: Titanium
- B01D 2255/20723: Vanadium
- B01D 2255/20738: Iron
- B01D 2255/20761: Copper
- B01D 2255/20769: Molybdenum
- B01D 2255/20776: Tungsten
- B01D 2255/20784: Chromium
- B01D 2257/602: Mercury or mercury compounds
- B01D 2258/0283: Flue gases
- B01J 35/45: Nanoparticles
- B01J 2523/00: Constitutive chemical elements of heterogeneous catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)

## Abstract

Disclosed are a catalyst for synergistic control of oxynitride and mercury and a method for preparing the same. The catalyst includes the following components by mass percentage: a carrier: TiO2 72%-98.6%, active components: V2O5 0.1%-5%, WO3 1%-10%, Cr2O3 0.1%-5% and Nb2O5 0.1%-5%, and a co-catalyst of 0.1%-3%. The present invention can be used for reducing the oxynitrides in a flue gas, meanwhile oxidizing zero-valent mercury into bivalent mercury and then controlling the reactions, has relatively high denitration performance and also has high mercury oxidation performance; compared with current commercial SCR catalysts, the mercury oxidation rate of the catalyst is improved to a great extent, which can adapt to the requirements for mercury removal in China's coal-fired power plants, the conversion rate of SO2/SO3 is relatively low, and the catalyst has a better anti-poisoning ability, and is a new catalyst with a low cost and high performance.

## Claims

### Claim 1

A catalyst for synergistic control of oxynitride and mercury, wherein the catalyst comprises the following components by mass percentage:
a carrier: TiO2 72-98.6%,
active components: V2O5 0.1-5%, WO31-10%, Cr2O3 0.1-5% and Nb2O5 0.1-5%,
and a co-catalyst of 0.1-3%.

### Claim 2 (depends on 1)

The catalyst for synergistic control of oxynitride and mercury according to claim 1, wherein the co-catalyst is selected from one of CuO, Fe2O3 and MoO3.

### Claim 3 (depends on 1, 2)

The catalyst for synergistic control of oxynitride and mercury according to claim 1 or claim 2, wherein the TiO2 is nanoscale anatase TiO2 with a particle size of less than 30 nm.

### Claim 4

A method for preparing a catalyst for synergistic control of oxynitride and mercury, wherein it comprises the following steps:
1) drying TiO2 and use it as a carrier;
2) stirring ammonium metavanadate and ammonium metatungstate under 50° C.-70° C. to dissolve in an oxalic acid or tartaric acid solution to obtain a solution A with pH value less than 2;
stirring chromic nitrate under 10-50° C. to dissolve in deionized water or tartaric acid to obtain a solution B;
stirring niobium oxalate under 50-70° C. to dissolve in deionized water or tartaric acid to obtain a solution C;
3) stirring cupric nitrate under 10-50° C. to dissolve in deionized water or tartaric acid to obtain a solution D;
or stirring ferric nitrate under 10-50° C. to dissolve in deionized water or tartaric acid to obtain a solution E;
or stirring ammonium molybdate under 10-50° C. to dissolve in deionized water or tartaric acid to obtain a solution F;
4) mixing the solution A, solution B and solution C with one of the solution D, solution E and solution F to obtain an impregnating solution, immersing the carrier from step 1) into the impregnating solution, stirring evenly for ultrasound concussion, evaporating and stirring with water bath for 10-60 minutes, drying in the oven and then calcine under 400° C.-550° C. for 3-5 hours to obtain the catalyst for synergistic control of oxynitride and mercury.

### Claim 5 (depends on 4)

The preparation method according to claim 4, wherein the drying in step 1) is drying under 105° C.-120° C. for 12 hours-24 hours.

### Claim 6 (depends on 4)

The preparation method according to claim 4, wherein the ultrasound concussion time in step 4) is 10-60 minutes.

### Claim 7 (depends on 4)

The preparation method according to claim 4, wherein the water bath temperature in step 4) is 70-90° C.

### Claim 8 (depends on 4)