# US 2016/0354759 A1 · Method for producing porous bodies with enhanced properties

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0354759 A1
- Document ID: US20160354759A1
- Status: Published application
- Kind: A1
- Application number: 15/171,273
- Filed: 2016-06-02
- Published: 2016-12-08
- Earliest claimed: 2015-06-02
- Assignees: Scientific Design Company, Inc.
- Applicants: Scientific Design Company, Inc.
- Inventors: Wojciech L. Suchanek; Matthew Julian
- Web page: https://patentgrep.com/patent/US20160354759A1

## CPC

- B01J 21/04: Alumina
- B01J 19/0013: {Controlling the temperature of the process}
- B01J 23/04: Alkali metals
- B01J 23/36: Rhenium
- B01J 23/50: Silver
- B01J 35/612: {less than 10 m2/g}
- B01J 35/633: {less than 0.5 ml/g}
- B01J 35/635: {0.5-1.0 ml/g}
- B01J 35/638: {more than 1.0 ml/g}
- B01J 35/66: Pore distribution
- B01J 37/0018: {Addition of a binding agent or of material, later completely removed among others as result of heat treatment, leaching or washing,(e.g. forming of pores; protective layer, desintegrating by heat)}
- B01J 37/086: {Decomposition of an organometallic compound, a metal complex or a metal salt of a carboxylic acid}
- C04B 38/00: Porous mortars, concrete, artificial stone or ceramic ware; Preparation thereof (treating slag with gases or gas generating material C04B5/06 {; expanded graphite C04B35/536})
- C04B 38/0096: {Pores with coated inner walls}
- C04B 38/08: by adding porous substances
- C04B 41/009: {characterised by the material treated}
- C04B 41/4535: {applied as a solution, emulsion, dispersion or suspension}
- C04B 41/5116: {Ag or Au}
- C04B 41/88: Metals
- C07D 301/10: with catalysts containing silver or gold
- C07D 301/22: by oxidation of saturated compounds with air or molecular oxygen (of mixtures of unsaturated and saturated compounds C07D301/04)
- B01J 2219/00051: Controlling the temperature
- C04B 2111/0081: {as catalysts or catalyst carriers}
- Y02P 20/52: using catalysts, e.g. selective catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C07D: HETEROCYCLIC COMPOUNDS (macromolecular compounds C08)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A precursor mixture for producing a porous body, wherein the precursor mixture comprises: (i) milled alpha alumina powder having a particle size of 0.1 to 6 microns, (ii) boehmite powder that functions as a binder of the alpha alumina powders, and (iii) burnout materials having a particle sizes of 1-10 microns. In some embodiments, an unmilled alpha alumina powder having a particle size of 10 to 100 microns is also included in said precursor mixture. Also described herein is a method for producing a porous body in which the above-described precursor mixture is formed to a given shape, and subjected to a heat treatment step in which the formed shape is sintered to produce the porous body.

## Claims

### Claim 1

A precursor mixture for producing a porous body, wherein the precursor mixture comprises: (i) at least one milled alpha alumina powder having a particle size of 0.1 to 6 microns, (ii) boehmite powder that functions as a binder of the alpha alumina powders, and (iii) at least one burnout material having a particle size of 1-10 microns.

### Claim 2 (depends on 1)

The precursor mixture of claim 1, further comprising unmilled alpha alumina powder having a particle size of 10 to 100 microns.

### Claim 3 (depends on 2)

The precursor mixture of claim 2, wherein the weight ratio of milled to unmilled alpha alumina powder is in a range of 0.25:1 to about 5:1.

### Claim 4 (depends on 1)

The precursor mixture of claim 1, wherein unmilled alpha alumina powder is excluded from the precursor mixture.

### Claim 5 (depends on 1)

The precursor mixture of claim 1, further comprising an additive selected from solvents and lubricants.

### Claim 6 (depends on 1)

The precursor mixture of claim 1, wherein said burnout material is selected from at least one of a polyolefin powder and graphite powder.

### Claim 7 (depends on 1)

The precursor mixture of claim 1, wherein said burnout material is selected from both a polyolefin powder and graphite powder.

### Claim 8 (depends on 7)

The precursor mixture of claim 7, wherein the weight ratio of polyolefin powder to graphite powder is in a range of 0.25:1 to about 5:1.

### Claim 9 (depends on 1)

The precursor mixture of claim 1, wherein the boehmite is present in an amount of at least 10% by weight of total alumina content.

### Claim 10 (depends on 1)

The precursor mixture of claim 1, wherein the boehmite is present in an amount of at least 25% by weight of total alumina content.

### Claim 11 (depends on 1)

The precursor mixture of claim 1, wherein the boehmite is nano-sized powder with dispersed particle size <100 nm.

### Claim 12 (depends on 1)

The precursor mixture of claim 1, wherein said milled alpha alumina powder has a particle/crystallite size of 0.25-4 microns.

### Claim 13 (depends on 1)

The precursor mixture of claim 1, wherein a silicon-containing substance is substantially excluded from the precursor mixture.

