# US 2016/0354764 A1 · Method for Preparing Ferrite Metal Oxide Catalyst

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0354764 A1
- Document ID: US20160354764A1
- Status: Published application
- Kind: A1
- Application number: 14/876,356
- Filed: 2015-10-06
- Published: 2016-12-08
- Earliest claimed: 2015-06-05
- Assignees: Korea Kumho Petrochemical Co., Ltd.
- Applicants: Korea Kumho Petrochemical Co., Ltd.
- Inventors: Ji Won Park; Jae Woo Kim; Yong Hee Yun; Yun Jung Kim; Kyoung Ho Row
- Web page: https://patentgrep.com/patent/US20160354764A1

## CPC

- B01J 23/78: with alkali- or alkaline earth metals
- B01J 35/30: characterised by their physical properties
- B01J 35/613: {10-100 m2/g}
- B01J 35/70: characterised by their crystalline properties, e.g. semi-crystalline (catalysts comprising carbon B01J21/18; molecular sieves B01J29/00)
- B01J 37/0045: {Drying a slurry, e.g. spray drying}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/082: {Decomposition and pyrolysis}
- C07C 5/48: with oxygen as an acceptor
- B01J 2235/15: X-ray diffraction
- C07C 2523/745: Iron
- C07C 2523/78: with alkali- or alkaline earth metals or beryllium
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

One aspect of the present invention provides a method for preparing a ferrite metal oxide catalyst, comprising (a) preparing a precursor solution by dissolving a magnesium nitrate precursor and an iron nitrate precursor in a polar solvent, (b) forming a catalyst powder by spray-pyrolyzing the precursor solution into a reactor using a carrier gas, and (c) calcinating the catalyst powder in a reservoir after conveying the catalyst powder to the reservoir. The method may increase the activity and stability of a catalyst powder by additionally performing a step of calcinating the catalyst powder at a certain temperature for a certain period of time, and may increase the purity of the catalyst by reducing moisture and nitrate remaining in the catalyst. Also, when using the catalyst in an oxidative dehydrogenation of n-butene, the selectivity and purity of 1,3-butadiene may increase.

## Claims

### Claim 1

A method for preparing a ferrite metal oxide catalyst, comprising:
(a) preparing a precursor solution by dissolving a magnesium nitrate precursor and an iron nitrate precursor in a polar solvent;
(b) forming a catalyst powder by spray-pyrolyzing the precursor solution into a reactor using a carrier gas; and
(c) calcinating the catalyst powder in a reservoir after conveying the catalyst powder to the reservoir.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the magnesium nitrate precursor and iron nitrate precursor in step (a) are mixed so that a molar ratio of magnesium to iron is 1.5:1 to 2.5:1.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the magnesium nitrate precursor and iron nitrate precursor in step (a) are magnesium nitrate and iron nitrate, respectively.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the polar solvent in step (a) is distilled water.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the carrier gas in step (b) is air.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the pressure of the air in step (b) is 2 to 4 atm.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the pyrolysis temperature in step (b) is 500° C. to 900° C.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the calcination temperature in step (c) is 500° C. to 600° C.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the calcination in step (c) is carried out for 1 to 4 hours.

### Claim 10 (depends on 1)

A ferrite metal oxide catalyst prepared by the method according to claim 1.

### Claim 11 (depends on 10)

A method for preparing 1,3-butadiene, comprising:
filling the ferrite metal oxide catalyst according to claim 10 in a reactor; and
introducing a reaction mixture containing n-butene into the reactor to pass through the reactor.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the reaction mixture comprises 4 to 12% by volume of n-butene, 16 to 30% by volume of air, and 60 to 80% by volume of steam.

### Claim 13 (depends on 11)

The method according to claim 11, wherein the reaction mixture is introduced in a gas hourly space velocity (GHSV) in range of 100 h−1 to 700 h−1.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the temperature of the reactor is controlled to be 300° C. to 500° C.