# US 2016/0354730 A1 · Method for the production of poly(meth)acrylonitrile-based polymer membranes, polymer membranes, and also solutions for the production of a polymer membrane

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0354730 A1
- Document ID: US20160354730A1
- Status: Published application
- Kind: A1
- Application number: 15/101,101
- Filed: 2014-12-03
- Published: 2016-12-08
- Earliest claimed: 2013-12-04
- Assignees: Fraunhofer-Gesellschaft zur Förderung der angewandten Forschung e.V.
- Applicants: Fraunhofer-Gesellschaft Zur FöRderung Der Angewandten Forschung E.V.
- Inventors: Detlev FRITSCH
- Web page: https://patentgrep.com/patent/US20160354730A1

## CPC

- B01D 71/421: {Polyacrylonitrile}
- B01D 67/0011: {Casting solutions therefor}
- B01D 67/0083: {Thermal after-treatment}
- B01D 67/0095: {Drying}
- B01D 69/087: {Details relating to the spinning process}
- C08L 33/20: Homopolymers or copolymers of acrylonitrile (C08L55/02 takes precedence)
- B01D 2323/06: Specific viscosities of materials involved
- B01D 2323/081: Heating
- B01D 2323/12: Specific ratios of components used
- B01D 2323/22: Specific non-solvents or non-solvent system
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present invention relates to a method for the production of a polymer membrane based on poly(meth)acrylonitrile, in which a poly(meth)acrylonitrile-comprising solution is used. The solution comprises a solvent for poly(meth)acrylonitrile and also a non-solvent. All of the components of the solution which are used are thereby non-toxic and do not represent chemicals which are a hazard to water. In addition, a solution which comprises a solvent for poly(meth)acrylonitrile and also a non-solvent is described. The solution is suitable in particular for implementing the method according to the invention.

## Claims

### Claim at position 1

1-18. (canceled)

### Claim 19

A method for the production of a polymer membrane, in which a solution comprising:
a) poly(meth)acrylonitrile, a copolymer based on (meth)acrylonitrile, or a mixture thereof,
b) dimethylsulphoxide (DMSO) as solvent for poly(meth)acrylonitrile or a copolymer based on (meth)acrylonitrile, and
c) at least one non-solvent in which poly(meth)acrylonitrile or the copolymer based on (meth)acrylonitrile does not dissolve and which is miscible with the solvent,
the solution being free of crosslinkers for poly(meth)acrylonitrile or copolymers based on poly(meth)acrylonitrile,
being poured as a film or spun to form a hollow fibre,
the poly(meth)acrylonitrile, copolymer based on (meth)acrylonitrile, or the mixture thereof being precipitated by a phase-inversion process,
and the poly(meth)acrylonitrile, copolymer based on (meth)acrylonitrile, or the mixture thereof being stabilised by heat treatment at temperatures increased relative to room temperature.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the non-solvent is selected from the group consisting of acetone, diacetone alcohol, ethyl lactate, 1,3-dioxolane, polyalkylene glycol, alcohols, water and mixtures thereof.

### Claim 21 (depends on 19)

The method according to claim 19, wherein the film is poured onto a substrate.

### Claim 22 (depends on 19)

The method according to claim 19, wherein the film or hollow fibre obtained after the phase-inversion process is washed with water.

### Claim 23 (depends on 19)

The method according to claim 19, wherein the heat treatment is effected at temperatures of 50 to 150° C., subsequent to the phase-inversion process, with water and/or over period of time of 5 min to 24 hours.

### Claim 24 (depends on 19)

The method according to claim 19, wherein, after crosslinking and/or or washing, drying of the membrane is implemented.

### Claim 25 (depends on 19)

The polymer membrane produced according to the method of claim 19, which is in the form of a flat membrane or hollow fibre membrane.

### Claim 26 (depends on 25)

The polymer membrane according to claim 25, wherein the thickness of the membrane, without any possibly present substrate, is of 20 to 200 μm.

### Claim 27 (depends on 25)

The polymer membrane according to claim 25, wherein the pore size of the membrane at the bubble point is of 15 to 100 nm.

### Claim 28 (depends on 25)

The polymer membrane according to claim 25, wherein the average pore size of the membrane is 15 to 30 nm.

### Claim 29 (depends on 25)

The polymer membrane according to claim 25, which has a nitrogen permeability JN2 of 10 to 1,000 m3/(m2·h·bar).

### Claim 30 (depends on 25)

The polymer membrane according to claim 25, which has a foam structure.

### Claim 31

A solution for the production of a polymer membrane, comprising
a) poly(meth)acrylonitrile, a copolymer based on (meth)acrylonitrile or a mixture thereof,
b) at least one solvent for poly(meth)acrylonitrile or a copolymer based on (meth)acrylonitrile in which the previously mentioned components are present in dissolved state; and
c) at least one non-solvent in which poly(meth)acrylonitrile or the copolymer based on (meth)acrylonitrile does not dissolve and which is miscible with the solvent, the solution being free of crosslinkers for poly(meth)acrylonitrile or copolymers based on poly(meth)acrylonitrile.

### Claim 32 (depends on 31)

The solution according to claim 31, wherein the non-solvent is selected from the group consisting of acetone, diacetone alcohol, ethyl lactate, 1,3-dioxolane, polyalkylene glycol, alcohols, water, and mixtures thereof.

### Claim 33 (depends on 31)

The solution according to claim 31, wherein the total content of poly(meth)acrylonitrile, of the copolymer based on (meth)acrylonitrile or mixtures thereof, relative to the sum of solvent and non-solvent is of 1 to 30% by weight.

### Claim 34 (depends on 31)

The solution according to claim 31, wherein the content of non-solvent, relative to the content of solvent or of the mixture of at least two solvents is 10 to 60% by weight.

### Claim 35 (depends on 31)

The solution according to claim 31, wherein the copolymer based on (meth)acrylonitrile is obtained by copolymerisation of (meth)acrylonitrile with at least one copolymer selected from the group consisting of (meth)allyl sulphonic acid or the salts thereof.

### Claim 36 (depends on 31)

The solution according to claim 31, which has a viscosity of 1.5 to 20 Pa·s.