### Claim 14 (depends on 1)

The precursor mixture of claim 1, wherein a sodium-containing substance is substantially excluded from the precursor mixture.

### Claim 15

A method for producing a porous body, the method comprising:
providing a precursor mixture comprising (i) milled alpha alumina powder having a particle size of 0.1 to 6 microns, (ii) boehmite powder that functions as a binder of the alpha alumina powders, and (iii) burnout material having a particle size of 1-10 microns;
forming a predetermined shape; and
subjecting the shape to a heat treatment step in which the shape is sintered to produce the porous body.

### Claim 16 (depends on 15)

The method of claim 15, further comprising unmilled alpha alumina powder having a particle size of 10 to 100 microns in said precursor mixture.

### Claim 17 (depends on 16)

The method of claim 16, wherein the weight ratio of milled to unmilled alpha alumina powder is in a range of 0.25:1 to about 5:1.

### Claim 18 (depends on 15)

The method of claim 15, wherein unmilled alpha alumina powder is excluded from the precursor mixture.

### Claim 19 (depends on 15)

The method of claim 15, wherein the method comprises:
(i) dispersing boehmite into water to produce a dispersion of boehmite;
(ii) adding a milled alpha alumina powder having a particle size of 0.1 to 6 microns to the dispersion of boehmite, and mixing until a first homogeneous mixture is obtained, wherein said boehmite functions as a binder of the alpha alumina powder;
(iii) adding burnout materials having a particle size of 1-10 microns, and mixing until a second homogeneous mixture is obtained;
(iv) forming the second homogeneous mixture to form a shape of said second homogeneous mixture; and
(v) subjecting the formed shape to a heat treatment step in which the formed shape is sintered to produce the porous body.

### Claim 20 (depends on 15)

The method of claim 15, wherein said heat treatment step comprises:
(a) subjecting the formed shape to a heat treatment step within a temperature in a range of 35-900° C. to remove water and burn out the burnout material to produce a pre-fired porous body; and
(b) subjecting the pre-fired porous body to a sintering step at a temperature within a range of 900-2000° C. to produce said porous body.

### Claim 21 (depends on 15)

The method of claim 15, wherein said porous body possesses at least one of a water absorption of at least 30%, a crush strength of at least 40 N, and a BET surface area of at least 0.3 m2/g.

### Claim 22 (depends on 15)

The method of claim 15, wherein said porous body possesses a pore architecture that provides at least one of a tortuosity of 7 or less, a constriction of 4 or less, and a permeability of 30 mdarcys or greater.

### Claim 23 (depends on 15)

The method of claim 15, wherein said burnout material is selected from a polyolefin powder and graphite powder.

### Claim 24 (depends on 19)

The method of claim 19, wherein said burnout material comprises a polyolefin powder, and said step (iii) comprises adding said polyolefin powder having a particle size of 1-10 microns, and mixing until a second homogeneous mixture is obtained.

### Claim 25 (depends on 24)

The method of claim 24, wherein said step (iii) further comprises, either simultaneous or subsequent to adding and mixing the polyolefin powder, adding graphite powder as an additional burnout material, and mixing until said second homogeneous mixture is obtained, which includes the graphite powder.

### Claim 26 (depends on 25)

The method of claim 25, wherein the weight ratio of polyolefin powder to graphite powder is in a range of 0.25:1 to about 5:1.

### Claim 27 (depends on 25)

The method of claim 25, wherein said graphite powder has a particle size of 3-10 microns.

### Claim 28 (depends on 19)

The method of claim 19, wherein said step (ii) includes, either simultaneous or subsequent to adding and mixing the milled alpha alumina powder, adding unmilled alpha alumina powder having a particle size in a range of 10-100 microns, and mixing until said first homogeneous mixture is obtained.

### Claim 29 (depends on 28)

The method of claim 28, wherein the weight ratio of milled to unmilled alpha alumina powder is in a range of 0.25:1 to about 5:1.

### Claim 30 (depends on 15)

The method of claim 15, wherein the boehmite is present in an amount of at least 10% by weight of total alumina content.

### Claim 31 (depends on 15)

The method of claim 15, wherein the boehmite is present in an amount of at least 25% by weight of total alumina content.

### Claim 32 (depends on 15)

The method of claim 15, wherein the boehmite is nano-sized powder with dispersed particle size <100 nm.

### Claim 33 (depends on 15)

The method of claim 15, wherein unmilled alpha alumina powder is excluded from the method to produce the porous body.

### Claim 34 (depends on 15)

The method of claim 15, wherein a silicon-containing substance is substantially excluded from the method to produce the porous body.

### Claim 35 (depends on 15)

The method of claim 15, wherein a sodium-containing substance is substantially excluded from the precursor mixture.

### Claim 36 (depends on 15)

The method of claim 15, wherein, after said heat treatment step to form a porous body, said method further comprises depositing silver on and/or in said porous body.

### Claim 37 (depends on 15)

The method of claim 15, wherein said milled alpha alumina powder has a particle size of 0.25-4 microns.

### Claim 38 (depends on 15)

The method of claim 15, wherein the precursor mixture is formed by one of extrusion or pressing.